| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 0.900 GPa | 131 ksi | |
|
Plastcom SLOVALEN EH 96 FRD 2 PP, flame retardant
FeaturesDetermined for environment, where contact with water is possible, because the electric properties do not change by conditioning. Application - terminals, coil forms, guides in washing machin..
|
|||
| Flexural Modulus | 0.900 GPa | 131 ksi | ASTM D790 |
|
Reliance Industries Relene B56003 Polyethylene
Relene B56003 is a High Density Polyethylene grade suitable for general purpose extrusion blow molding applications. Articles blown from this grade exhibit good stiffness. The resin offers good me..
|
|||
| Flexural Modulus | 0.900 GPa | 131 ksi | 3 pt. secant. ASTM D790 |
|
Chevron Phillips HiD® 9396T HDPE Natural Pipe Resin
(discontinued **)
Resin Type: Linear Copolymer; ASTM D 3350 Classification: 345420A; ASTM D 4976 Classification: PE 235, A 56601Applications:Base Resin for use in Utility and Conduit Pipe ApplicationsData provided by..
|
|||
| Flexural Modulus | 0.900 GPa | 131 ksi | 3 pt. secant. ASTM D790 |
|
Chevron Phillips HiD® 9398T HDPE Natural Pipe Resin
(discontinued **)
Resin Type: Linear Copolymer; ASTM D 3350 Classification: 345420A; ASTM D 4976 Classification: PE 235, A 56601Applications:Base Resin for use in Utility and Conduit Pipe ApplicationsData provided by..
|
|||
| Flexural Modulus | 0.900 GPa | 131 ksi | ASTM D790 |
|
Reliance Industries Relene L60075 Polyethylene
Relene L60075 is UV stabilized. It is available with a recommended service life of more then 5 years L60075 is suitable for applications where articles are exposed to sunlight e.g. soft drink crates..
|
|||
| Flexural Modulus | 0.900 - 11.4 GPa | 131 - 1650 ksi | Average value: 3.28 GPa Grade Count:12 |
|
Overview of materials for Nylon 46, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
|
|||
| Flexural Modulus | >= 0.900 GPa | >= 131 ksi | ASTM D790 |
|
Forever Plast Namtene® Recycled Standard HDPE
Standard Namtene® is used for dimple sheet, plastic slabs, and agricultural and construction applications.
|
|||
| Flexural Modulus | 0.900 GPa | 131 ksi | ISO 178 |
|
Iran Petrochemical (PCC) EP2C 37 F Polypropylene
EP2S 37 F offers good process ability, excellent clarity and gloss and exhibits very good heat weld ability.Applications: packaging of stationery, packaging of food stuffs, lamination.Information pr..
|
|||
| Flexural Modulus | 0.900 GPa | 131 ksi | ASTM D790 |
|
Kaneka PHBH Semi-Rigid Bio-based Polymer
A copolymer produced of 3-hydroxybutyrate and 3-hydroxyhexanoate produced by fermentation of plant oils. It has excellent biodegradability (under anaerobic, aerobic, aquatic, and compost conditions..
|
|||
| Flexural Modulus | 0.900 GPa | 131 ksi | DIN 53457 |
|
Schwartz Technical Plastics LAMIGAMID® 710 High Density Polyethylene
Application: chain-guides, cutting plates, linersInformation provided by Schwartz Technical Plastics GmbH
|
|||
| Flexural Modulus | 0.900 GPa | 131 ksi | ISO Data |
|
Styrolution Styrolux 3G55 SBC
Styrolux 3G55 is a thermoplastic styrene-butadiene block copolymer which is suitable for film and sheet extrusion, and thermoforming. It offers and outstanding combination of crystal clarity and ex..
|
|||
| Flexural Modulus | 0.900 GPa | 131 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics LNP THERMOCOMP TF002 PU
LNP* THERMOCOMP* TF002 is a compound based on Polyurethane resin containing 10% Glass Fiber.
|
|||
| Flexural Modulus | 0.900 GPa | 131 ksi | ASTM D790 |
|
SCG Chemicals EL-Leneâ„¢ H1000PYL High Density Polyethylene Pipe Resin
Key Characteristics: Good processing, high thermal stability, good resistance to weatheringRecommended Applications: Stripe lines for PE100 pipe, non pressure pipesCertification: Certified by LNE..
|
|||
| Flexural Modulus | 0.900 GPa | 131 ksi | ASTM D790 |
|
SCG Chemicals EL-Leneâ„¢ S10 Butene (C4) Rotational Molding Resin
Color compound resin available in pellet / powder formKey Characteristics:Excellent stiffnessFair impact resistanceFair processingTypical Applications: High-load/High performance products, such as ..
