| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Secant Modulus, MD | 0.150 GPa | 21.8 ksi | at 1%; ASTM D882 |
|
NOVA Chemicals Novapol® LA-0219-AM LDPE Foam Resin
Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinFilm properties are typical of blo..
|
|||
| Secant Modulus, MD | 0.150 GPa | 21.8 ksi | at 1%; ASTM D882 |
|
NOVA Chemicals Novapol® LF-0219-A LDPE Film Resin
Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Industrial packaging, Liners, Blends with LLDPE, Foam articlesAdditives: Base resinInformation provided by NOVA Chemi..
|
|||
| Secant Modulus, MD | 0.150 GPa | 21.8 ksi | ASTM D882 |
|
NOVA Chemicals Novapol® LF-0219-D LDPE Film Resin
Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Liners, industrial packaging, blends with LLDPE.Data provided by the manufacturer.
|
|||
| Secant Modulus, MD | 0.150 GPa | 21.8 ksi | 5%; ASTM D882 |
|
Petroquimica Triunfo Trithene® TS 9022 MDPE - Overwrap Packaging
The Trithene TS 9022 resin is a medium-density polyethylene (MDPE) with good optical properties, excellent stiffness and processability, that warrants the production of thin films with good appearan..
|
|||
| Secant Modulus, MD | 0.150 GPa | 21.8 ksi | at 1%; ASTM D882 |
|
Chevron Phillips mPact™ D143SA m-LLDPE Linear Low Density Polyethylene
(discontinued **)
Low Density PolyethyleneCustomer Benefits: This metallocene LLDPE film resin possesses the typical physical properties of metallocene polyethylenes with the added potential benefit of improved proce..
|
|||
| Secant Modulus, MD | 0.150 GPa | 21.8 ksi | ASTM D882 |
|
Chevron Phillips Vytek™ V208C3 Enhanced LLDPE Blown Film Resin
(discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use..
|
|||
| Secant Modulus, MD | 0.150 GPa | 21.8 ksi | ASTM D882 |
|
NOVA Chemicals Novapol® LF-0218-AB LDPE Film Resin
(discontinued **)
Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Specifically designed for foam process, blends with LLDPE.Data provided by the manufactu..
|
|||
| Secant Modulus, MD | 0.150 GPa | 21.8 ksi | at 1%; ASTM D882 |
|
NOVA Chemicals Novapol® LA-0218-AB LDPE Foam Resin
(discontinued **)
Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Specifically designed for foam process, Blends with LLDPEAdditives: Good heat sealing latitude, Moderate toughness, E..
|
|||
| Secant Modulus, MD | 0.150 GPa | 21.8 ksi | at 1%; ASTM D882 |
|
NOVA Chemicals Novapol® LA-0218-AF LDPE Foam Resin
(discontinued **)
Good heat sealing latitude, Moderate toughness, Easy processabilityApplications: Specifically designed for foam process, Blends with LLDPEAdditives: Base resinFilm properties are typical of blown fi..
|
|||
| Secant Modulus, MD | 0.150 GPa | 21.8 ksi | ASTM D882 |
|
Eastman 5251 LDPE 4% VA Copolymer, High Clarity, High Impact Film Resin for Laminations
(discontinued **)
Resin Type: VA CopolymerCharacteristics: Excellent adhesion, Excellent processability and bubble stability, High slip and antiblock, Good impact strengthApplications:Laminations, Heavy produce and s..
|
|||
| Secant Modulus, MD | 0.150 GPa | 21.8 ksi | ASTM D882 |
|
Eastman 5254 LDPE 4% VA Copolymer, High Clarity, High Impact Film Resin for Laminations
(discontinued **)
Resin Type: VA CopolymerCharacteristics: Good adhesion, Good processability and bubble stability, Low slip, Medium antiblock, Good optical properties, Good impact strengthApplications:Laminations, H..
|
|||
| Secant Modulus, MD | 0.150 GPa | 21.8 ksi | ASTM D882 |
|
Eastman 5272 LDPE 4% VA Copolymer, High Clarity, High Impact Film Resin
(discontinued **)
Resin Type: VA CopolymerCharacteristics: Good impact strength, Good bubble stability, Low coefficient of friction, Medium antiblock, Medium slip, Good low temperature properties, Good heat seal char..
|
|||
| Secant Modulus, MD | 0.150 GPa | 21.8 ksi | ASTM D882 |
|
Eastman 5274 LDPE 4% VA Copolymer, High Clarity, High Impact Film Resin
(discontinued **)
Resin Type: VA CopolymerCharacteristics: Good impact strength, Good bubble stability, Low coefficient of friction, High antiblock, Medium slip, Good low temperature properties, Good heat seal charac..
