| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 1.30 GPa | 189 ksi | |
|
Plastcom SLOVALEN PH 91 N PP, basic type
FeaturesCompounded homopolymer PP. General use in all industry branches. Packing material, garden flower-pots, toys, furniture industry, guides, dowels, clamps, office chairs, holders etc. Delivered..
|
|||
| Flexural Modulus | 1.30 GPa | 189 ksi | Tangent; 1.3 mm/min; ASTM D790 |
|
Mytex Polymers AS66K-01 Polypropylene, Talc filled, Compounded
Description: Talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology.Key Applications: General purpose interiorInformation provided by Mytex Polym..
|
|||
| Flexural Modulus | 1.30 - 1.70 GPa | 189 - 247 ksi | ASTM D790-04 |
|
Proto3000 Objet Digital Materials™ DM_4510 Polypropylene-like Prototyping Polymer
Primary material: DurusWhiteSecondary material: VeroWhitePlus, VeroBlue, VeroBlack or FullCure720Digital Materials are made up of two Objet materials. The two materials are combined in specific conc..
|
|||
| Flexural Modulus |
1.30
GPa @Temperature 23.0 °C |
189
ksi @Temperature 73.4 °F |
ISO 178 |
|
Polykemi AB POLYfill PPC 12000 Polypropylene Copolymer
Information provided by Polykemi AB
|
|||
| Flexural Modulus | >= 1.30 GPa | >= 189 ksi | ASTM D790 |
|
NIZHNEKAMSKNEFTEKHIM PP 1401D (Q30P) Propylene Homopolymer
Product obtained by polymerization of propylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation resistance when P..
|
|||
| Flexural Modulus | 1.30 GPa | 189 ksi | 1% secant at 0.05 in/min; ASTM D790A |
|
LyondellBasell Pro-fax PD702NW Polypropylene Homopolymer, Nucleated/Antistat
Primary Processing Method: Injection MoldingKey Features: nucleated and antistatic, high flow polypropylene homopolymer resin, FDA acceptable, short cycle time for high productivity, resists dust pi..
|
|||
| Flexural Modulus | 1.30 GPa | 189 ksi | ISO 178 |
|
LyondellBasell Hifaxâ„¢ CB228 Thermoplastic Olefin Resin
Key Features: medium melt flow, medium high modulus, paintable thermoplastic elastomeric olefin resin, excellent impact and stiffness balance, good paintability, good processabilityApplications: aut..
|
|||
| Flexural Modulus | 1.30 GPa | 189 ksi | ISO 178 |
|
LyondellBasell Hostacomâ„¢ CB189FC/1 Thermoplastic Polyolefin Elastomer
Description: Hostacomâ„¢ CB189FC/1 medium melt flow, 1,300 MPa flexural modulus, precolored, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of impact, stiffne..
|
|||
| Flexural Modulus | 1.30 GPa | 189 ksi | ISO 178 |
|
Solvay TECHNYL® A 402H1 Natural PA66, Conditioned
Description: TECHNYL® A 402H1 is an unreinforced polyamide 66, very high viscosity, heat stabilized, for extrusion and injection molding. This product is available in natural color.Benefits: The ..
|
|||
| Flexural Modulus | 1.30 GPa | 189 ksi | DIN 53457 |
|
Schwartz Technical Plastics LAMIGAMID® 410 Cast Polyamide 6, Elastomer Modified, Low Temp, Dry
Application: outrigger floats, rollersInformation provided by Schwartz Technical Plastics GmbH
|
|||
| Flexural Modulus | 1.30 GPa | 189 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP LUBRICOMP SP003 PA12 (Europe-Africa-Middle East)
LNP* LUBRICOMP* SP003 is a compound based on PA 12 resin containing PTFE/Silicone. Added features include: Internally Lubricated.
|
|||
| Flexural Modulus | 1.30 GPa | 189 ksi | |
|
SPS Guang Zhou SAMATâ„¢ 666(f1) Flame-retarded Polypropylene
Characteristic: Flame retardance, weather resistance, good mechanical propertiesApplications: X'mas decorative product, E/E applianceInformation Provided by SPS (Guang Zhou) Ltd.
|
|||
| Flexural Modulus | 1.30 GPa | 189 ksi | ISO 178 |
|
Suzhou Hipro Polymers Hiprolon® 400 NN Nylon, dry
Hiprolon® 400 NN is a medium viscosity specialty polyamide. Features: low density, low water absorption, high dimension stability, high notched impact resistance in large temperature ranges, and..
