| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus |
10.4
GPa @Temperature 23.0 °C |
1510
ksi @Temperature 73.4 °F |
ISO 178 |
|
Polykemi AB SCANAMID 66 A53^ F43 Nylon 66, Glass Fiber Reinforced, Modified
Information provided by Polykemi AB
|
|||
| Flexural Modulus |
10.4
GPa @Temperature 23.0 °C |
1510
ksi @Temperature 73.4 °F |
ISO 178 |
|
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA)
(Unverified Data**)
Amodel AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Typical applications include ..
|
|||
| Flexural Modulus | 10.4 GPa | 1510 ksi | ASTM D790 |
|
Plenco 51240 PET, Pellet, Injection Molded, Green
(discontinued **)
PLENCO 51240 is an engineering grade glass reinforced flame retarded recycled polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed.Information supplied by P..
|
|||
| Flexural Modulus | 10.4 GPa | 1510 ksi | ASTM D790 |
|
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK)
(Unverified Data**)
AV-742 SL30 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wear re..
|
|||
| Flexural Modulus | 10.4 GPa | 1510 ksi | ISO 178 |
|
Idemitsu Kosan Xarec® EA 528 SPS, 30% Glass Filled
(discontinued **)
Crystalline Polymer, Glass Filled, Ignition Resistant, Impact Modified. Used in Electronic and Electrical applications
|
|||
| Flexural Modulus | 10.4 GPa | 1510 ksi | ASTM D790 |
|
Mitsui AURUM® JGN6230 Thermoplastic Polyimide Resin, Crystalline
(discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
|
|||
| Flexural Modulus | 10.4 GPa | 1510 ksi | ASTM D790 |
|
Plenco 506 Black Heat Resistant Mineral Filled Phenolic Molding Compound
(discontinued **)
Plaslok 506 is a two-stage, mineral-filled phenolic molding compound. It is formulated for automotive ashtrays and for appliance applications such as utensil handles receiving repeated exposure to ..
|
|||
| Flexural Modulus | 10.4 GPa | 1510 ksi | ASTM D790 |
|
Plaslok 506 Black Heat Resistant Mineral Filled Phenolic Molding Compound
(discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 506 is a two-stage, mineral-filled ph..
|
|||
| Flexural Modulus | 10.4 GPa | 1510 ksi | 5 mm/min; ISO 178 |
|
Gromax BFG45-DN00N1 Nylon 6 46% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.
|
|||
| Flexural Modulus | 10.4 GPa | 1510 ksi | ISO 178 |
|
Solvay Specialty Polymers Amodel® HFZ A-1133 L Polyphthalamide (PPA), 33% Glass Fiber
Amodel® HFZ A-1133 L is a high-flow, 33% glass fiber reinforced polyphthalamide (PPA) grade.Features: Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Stiffness; ..
|
|||
| Flexural Modulus | 10.4 GPa | 1510 ksi | ASTM D790 |
|
Solvay Specialty Polymers AvaSpire® AV-742 SL30 Polyaryletherketone (PAEK)
AV-742 SL30 is a wear resistant grade of AvaSpire® polyaryletherketone (PAEK) designed to provide low wear rates in both non-lubricated and lubricated environments. In addition to outstanding wea..
|
|||
| Flexural Modulus | 10.4 GPa | 1510 ksi | ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP LF008 PEEK
LNP* THERMOCOMP* LF008 is a compound based on Polyetheretherketone resin containing 40% Glass Fiber.
|
|||
| Flexural Modulus | 10.4 GPa | 1510 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics LNP THERMOCOMP RF008 PA 66 (Asia Pacific)
LNP Thermocomp RF008 is a compound based on PA66 resin containing glass fiber. It is used in many applications requiring high strength over weight performance. Also known as Thermocomp RF-1008
|
|||
| Flexural Modulus | 10.4 GPa | 1510 ksi | ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP LF008 PEEK (Asia Pacific)
LNP* Thermocomp* LF008 is a compound based on Polyetheretherketone resin containing Glass Fiber.
|
|||
| Flexural Modulus | 10.4 GPa | 1510 ksi | ASTM D790 |
|
A. Schulman SCHULAMID® 66 GF33HS 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66
Information provided by A. Schulman.
