| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 1.10 GPa | 160 ksi | Tangent; ASTM D790 |
|
RheTech Products P256-674UV Polypropylene Copolymer, UV Stabilized, 447B Fawn
Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Flexural Modulus | 1.10 GPa | 160 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
|
Network Polymers NPP 50-1060
Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc.
|
|||
| Flexural Modulus | 1.10 GPa | 160 ksi | ISO 178 |
|
Premix Thermoplastics PRE-ELEC® PE 1296 Conductive Thermoplastic Compound
PRE-ELEC® PE 1296 is a conductive thermoplastic masterbatch/compound based on PE-HD. Conductivity is achieved by using special conductive carbon black. PRE-ELEC® PE 1296 has a high concentration o..
|
|||
| Flexural Modulus | 1.10 GPa | 160 ksi | 0.05 in/min; 1% secant; Procedure A; ASTM D790 |
|
Phillips 66 COPYLENE® CR350LN Polypropylene, Random Copolymer
COPYLENE™ CR350LN is a high flow random copolymer nucleated and with antistat for good mold release in injection molding applications. Applications: Containers, Closures, HousewaresInformation prov..
|
|||
| Flexural Modulus | 1.10 GPa | 160 ksi | 1% secant; ASTM D790A |
|
Reliance Industries Repol B400MN Polypropylene
REPOL Polypropylene B400MN is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly..
|
|||
| Flexural Modulus | 1.10 GPa | 160 ksi | 0.05 in/mm, 1% Secant, Procedure A; ASTM D790 |
|
Phillips 66 COPYLENE® CM200LN Polypropylene Impact Copolymer
COPYLENE™ CM200LN has a superior balance of stiffness and impact strength. The high melt flow allows for quick filling of molds and the antistat and nucleation facilitates fast cycle times.Applicat..
|
|||
| Flexural Modulus | 1.10 - 17.9 GPa | 160 - 2600 ksi | Average value: 7.09 GPa Grade Count:96 |
|
Overview of materials for Nylon 6, Glass Fiber Filled, Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Fiber Filled, Flame Retardant". Each property range of values reported is minimum and max..
|
|||
| Flexural Modulus | 1.10 GPa | 160 ksi | ISO 178 |
|
LyondellBasell Pro-faxâ„¢ SG899 Polypropylene Copolymer
Description: Pro-faxâ„¢ SG899 high flow, high impact polypropylene copolymer resin is tailored for use in automotive interior head impact applications. This resin is designed to be run in convent..
|
|||
| Flexural Modulus | 1.10 GPa | 160 ksi | ASTM D790 |
|
M. Holland Company CP310 Polypropylene Impact Copolymer
Impact CopolymerMedium flowHigh impact resistanceApplications: ClosuresInformation provided by M. Holland
|
|||
| Flexural Modulus | 1.10 GPa | 160 ksi | Tangent; ASTM D790 |
|
Flint Hills AP6412-HS Impact Copolymer Polypropylene
High impact copolymer, and FDA compliant. Features: Blush resistant and heat stabilized.Applications: Injection molding: consumer durables, automotive interior trim, furniture trim and housing, and ..
|
|||
| Flexural Modulus | 1.10 GPa | 160 ksi | ASTM D790A |
|
Ineos N12N-00 Polypropylene Impact Copolymer
Grade N12N-00 is a nucleated polypropylene impact copolymer with an excellent balance of stiffness and impact resistance for injection molding applications and compounding products used in Lawn and ..
|
|||
| Flexural Modulus | 1.10 GPa | 160 ksi | ASTM D790 |
|
Iran Petrochemical (PCC) 5030UA High Density Polyethylene
HD-5030UA is a high-density polyethylene copolymer grade with a narrow molecular weight distribution, specially developed for injection molding application requiring very high environmental stress c..
|
|||
| Flexural Modulus | 1.10 GPa | 160 ksi | 1.3 mm/min, tangent; ASTM D790 |
|
A. Schulman PP 1930L-01 Polypropylene Copolymer Polypropylene
DescriptionPolypropylene PP 1930L-01 is an impact grade of polypropylene for use in parts which require good impact and good appearance in light weight injection molded parts. Information provided b..
|
|||
| Flexural Modulus | 1.10 GPa | 160 ksi | 1% Secant; ASTM D790 |
|
Plastics Group Polifil® RP-PP Polypropylene, Black
Polifil® RP-PP reprocessed polypropylene has the highest stiffness of the commodity olefin resins, while retaining sufficient impact properties for many applications. Due to its low cost and low de..
