| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Shear Strength | 20.7 MPa | 3000 psi | |
|
ND Industries 230 Structural Adhesive
Multi Cure, High Viscosity Adhesive
|
|||
| Shear Strength | 20.7 - 24.1 MPa | 3000 - 3500 psi | |
|
ND Industries 306 Surface Insensitive Instant Superglue
Low viscosity for difficult to bond rubber compounds
|
|||
| Shear Strength | 20.7 - 24.1 MPa | 3000 - 3500 psi | |
|
ND Industries 331 Surface Insensitive Instant Superglue
Medium-high viscosity for difficult to bond surfaces
|
|||
| Shear Strength | 20.7 - 24.1 MPa | 3000 - 3500 psi | |
|
ND Industries 354 Surface Insensitive Instant Superglue
Gel for porous, hard to bond surfaces - large gap
|
|||
| Shear Strength | 20.7 - 24.1 MPa | 3000 - 3500 psi | |
|
ND Industries 360 Surface Insensitive Instant Superglue
General DescriptionA medium viscosity, general purpose cyanoacrylate which is also surface sensitive. Can handle a wide array of materials which include wood, cork, leather, stone and plastics, in ..
|
|||
| Shear Strength | 20.7 - 24.1 MPa | 3000 - 3500 psi | |
|
ND Industries SuperGlue Ethyl 309
Non-running gel for porous surfaces, general purpose
|
|||
| Shear Strength | 20.7 - 24.1 MPa | 3000 - 3500 psi | |
|
ND Industries SuperGlue Ethyl 314
General DescriptionA medium viscosity ethyl-based cyanoacrylate particularly suitable for rubbers and plastics. It is fast acting and may be fillet cured using ND Excel Accelerators.rubber O-rings,..
|
|||
| Shear Strength | 20.7 - 24.1 MPa | 3000 - 3500 psi | |
|
ND Industries SuperGlue Ethyl 316
Medium-high viscosity for gap fillingMeets military spec Mil-A-46050C Type II Class III
|
|||
| Shear Strength | 20.7 - 24.1 MPa | 3000 - 3500 psi | |
|
ND Industries SuperGlue Ethyl 322
High viscosity for large gap filling non-metallic surfacesMeets military spec Mil-A-46050C Type II Class III
|
|||
| Shear Strength | 20.7 MPa | 3000 psi | |
|
NextGen Adhesives M907-20 Medical Grade Epoxy Adhesive
Description: NGAC M907-20 is a medium viscosity adhesive system that is specifically formulated for medical device assembly applications.Advantages and Applications: Uses include laminating, bonding..
|
|||
| Shear Strength | 20.7 MPa | 3000 psi | |
|
ND Industries 240 Structural Adhesive
Excellent impact and solvent resistance
|
|||
| Shear Strength | 20.7 MPa | 3000 psi | |
|
NextGen Adhesives G907-21 Structural Epoxy Adhesive
Description: NGAC G907-21 is a high viscosity and thixotropic adhesive system that is specifically formulated for structural bonding applications: industrial, electronics and aerospace.Advantages an..
|
|||
| Shear Strength | >= 20.7 MPa | >= 3000 psi | Tensile lap, Al to Al |
|
Master Bond EP21HTND High Temperature Resistant, Non-Drip Epoxy Compound
Description: Master Bond EP21HTND is a two component, room temperature curing epoxy adhesive, sealant and coating with a paste viscosity and non-drip application feature. Its features are easy handl..
|
|||
| Shear Strength | >= 20.7 MPa | >= 3000 psi | Bond, Al to Al |
|
Master Bond EP30LV-1 Ultra Low Viscosity, Two Part Epoxy System
Description: Master Bond Polymer System EP30LV-1 is an ultra low viscosity, two component epoxy system for high performance bonding, coating, sealing, potting and encapsulation. It readily cures at ..
|
|||
| Shear Strength | 20.7 MPa | 3000 psi | |
|
Dymax Magnet Bonder™ 2020 Adhesive
DYMAX® Magnet Bonder™ Adhesives for Higher Performance and Lower CostDymax 2020 Magnet Bonder™ AdhesiveAcrylic and methacrylic acid-free; bond ferrite to metal, plated metals, E-coat, sealed cans..
|
|||
| Shear Strength |
20.7
MPa @Temperature 24.0 °C |
3000
psi @Temperature 75.2 °F |
Aluminum Overlap; ASTM D1002 |
|
3M Scotch-Weld™ 183 B/A Green Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 1838 B/A is a controlled flow product. This epoxy adhesives are two-part, room temperature curing structural adhesives with high shear strengths and excellent envir..
