Polymer Property : Flexural Modulus = 0.00538 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Modulus 0.00538 GPa
0.780 ksi
1% secant; ASTM D790
ExxonMobil ENABLE™ EN 33900 Adhesive and Sealant Applications Resin  (discontinued **)
Enable EN 33900 is a high flow, 32.5% nBA copolymer suitable for use in hot melt adhesives and sealants.Information provided by ExxonMobil Chemical
Flexural Modulus 0.00538 - 4.35 GPa
0.780 - 631 ksi
Average value: 1.49 GPa Grade Count:35
Overview of materials for Ethylene Butyl Acrylate
This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Butyl Acrylate". Each property range of values reported is minimum and maximum values of approp..