|
|||
| Flexural Modulus | 1.10 GPa | 160 ksi | ASTM D790 |
|
A. Schulman POLYFORT™ PP 3719 Impact Copolymer Polypropylene
DescriptionPolyfort® PP 3719 is a UV stabilized impact copolymer polypropylene compound. Information provided by A. Schulman.
|
|||
| Flexural Modulus | 1.10 GPa | 160 ksi | ASTM D790 |
|
Elastomer Engineering Elastamide 150 Elastomer Modified RIM Nylon 6
29% crystallinity. Information supplied by Elastomer Engineering.
|
|||
| Flexural Modulus | 1.10 GPa | 160 ksi | ASTM D790 |
|
A. Schulman POLYFORT™ PP 3719 Impact Copolymer Polypropylene
DescriptionPolyfort® PP 3719 is a UV stabilized impact copolymer polypropylene compound. Information provided by A. Schulman.
|
|||
| Flexural Modulus | 1.10 GPa | 160 ksi | 1.3mm per min, 1% secant; ASTM D790 |
|
Formosa Plastics Formolene® 6501A Blow Molding and Injection Molding Polypropylene
Impact CopolymerApplications: Blow molded bottles and containers, blown and cast film applications, and profile extrusions such as corrugated board.Formolene 6501A is a medium impact copolymer with ..
|
|||
| Flexural Modulus | 1.10 GPa | 160 ksi | ASTM D790 |
|
A. Schulman POLYFORT™ PP 3719 Impact Copolymer Polypropylene
DescriptionPolyfort® PP 3719 is a UV stabilized impact copolymer polypropylene compound. Information provided by A. Schulman.
|
|||
| Flexural Modulus | 1.10 GPa | 160 ksi | 2% Secant; ASTM D790 |
|
ExxonMobil HD 6719.62 Injection Molding Resin
Product Description: HD 6719 is a narrow molecular weight hexane copolymer designed for a wide rage of injection molding applications, combining easy processability with good toughness properties. I..
|
|||
| Flexural Modulus | 1.10 GPa | 160 ksi | 2% Secant; ASTM D790B |
|
ExxonMobil HDPE HD 6719.17 High Density Polyethylene Copolymer Resin
Product Description: HD 6719 is a narrow molecular weight hexane copolymer designed for a wide rage of injection molding applications, combining easy processability with good toughness properties. I..
|
|||
| Flexural Modulus | 1.10 GPa | 160 ksi | 2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 B |
|
Dow DMDA-8904 NT 7 High Density Polyethylene Resin
DOW DMDA-8904 NT 7 is produced using UNIPOL™ process technology. It is intended for use in injection molding applications such as pails, industrial parts and other shipping containers. Information..
|
|||
| Flexural Modulus | 1.10 GPa | 160 ksi | ISO 178 |
|
Eurostar Starflam PF0023E PA6, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam PF0023E is a Mineral Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Flexural Modulus | 1.10 GPa | 160 ksi | ASTM D790 |
|
Clariant Renol PA2SP0004 Nylon 6 Alloy
Data provided by Clariant Masterbatches
|
|||
| Flexural Modulus | 1.10 GPa | 160 ksi | 2% Secant; ASTM D790 |
|
ExxonMobil HD 6706.17 Injection Molding Resin
Product Description: HD 6706 is a narrow molecular weight hexane copolymer designed for good processability and excellent balance of ESR, Toughness and Stiffness properties. This resin is ideally su..
|
|||
| Flexural Modulus | 1.10 GPa | 160 ksi | .05 in/min, 1% Secant; ASTM D790 |
|
Amco PRIMATOP PP CO 005NB Fractional Melt Polypropylene Copolymer
Features:heat aging resistanceimpact resistancelow temperature melt strengthgood stiffnessApplications:containerspipestoysextrusion coatingFormer A-Top Polymers product; part of Amco product line si..
|
|||
| Flexural Modulus | 1.10 GPa | 160 ksi | ASTM D790 |
|
Buckeye Polymers BP Flex D8020 UC85 TPO
TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a..
|
|||
| Flexural Modulus | 1.10 GPa | 160 ksi | ASTM D790 |
|
Asahi Kasei Thermofil P-9900-1760 Unreinforced, Heat Stabilized, Impact Modified
Information provided by Asahi Thermofil
|
|||
| Flexural Modulus | 1.10 GPa | 160 ksi | ASTM D790 |
|
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 13% Plasticizer
(discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
|
|||
| Flexural Modulus | 1.10 GPa | 160 ksi | ASTM D790 |
|
Albis Plastics Cellulose Acetate Butyrate B908 , 13% Plasticizer
(discontinued **)
Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T..
|
|||