|
|||
| Shear Strength | 20.7 MPa | 3000 psi | Overlap, Galvanized Steel Okite degrease Electrodeposited |
|
3M Scotch-Weld™ DP460 NS Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.Informat..
|
|||
| Shear Strength | 20.7 MPa | 3000 psi | Overlap, Green FRP, Cohesive Failure |
|
3M Scotch-Weld™ DP810 Black Structural Adhesive
3M™ Scotch-Weld™ Low-Odor Acrylic Adhesives are two-part, 1:1 mix ratio, toughened structural adhesives with less odor than most acrylic adhesives. The adhesives have excellent shear and peel stre..
|
|||
| Shear Strength |
20.7
MPa @Temperature -55.0 °C |
3000
psi @Temperature -67.0 °F |
Etched Aluminum Overlap |
|
3M Scotch-Weld™ EC-2086 Structural Adhesive
3M™ Scotch-Weld™ Structural Adhesive EC-2086 is a one-part, 100% solids thermosetting liquid adhesives.Information provided by 3M
|
|||
| Shear Strength | 20.7 MPa | 3000 psi | cured, grit-blasted steel; ASTM D1002 |
|
3M Scotch-Weld™ ECI Gel General Purpose Instant Adhesive
3M™ Scotch-Weld™ General Purpose Instant Adhesives are single component, high strength ethyl cyanoacrylate adhesive designed to bond to a variety of substances including most plastics, rubbers, me..
|
|||
| Shear Strength | 20.7 MPa | 3000 psi | ASTM D1002-94 |
|
Aremco Aremco-Bond™ 631 High Performance Epoxide
Clear-Amber, 1:1, Good Bond Strength and Corrosion Resistance.Also available filled with aluminum oxide (Alumina) or pigments.
|
|||
| Shear Strength |
20.7
MPa @Temperature -58.0 - -56.0 °C |
3000
psi @Temperature -72.4 - -68.8 °F |
Average |
|
3M Scotch-Weld™ EC-1386 Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive EC-1386 is a one-part, 100% solids, thermosetting liquid adhesive.Information provided by 3M
|
|||
| Shear Strength | 20.7 MPa | 3000 psi | cured, grit-blasted steel; ASTM D1002 |
|
3M Scotch-Weld™ EC600 General Purpose Instant Adhesive
3M™ Scotch-Weld™ General Purpose Instant Adhesives are single component, high strength ethyl cyanoacrylate adhesive designed to bond to a variety of substances including most plastics, rubbers, me..
|
|||
| Shear Strength | 20.7 MPa | 3000 psi | cured, grit-blasted steel; ASTM D1002 |
|
3M Scotch-Weld™ SF20 Super Fast Instant Adhesive
3M™ Scotch-Weld™ Super Fast Instant Adhesives rely less on surface moisture for cure speed than standard cyanoacrylates. They are designed to join together difficult-to-bond plastics and rubbers, ..
|
|||
| Shear Strength |
20.7
MPa @Temperature -73.0 °C |
3000
psi @Temperature -99.4 °F |
Overlap, Etched Aluminum; ASTM D1002 |
|
3M Scotch-Weld™ 2216 B/A Gray Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel..
|
|||
| Shear Strength | 20.7 MPa | 3000 psi | Overlap, Etched Al, Hydrocarbon Fluid for 7 days |
|
3M Scotch-Weld™ 2216 B/A Translucent Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive 2216 B/A is a flexible, two-part, room temperature curing epoxy with high peel and shear strength. Scotch-Weld epoxy adhesive 2216 B/A is identical to 3M Scotch-Wel..
|
|||
| Shear Strength | 20.7 MPa | 3000 psi | Overlap, Antifreeze/H2O (50/50) immersion, 82°C for 30 days |
|
3M Scotch-Weld™ DP420 Black Epoxy Adhesive
3M™ Scotch-Weld™ Epoxy Adhesive are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion, and very high levels of durability.Information provided by 3M
|
|||
| Shear Strength | 20.7 MPa | 3000 psi | |
|
Dymax Magnet Bonder™ 2010 Adhesive
DYMAX® Magnet Bonder™ Adhesives for Higher Performance and Lower CostDymax 2010 Magnet Bonder™ AdhesiveHigh performance; bond plated materials, E-coat Typical Use: D.C. motor magnet to can bond..
|
|||