|
|||
| Flexural Modulus | 10.4 GPa | 1510 ksi | ASTM D790 |
|
A. Schulman SCHULAMID® 66 GF33HS 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66
Information provided by A. Schulman.
|
|||
| Flexural Modulus | 10.4 GPa | 1510 ksi | ISO 178 |
|
Polyplastics FR-PET® B3030FA Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose
Information provided by PolyPlastics.
|
|||
| Flexural Modulus | 10.4 GPa | 1510 ksi | ISO 178 |
|
Polyplastics FR-PET® C3030FA Glass Fiber Reinforced Polyethylene Terephthalate (GF-PET), Slow burning, General purpose
Information provided by PolyPlastics.
|
|||
| Flexural Modulus | 10.4 GPa | 1510 ksi | ASTM D790 |
|
A. Schulman SCHULAMID® 66 GF33HS 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66
Information provided by A. Schulman.
|
|||
| Flexural Modulus | 10.4 GPa | 1510 ksi | ASTM D790 |
|
A. Schulman SCHULAMID® 66 GF33HS 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66
Information provided by A. Schulman.
|
|||
| Flexural Modulus | 10.4 GPa | 1510 ksi | ASTM D790 |
|
A. Schulman SCHULAMID® 66 GF33HS 33% Glass Fiber Reinforced, Heat Stabilized Nylon 66
Information provided by A. Schulman.
|
|||
| Flexural Modulus | 10.4 GPa | 1510 ksi | dry; ISO 178 |
|
DSM Novamid® 3010GN30 NAT PA66-GF30 FR(17)
30% Glass Reinforced, Flame Retardant
|
|||
| Flexural Modulus | 10.4 GPa | 1510 ksi | 2 mm/min; ISO 178 |
|
Eurostar Starflam RF0077E PA66, 35% Glass Filled, Injection Molded
Starflam RF0077E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Polyamide 66 Injection Molding Resin (also known as RF1007Z270)Information provided by Polymer T..
|
|||
| Flexural Modulus | 10.4 GPa | 1510 ksi | ASTM D790 |
|
Ashley Polymers Ashlene® 528L-43G Nylon 66, 43% Glass Reinforced
A general purpose 43% glass reinforced nylon resin.Data provided by the manufacturer
|
|||
| Flexural Modulus | 10.4 GPa | 1510 ksi | Dry; ASTM D790 |
|
Asahi Kasei Leona® 14G33 33% Glass Filled Nylon 66
Enhanced strength and stiffness; with 33% GF. Superior heat aging resistance, fatigue resistance, and creep resistance.Applications:Mechanical and electrical parts, engine mounts and other under-the..
|
|||
| Flexural Modulus | 10.4 GPa | 1510 ksi | ASTM D790 |
|
Ashley Polymers Ashlene® 990L-50G Nylon 610, 50% Glass Reinforced
50% glass reinforced, excellent dimensional stability and low water absorption. Also available as: 990LS-50G, same with heat stabilizer.Data provided by the manufacturer
|
|||
| Flexural Modulus |
10.4
GPa @Temperature 23.0 °C |
1510
ksi @Temperature 73.4 °F |
ISO 178 |
|
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer
Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp..
|
|||
| Flexural Modulus |
10.4
GPa @Temperature 23.0 °C |
1510
ksi @Temperature 73.4 °F |
ISO 178 |
|
Solvay Specialty Polymers Amodel® HFZ A-1133 L Polyphthalamide (PPA)
(Unverified Data**)
Amodel® HFZ A-1133 L is a high-flow, 33% glass fiber reinforced polyphthalamide (PPA) grade. Natural: HFZ A-1133 L NT Black: HFZ A-1133 L BK 937Information provided by Solvay Specialty Polymers.
|
|||
| Flexural Modulus |
10.4
GPa @Temperature 23.0 °C |
1510
ksi @Temperature 73.4 °F |
ISO 178 |
|
Solvay Specialty Polymers Amodel® A-4133 L Polyphthalamide (PPA), Dry
(discontinued **)
Amodel A-4133L polyphthalamide (PPA) is a 33% glass reinforced resin designed to offer high crystallinity when molded in water-cooled molds. Key properties include high heat resistance, reduced outg..
|
|||