|
|||
| Secant Modulus, MD | 0.150 GPa | 21.8 ksi | ASTM D882 |
|
ExxonMobil Escorene® LD-302 EVA Film Resin, High Clarity, High Impact
(discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 3.4% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit ..
|
|||
| Secant Modulus, MD | 0.150 GPa | 21.8 ksi | ASTM D882 |
|
ExxonMobil Escorene® LD-303 EVA Film Resin, Clarity, High Impact
(discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, clarity film resin. The low melt index and comonomer context of this resin help produce films with superior impact ..
|
|||
| Secant Modulus, MD | 0.150 GPa | 21.8 ksi | ASTM D882 |
|
ExxonMobil Escorene® LD-312 EVA Film Resin, High Impact
(discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 4.6% vinyl acetate copolymer resin for films with good toughness. This resin's low melt index and comonomer content help produce films which exhi..
|
|||
| Secant Modulus, MD | 0.150 GPa | 21.8 ksi | ASTM D882 |
|
ExxonMobil Escorene® LD-314 EVA Packaging Film Resin
(discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 3.5% vinyl acetate copolymer resin for higher clarity films. Film made from LD-314 offers good impact strength, heat sealability, and low tempera..
|
|||
| Secant Modulus, MD | 0.150 GPa | 21.8 ksi | ASTM D882 |
|
ExxonMobil Escorene® LD-325 EVA Film Resin, High Clarity, High Impact
(discontinued **)
Data provided by the manufacturer, Exxon Chemical.A 3.8% vinyl acetate copolymer, high clarity film resin. The combination of low melt index and comonomer content helps produce films which exhibit ..
|
|||
| Secant Modulus, MD | 0.150 GPa | 21.8 ksi | 5%; ASTM D882 |
|
Petroquimica Triunfo Trithene® CX 8087 MDPE - Cast Film
The Trithene CX 8087 resin is a medium density polyethylene (MDPE) with medium molecular weight that presents excellent balance between mechanical properties, processability and stiffness, allowing ..
|
|||
| Secant Modulus, MD | 0.150 GPa | 21.8 ksi | ISO 527-3 |
|
Borealis Borsoft™ SD233CF High Impact Polypropylene Random Heterophasic Copolymer for Cast Film
Borsoft SD233CF is a very soft random heterophasic copolymer, suitable for use on chill roll process. The product combines unique softness with outstanding mechanical properties making it the ideal..
|
|||
| Secant Modulus, MD | 0.150 GPa | 21.8 ksi | 1%; ASTM D882 |
|
Braskem LL 218/21 LLDPE Blown Film Extrusion Polyethylene
38µm film gauge, obtained in 40mm extruder, with blow up ratio 2, 2:1Applications: Automatic packaging (FFS); "liners"; general purpose; HDPE and LDPE blends. Information provided by Braskem
|
|||
| Secant Modulus, MD | 0.150 GPa | 21.8 ksi | 2% Secant Modulus; ASTM-D882 |
|
Braskem TX7001 LDPE Blown Film Extrusion Polyethylene
TX7001 is a low-density polyethylene (LDPE) with high molecular weight designed to satisfy those applications that require high mechanical strength and environmental stress cracking resistance (ESCR..
|
|||
| Secant Modulus, MD | 0.150 GPa | 21.8 ksi | ASTM D882 |
|
Chevron Phillips Vytek™ V208A3 Enhanced LLDPE Blown Film Resin
(discontinued **)
Resin Type: enhanced linear low density polyethylene, slip, antiblock and processing aid additivesCharacteristics: excellent dart impact, hot-tack and heat seal properties, good drawdown, can be use..
|
|||
| Secant Modulus, MD | 0.150 GPa | 21.8 ksi | ASTM D882 |
|
NOVA Chemicals Novapol® LF-0218-AF LDPE Extrusion Resin
(discontinued **)
Film Properties. Features: Good heat sealing latitude, moderate toughness, easy processability.Applications: Specifically designed for foam process, blends with LLDPE.Data provided by the manufactu..
|
|||
| Secant Modulus, MD | 0.150 - 0.896 GPa | 21.8 - 130 ksi | Average value: 0.425 GPa Grade Count:5 |
|
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Impact Modified; Molded/Extruded". Each property range of values reported is minimum and ..
|
|||