Polymer Property : Shear Strength = 24.1 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Shear Strength 20.7 - 24.1 MPa
3000 - 3500 psi
ND Industries 301 Surface Insensitive Instant Superglue
Low-medium viscosity for difficult to bond substrates
Shear Strength 20.7 - 24.1 MPa
3000 - 3500 psi
ND Industries 306 Surface Insensitive Instant Superglue
Low viscosity for difficult to bond rubber compounds
Shear Strength 20.7 - 24.1 MPa
3000 - 3500 psi
ND Industries 331 Surface Insensitive Instant Superglue
Medium-high viscosity for difficult to bond surfaces
Shear Strength 20.7 - 24.1 MPa
3000 - 3500 psi
ND Industries 333 Surface Insensitive Instant Superglue
Low-medium viscosity for difficult to bond substrates
Shear Strength 20.7 - 24.1 MPa
3000 - 3500 psi
ND Industries 354 Surface Insensitive Instant Superglue
Gel for porous, hard to bond surfaces - large gap
Shear Strength 20.7 - 24.1 MPa
3000 - 3500 psi
ND Industries 360 Surface Insensitive Instant Superglue
General DescriptionA medium viscosity, general purpose cyanoacrylate which is also surface sensitive. Can handle a wide array of materials which include wood, cork, leather, stone and plastics, in ..
Shear Strength 20.7 - 24.1 MPa
3000 - 3500 psi
ND Industries SuperGlue Ethyl 309
Non-running gel for porous surfaces, general purpose
Shear Strength 20.7 - 24.1 MPa
3000 - 3500 psi
ND Industries SuperGlue Ethyl 314
General DescriptionA medium viscosity ethyl-based cyanoacrylate particularly suitable for rubbers and plastics. It is fast acting and may be fillet cured using ND Excel Accelerators.rubber O-rings,..
Shear Strength 20.7 - 24.1 MPa
3000 - 3500 psi
ND Industries SuperGlue Ethyl 316
Medium-high viscosity for gap fillingMeets military spec Mil-A-46050C Type II Class III
Shear Strength 20.7 - 24.1 MPa
3000 - 3500 psi
ND Industries SuperGlue Ethyl 322
High viscosity for large gap filling non-metallic surfacesMeets military spec Mil-A-46050C Type II Class III
Shear Strength 20.7 - 24.1 MPa
3000 - 3500 psi
ND Industries SuperGlue Ethyl 344
Medium viscosity, general purposeMeets military spec Mil-A-46050C Type II Class III
Shear Strength 20.7 - 24.1 MPa
3000 - 3500 psi
ITW Plexus Plexusâ„¢ MA300 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose adhesive high strength.Information provided by Illinois Tool Works.
Shear Strength 20.7 - 24.1 MPa
3000 - 3500 psi
ITW Plexus Plexusâ„¢ MA310 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Use with "difficult to bond" plastics, high strength.Information provided by Illinois Tool Works.
Shear Strength 20.7 - 24.1 MPa
3000 - 3500 psi
ITW Plexus Plexusâ„¢ MA330 Methacrylate Adhesive
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Pigmented MA310, use with "difficult to bond" plastics.Information provided by Illinois Tool Works..