|
|||
| Flexural Modulus | 0.900 GPa | 131 ksi | at 70°C, tangent |
|
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
|
|||
| Flexural Modulus | 0.900 GPa | 131 ksi | ISO 178 |
|
Unipetrol PE HD LITEN® MB/ML 62 HDPE
Made for injection molding applications.Information provided by Unipetrol RPA
|
|||
| Flexural Modulus | 0.900 GPa | 131 ksi | ASTM D790 |
|
A. Schulman POLYFORT™ PP 7001
Information provided by A. Schulman.
|
|||
| Flexural Modulus | 0.900 GPa | 131 ksi | ISO 178 |
|
Unitika A1030BRL PA6, Conditioned
Information provided by Unitika Ltd.
|
|||
| Flexural Modulus | 0.900 GPa | 131 ksi | at 70°C, tangent |
|
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
|
|||
| Flexural Modulus | 0.900 GPa | 131 ksi | ISO 179 |
|
Total PPM R020 Polypropylene, Random Copolymer for Medical Grade
Polypropylene PPM R020 is a random copolymer polypropylene with a Melt Flow Index of 1.8 g/10 min specially developed for the extrusion blow molding of medical containers and medical devices, to the..
|
|||
| Flexural Modulus | 0.900 GPa | 131 ksi | at 70°C, tangent |
|
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
|
|||
| Flexural Modulus | 0.900 GPa | 131 ksi | 1.3 mm/min at 70°C |
|
A. Schulman POLYPUR™ FPU 1380 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
|
|||
| Flexural Modulus | 0.900 GPa | 131 ksi | 3 pt. secant. ASTM D790 |
|
Chevron Phillips Marlex® 9346 HDPE Natural Pipe Resin
Resin Type: Linear Copolymer; PE3408 Pipe Resin; ASTM D 3350 Classification:345464C when used with an approved color concentrate; ASTM D 4976 Classification: PE 235, A 56607Applications:Pressure Pip..
|
|||
| Flexural Modulus | 0.900 GPa | 131 ksi | 1% Secant; ASTM D 790 |
|
Chevron Phillips Marlex® 9503HF High Performance Series HDPE Blow Molding Resin
Resin Type: linear copolymerCharacteristics: outstanding ESCR, excellent impact resistance, medium molecular weight distribution, wide range of processing conditions, high melt strength, good pariso..
|
|||
| Flexural Modulus | 0.900 GPa | 131 ksi | SAE J949 |
|
Azdel SuperLite® SL551200-100 PP Resin Matrix / 55% Glass Fiber (5 mm Molded Thickness)
AZDEL SuperLite® SL551200-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic..
|
|||
| Flexural Modulus | 0.900 GPa | 131 ksi | ASTM D790 |
|
Carmel Olefins CAPILENE® QM 45 F Propylene Random Copolymer
Description: CAPILENE® QM 45 F is a slip and anti-block formulated random copolymer. It is characterized by high gloss and easy processing.Applications: CAPILENE® QM 45 F is suitable for cast u..
|
|||
| Flexural Modulus | 0.900 GPa | 131 ksi | ASTM D790 |
|
Asahi Glass Fluon® ETFE
A thermoplastic fluoropolymer developed by Asahi Glass. It is a copolymer comprising of tetrafluoroethylene and ethylene. Fluon® ETFE is a balanced fluoropolymer that has chemical resistance and el..
|
|||
| Flexural Modulus | >= 0.900 GPa | >= 131 ksi | ASTM D790 |
|
Centro Plastica CiPiTENE® Recycled High Density Polyethylene Granules
Bottle Grade. Source: Italian post-consumer plastic bottles coming from collection of municipal waste and selected by PE/PP matrix.
|
|||
| Flexural Modulus | 0.900 GPa | 131 ksi | 80x10x4 mm specimen, 2 mm/min; ISO 178 |
|
Solvay Engineered Polymers DEXFLEX® 980HF TPO
(discontinued **)
Description: DEXFLEX® 980HF is a thermoplastic olefinic elastomer (TPO) designed for large automotive exterior applications that require high flow for excellent processability, ductile impact prope..
|
|||
| Flexural Modulus | 0.900 GPa | 131 ksi | 1.3 mm/min at 70°C |
|
A. Schulman POLYPUR™ FPU 1380 Thermoplastic Polyurethane Compound