Mechanical Properties Metric English Comments
Flexural Modulus 0.896 GPa
130 ksi
Tangent; ASTM D790
RheTech Products P601-01 Polypropylene Copolymer, Black
Applications: Engine componentChassis componentConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 0.896 GPa
130 ksi
ASTM D790
Ravago Manufacturing Americas Hylon® N1000THL Nylon 6/6 (DAM)
Information provided by Ravago.
Flexural Modulus 0.896 GPa
130 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Eastman M3007-P Polyethylene  (discontinued **)
M3007-P is suggested for applications such as spiral-wound can linings, release paper, and photographic paper. M3007-P Has been found to exhibit good barrier properties, temperature resistance, and..
Flexural Modulus 0.896 GPa
130 ksi
ASTM D790
LNP Lubricomp® FL-4410 Polyetherimide, Silicone Lubricant Additive  (discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
Flexural Modulus 0.896 GPa
130 ksi
Tangent; ASTM D790
Fiberfil® PP-61/VO Polypropylene Copolymer, Flame Retardant, UL94 V0
Information provided by FIBERFIL Engineered Plastics
Flexural Modulus 0.896 GPa
130 ksi
ASTM D790
Fibre Glast 90L Isophthalic Polyester Resin (Laminate Properties)
Description:#90 Isophthalic Polyester Resin is perfect for making dimensionally stable polyester molds, corrosive service part fabrication, and as a durable repair material for tank linings. #90 per..
Flexural Modulus 0.896 GPa
130 ksi
ASTM D790
Techmer ES Luriblend® TPX-HDPE-99018
Availability: North AmericaForms: Pellets)Features: Good Wear Resistance and Low FrictionProcessing Method: Injection MoldingTPCI# 8869115Information provided by TP Composites, Inc.
Flexural Modulus 0.896 GPa
130 ksi
ASTM D790
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene
DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman...
Flexural Modulus 0.896 GPa
130 ksi
ASTM D790-90
Lubrizol Stat-Rite® X-5111 Static Control Polypropylene
Stat-Rite® X-5111 is a static dissipative Polypropylene alloy. Stat-Rite® X-5111 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ES..
Flexural Modulus 0.896 GPa
130 ksi
ASTM D790
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene
DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman...
Flexural Modulus 0.896 GPa
130 ksi
1% secant; ASTM D790
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of..
Flexural Modulus 0.896 GPa
130 ksi
ASTM D790
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene
DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman...
Flexural Modulus 0.896 GPa
130 ksi
Westlake MC3016 High Density Polyethylene Coating
Westlake MC3016 is a high density polyethylene designed for extrusion coating and lamination applications. MC3016 provides improved barrier properties, temperature resistance, stress crack resistanc..
Flexural Modulus 0.896 GPa
130 ksi
ASTM D790
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene
DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman...
Flexural Modulus 0.896 GPa
130 ksi
ASTM D 790
Total PPC 5724 Polypropylene, Extra High Impact Copolymer
ATOFINA 5724 is characterized by a high fluidity offering a combination of processing and excellent impact properties in applications ranging from industrial to household.ApplicationATOFINA 5724 has..
Flexural Modulus 0.896 GPa
130 ksi
1% secant; ASTM D790
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of..
Flexural Modulus 0.896 GPa
130 ksi
1% secant; ASTM D790
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of..
Flexural Modulus 0.896 GPa
130 ksi
ISO 178
ExxonMobil HDPE HMA 016 High Density Polyethylene Resin
Product Description: HMA 016 is a HDPE grade, characterized by fast cycling and good impact strength. It has high gloss and high dimensional stability.Availability: Africa & Middle East, Asia Pacifi..
Flexural Modulus 0.896 GPa
130 ksi
ISO 178
ExxonMobil HDPE HMA 018 High Density Polyethylene Resin
Product Description: HMA 018 is an easy flow HDPE grade, characterized by high gloss and dimensional stability. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Thermal Stabili..
Flexural Modulus 0.896 GPa
130 ksi
CMW® ELKONITE® 3W3 Tungsten Copper material ASTM B702
For arcing and current carrying electrical contacts, power transformer contacts, resistance welding electrodes.Information provided by CMW Inc.
Flexural Modulus 0.896 GPa
130 ksi
1% Secant; ASTM D790
ExxonMobil HD 8660.29 Rotational Molding Resin
Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o..
Flexural Modulus >= 0.896 GPa
>= 130 ksi
ASTM D790
Buckeye Polymers BP PPC 0220 BLK Polypropylene Copolymer
Product Information: Black Polypropylene Copolymer good for general purpose programs requiring moderate impact resistance.Product Features:Good impact resistanceGood UV resistanceGood chemical resis..
Flexural Modulus 0.896 GPa
130 ksi
1% secant; ASTM D790
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of..
Flexural Modulus 0.896 GPa
130 ksi
Tangent; ASTM D790
RheTech Products E204-00 High Density Polyethylene, Natural
Applications: Electrical housingsUnderhood componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 0.896 GPa
130 ksi
1% Secant; ASTM D790
Chevron Phillips HiD® 9330T HDPE Natural Pipe Resin  (discontinued **)
Resin Type: Gas Phase Linear Hexene CopolymerASTM D 4976 Classification: PE 235, A 54607ASTM D3350 Classification: 335540AApplications: Base resin for use in utility and conduit pipe applications.Da..