Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Shear Strength = 1700 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Shear Strength >= 11.7 MPa
>= 1700 psi
Die
Epoxy Technology EPO-TEK® 302 Fast Setting, Optical Epoxy
Product Description: EPO-TEK® 302 is a two component, fast-gelling, room temperature curing epoxy, designed for electronic, optical, medical, and general applications. Advantages & Application No..
Shear Strength >= 11.7 MPa
>= 1700 psi
Die
Epoxy Technology EPO-TEK® B9021-6 Epoxy Paste
Material Description: A single component, B-stageable epoxy paste for semiconductor, microelectronics, and optical assemblies. It can be used in hybrid assemblies for lid-sealing and substrate atta..
Shear Strength >= 11.7 MPa
>= 1700 psi
Die
Epoxy Technology EPO-TEK® E2001 Electrically Conductive, Silver-Filled Epoxy
Product Description: EPO-TEK® E2001 is a two component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications using a snap-cure profile. Advantages & Appl..
Shear Strength >= 11.7 MPa
>= 1700 psi
Die
Epoxy Technology EPO-TEK® E2036 Epoxy
Product Description: A two component, slightly flexible, silver-filled, electrically conductive adhesive for semiconductor and electronic assemblies. It is a low Tg epoxy, intended for many kinds o..
Shear Strength >= 11.7 MPa
>= 1700 psi
Die
Epoxy Technology EPO-TEK® E4110-PFC Electrically Conductive Epoxy
Product Description: EPO-TEK®E4110-PFC is a two-component, silver filled, electrically conductive adhesive designed for semiconductor IC packaging and general electronic assembly. It is a thixotr..
Shear Strength >= 11.7 MPa
>= 1700 psi
Die
Epoxy Technology EPO-TEK® EE165-3 Silver Filled Epoxy
A two component, silver-filled, electrically conductive epoxy made for bonding of SMDs, and general solder replacement at the PCB level and circuit assembly. It was designed to be low modulus and f..
Shear Strength >= 11.7 MPa
>= 1700 psi
Die after 1000 hrs 85C/85%R
Epoxy Technology EPO-TEK® EK1000-MP Epoxy
Material Description: A single component, silver-filled adhesive that exhibits exceptional thermal and electrical conductivity along with a shiny silver appearance making it ideal for the demanding ..
Shear Strength >= 11.7 MPa
>= 1700 psi
Die after 1000 hrs 85C/85%R
Epoxy Technology EPO-TEK® EK2000 Epoxy
Preliminary Product Information SheetMaterial Description: A two component, silver-filled adhesive that exhibits exceptional thermal and electrical conductivity along with a shiny silver appearance ..
Shear Strength >= 11.7 MPa
>= 1700 psi
Die
Epoxy Technology EPO-TEK® H20E-MP Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® H20E-MP is a two component, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is al..
Shear Strength 11.7 MPa
1700 psi
Lap
Epoxy Technology EPO-TEK® H20-HC Electrically Conductive Epoxy
Product Description: EPO-TEK® H20E-HC is a two component, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is al..
Shear Strength >= 11.7 MPa
>= 1700 psi
Die
Epoxy Technology EPO-TEK® H20-LC Electrically Conductive, Silver Epoxy
Product Description: EPO TEK® H20E-LC is a two component, silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is also used exte..
Shear Strength >= 11.7 MPa
>= 1700 psi
Die
Epoxy Technology EPO-TEK® H20S Electrically Conductive, Silver Epoxy for Die Stamping
Product Description: EPO-TEK® H20S is a modified version of EPO-TEK® H20E, designed primarily for die stamping and dispensing techniques for chip bonding. EPO-TEK®H20S is a highly reliable, two ..
Shear Strength >= 11.7 MPa
>= 1700 psi
Die
Epoxy Technology EPO-TEK® H24 Electrically Conductive Epoxy
Product Description: EPO-TEK® H24 is a two component, electrically and thermally conductive epoxy adhesive designed for semiconductor die attach and hybrid micro-electronics assembly.Advantages & A..
Shear Strength >= 11.7 MPa
>= 1700 psi
Die
Epoxy Technology EPO-TEK® H31D-LV Epoxy
Material Description: A single component, silver-filled, electrically conductive epoxy designed for semiconductor die attach applications found in hybrids, JEDEC, and optoelectronic packaging. It i..
Shear Strength >= 11.7 MPa
>= 1700 psi
Die
Epoxy Technology EPO-TEK® P1011 Electrically Conductive Modified Polyimide
Product Description: EPO-TEK® P-1011 is a single component, modified polyimide, silver-filled adhesive designed for chip bonding in microelectronic and optoelectronic applications.Advantages & Appl..
Shear Strength >= 11.7 MPa
>= 1700 psi
Die
Epoxy Technology EPO-TEK® H20E Electrically Conductive, Silver Epoxy
Product Description: EPO-TEK® H20E is a two component, 100% solids silver-filled epoxy system designed specifically for chip bonding in microelectronic and optoelectronic applications. It is also ..
Shear Strength 11.7 MPa
1700 psi
Overlap, Stainless Steel MEK/abrade/MEK
3M Scotch-Weld™ DP420 Off-White Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
Shear Strength 11.7 MPa
1700 psi
Overlap, PVC, Substrate Failure
3M Scotch-Weld™ DP8810NS Low Odor Acrylic Adhesives
3M™ Scotch-Weld™ Low Odor Acrylic Adhesives are high performance, two-part acrylic adhesives with lower odor than most acrylic adhesives. These toughened products offer excellent shear, peel, and ..
Shear Strength 11.7 MPa
1700 psi
Overlap, Aluminum-MEK/abrade/MEK-Adhesive Failure/Cohesive Failure; ASTM D1002
3M Scotch-Weld™ LSB90 Flexible Epoxy
3M™ Scotch-Weld™ Epoxy Adhesive LSB90 is a high performance, two-part, flexible epoxy adhesive offering high shear and peel adhesion and very high levels of durability. It has a 90 minute worklife..
Shear Strength 11.7 MPa
1700 psi
Overlap, Aluminum, Adhesive Failure
3M Scotch-Weld™ Thin Instant Wood Adhesives and Surface Activator
3M™ Scotch-Weld™ Instant Wood Adhesives an Surface Activator are single component, room temperature-curing adhesives that provides cure and speed and shear strength for demanding applications in t..
Shear Strength 11.7 MPa
1700 psi
Overlap, Steel; ASTM D1002-64
3M Scotch-Weld™ CA40 Instant Adhesive
3M™ Scotch-Weld™ Instant Adhesives are single component, high strength cyanoacrylate adhesives. Very fast setting and excellent adhesion to many substrates including flexible vinyl and EPDM rubbe..
Copyright © lookpolymers.com All Rights Reserved