|
|||
| Flexural Modulus | 1.30 GPa | 189 ksi | ASTM D790 |
|
SCG Chemicals EL-Leneâ„¢ H570P High Density Polyethylene Pipe Resin
Key Characteristics: High stiffness, good processingRecommended Applications: Corrugated pipes, non pressure pipes, conduit, sewage drainage pipesInformation provided by SCG Chemicals
|
|||
| Flexural Modulus | 1.30 GPa | 189 ksi | 2mm/min; ISO 178 |
|
Borealis BA202E Polypropylene Block Copolymer for Non-Pressure Pipes
BA202E is a high molecular weight, low melt flow rate polypropylene block copolymer with very high impact strength. Applications: BA202E is recommended for non-pressure pipes & fittings, thin-walled..
|
|||
| Flexural Modulus | 1.30 GPa | 189 ksi | ASTM D790 |
|
Lubrizol Pellethane® 2363-75D Thermoplastic Polyurethane Elastomer
Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
|
|||
| Flexural Modulus | 1.30 GPa | 189 ksi | ASTM D790 |
|
A. Schulman PP 3475-01 Polypropylene High Melt Homopolymer Polypropylene
DescriptionPolypropylene PP 3475-01 Natural is a high melt homopolymer polypropylene with consistent general purpose homopolymer characteristics. Information provided by A. Schulman.
|
|||
| Flexural Modulus | 1.30 GPa | 189 ksi | ISO 527-2 |
|
Total Lumicene® MR 2002 Polypropylene, Metallocene Polypropylene
ATOFINA Polypropylene MR 2002 is a metallocene polypropylene, and is characterized by high fluidity for high speed spinning on spun laid non-woven lines where spun filaments are produced to form a w..
|
|||
| Flexural Modulus | 1.30 GPa | 189 ksi | ASTM D790 |
|
A. Schulman POLYFORT™ PP 3045
Information provided by A. Schulman.
|
|||
| Flexural Modulus | 1.30 GPa | 189 ksi | ASTM D790 |
|
Total PPC 4920WZ Polypropylene, Impact Copolymer
TOTAL Petrochemicals Polypropylene 4920WZ is a nucleated impact copolymer with a Melt Flow index of 105 g/10 min.TOTAL Polypropylene 4920WZ is characterized by excellent stiffness and impact resista..
|
|||
| Flexural Modulus | 1.30 GPa | 189 ksi | ASTM D790 |
|
A. Schulman PP 3475-01 Polypropylene High Melt Homopolymer Polypropylene
DescriptionPolypropylene PP 3475-01 Natural is a high melt homopolymer polypropylene with consistent general purpose homopolymer characteristics. Information provided by A. Schulman.
|
|||
| Flexural Modulus | 1.30 GPa | 189 ksi | ISO 178 |
|
ExxonMobil PP1064L1 Polypropylene Homopolymer
Product Description: A homopolymer resin designed for general use. It is suitable for masterbatch carrier and other compounding applications and for the molding of caps, cups, containers and other ..
|
|||
| Flexural Modulus | 1.30 GPa | 189 ksi | cond; ISO 178 |
|
DSM EcoPaXX® Q-X07290 PA410-I
Impact Modified
|
|||
| Flexural Modulus | 1.30 GPa | 189 ksi | 50%RH; ISO 178 |
|
DuPont Performance Polymers Zytel® 103FHS NC010 Nylon 66
(Unverified Data**)
Unreinforced Heat Stabilized Polyamide 66 Zytel 103FHS NC010 is a heat stabilized internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivi..
|
|||
| Flexural Modulus | 1.30 GPa | 188 ksi | 2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 B |
|
Dow UNIVAL™ DMDH-6400 NT 7 High Density Polyethylene Resin (HDPE)
Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 2.2 UNIVAL™ DMDH-6400 NT 7 is a multipurpose polymer designed for producing containers used to package dairy, water and fruit drinks. In a..
|
|||
| Flexural Modulus | 1.30 GPa | 189 ksi | Dry; ISO 178 |
|
Arkema Group Orgalloy® LE 6000 Polyamide 6 Alloy
Polyamide Alloy, Semi-Flexible grade, Nylon 6 basedTubes / Mandrels / Profiles / CablesInformation provided by Arkema Group
|
|||
| Flexural Modulus | 1.30 GPa | 189 ksi | ASTM D790 |
|
Buckeye Polymers BP Flex D9010 UC85 TPO
TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resistance and have a..
|
|||
| Flexural Modulus | 1.30 GPa | 189 ksi | ASTM D790 |
|
A. Schulman ComAlloy Comtuf® 608 Nylon 6/12, Impact Modified
Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc..
|
|||
| Flexural Modulus | 1.30 GPa | 189 ksi | ASTM D790 |
|
A. Schulman POLYFORT™ PP 3045