Mechanical Properties Metric English Comments
Flexural Modulus 1.24 GPa
180 ksi
Tangent; ASTM D790
RheTech Products FRP256-00 Polypropylene Copolymer, Flame Retardant, Natural
Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 1.24 GPa
180 ksi
Tangent; ASTM D790
RheTech Products FT4500-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black
Applications: Automotive componentsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 1.24 GPa
180 ksi
Tangent; ASTM D790
RheTech Products FT4802-690UVA Thermoplastic Polyolefin, UV Stabilized, HS5 Medium Dark Neutral
Applications: Bodyside moldings and claddingsFacia and bumper coversExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
PolyOne Maxxam™ FR PP FR 7A11 Polypropylene, Unspecified (PP, Unspecified)
Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V..
Flexural Modulus 1.24 GPa
180 ksi
Tangent; ASTM D790
RheTech Products RCC233-01 33% Calcium Carbonate Reinforced Polypropylene Copolymer, Black, Recycled Content
Applications: Fender linersSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 1.24 GPa
180 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Network Polymers NPP 50-0753
Description: High Density Polyethylene (HDPE)Information provided by Network Polymers Inc.
Flexural Modulus 1.24 GPa
180 ksi
ASTM D 790
NOVA Chemicals Sclair® 19C (High Gloss) HDPE Blow Molding Resin
19C complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food, without te..
Flexural Modulus 1.24 GPa
180 ksi
0.05 in/min; 1% secant; Procedure A; ASTM D790
Phillips 66 COPYLENE® CM500LN Polypropylene, Impact Copolymer, High Flow, Medium Impact, Nucleated, Lube, Injection Molding
COPYLENE™ CM500LN is a very high melt flow, medium impact polypropylene copolymer resin, designed for injection molding applications requiring a good balance of properties with faster cycling capab..
Flexural Modulus 1.24 GPa
180 ksi
3 pt. Tangent; ASTM D790
Chevron Phillips HiD® 9035 HDPE Injection Molding Resin  (discontinued **)
Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 231, A 52600Characteristics: Excellent Flow, Moderate Impact Strength, Good Stiffness, Moderate ESCR, Excellent Shrinkage ResistanceAppli..
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
Formosa Plastics Formolene® HP5221 Pipe HDPE  (discontinued **)
High Density Hexene Copolymer Formolene® HP5221 is a high performance copolymer that is designed for the most demanding requirements of corrugated pipe applications. Formolene® HP5221 meets the re..
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
Albis Plastics Cellulose Acetate Propionate CP808 (FDA), 10% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and ..
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
Honeywell Aegis™ PL56HS High Viscosity, Heat Stabilized, Flexible Nylon 6/66 Copolymer  (discontinued **)
Description: Aegis PL56HS is a high viscosity, heat stabilized, flexible nylon 6/66 copolymer. It possesses a balance of flexibility, toughness and abrasion resistance. Combined with its high melt v..
Flexural Modulus 1.24 GPa
180 ksi
1% Secant; ASTM D790
Flint Hills P4C5T-013 Homopolymer Polypropylene
Homopolymer, UL certified, and FDA compliant.Features: Antistat, and controlled rheology.Applications: Injection molding: general purpose.Former Huntsman polypropylene products are now produced by F..
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
Techmer ES HiFill® HDPE TM20 20% Talc Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 20% Filler by WeightInformation provided by TP Composites, Inc.
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790-92
Lubrizol Stat-Rite® M-690 Static Control PETG Alloy
Stat-Rite® M-690 is a static dissipative PETG alloy. Stat-Rite® M-690 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protectio..
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
A. Schulman PP 3052X-01 Polypropylene Impact Resistant Copolymer
DescriptionPolypropylene PP 3052X-01 is an extra high flow impact resistant copolymer with relatively high stiffness. Information provided by A. Schulman.
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
A. Schulman PP 828S-01 Polypropylene Medium Impact Molding Grade Polypropylene
DescriptionPolypropylene PP 828S-01 is a medium impact molding grade created for applications needing good impact and higher H.D.T., such as tote bins, automotive ducting and housings. Information p..
Flexural Modulus 1.24 GPa
180 ksi
1% Secant; ASTM D 790
Chevron Phillips Marlex® 9512H - 9513H High Performance Series HDPE Blow Molding Resin
Resin Type: linear copolymerCharacteristics: excellent physical properties, medium molecular weight distribution, wide range of processing conditions, good flow for injection blow molding applicatio..
Flexural Modulus 1.24 GPa
180 ksi
chs 0.05 in/min; tangent; ASTM D790
Diamond Polymers NPP30-3500F Homopolymer Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Flexural Modulus 1.24 GPa
180 ksi
CMW® THERMKON® 62 Tungsten Copper parts
For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc.
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
Quadrant EPP Proteus® White Homopolymer Polypropylene (ASTM Product Data Sheet)
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
Ravago Manufacturing Americas Echo® RPEHD BK HDPE
Available in North AmericaDescription: Fractional Melt Recycled Content: Yes Color: Black Form: Pellets Information provided by Entec
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
Asahi Kasei Thermofil P-10CC-Y488 10% Calcium Carbonate Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790-92
Lubrizol Stat-Rite® SIS535 Static Control System
Product Description: Stat-Rite® SIS535 is a static dissipative HIPS alloy. Stat-Rite SIS535 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, perma..
Flexural Modulus 1.24 GPa
180 ksi
1.3mm per min, 1% secant; ASTM D790
Formosa Plastics Formolene® 4100N Injection Molding Polypropylene
Homopolymer with ESCR AdditivesApplications: Closures, small appliances, housewares and toys.Formolene 4100N is a medium viscosity, highly isotactic polypropylene homopolymer designed for various in..