| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 6.89 GPa | 1000 ksi | ASTM D790 |
|
Polymer Resources NY66-IMG33 Nylon, 33% Glass Reinforced, Impact Modified (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Flexural Modulus | 6.89 GPa | 1000 ksi | ASTM D790 |
|
Polymer Resources TP-FRHG30 Polybutylene Terephthalate, 30% Glass Reinforced Alloy, Flame Retardant
Polybutylene Terephthalate, 30% Glass Reinforced Alloy, Flame RetardantProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s..
|
|||
| Flexural Modulus | 6.897 GPa | 1000 ksi | ASTM D790 |
|
Ravago Manufacturing Americas Hylex® P1310G30 HB Polycarbonate, 30% Fiberglass Reinforced, UV Stabilized
Information provided by Ravago.
|
|||
| Flexural Modulus | 6.89 GPa | 1000 ksi | ASTM D790 |
|
PolyOne Lubri-Tech™ PS-30GF/15T Polybutylene Terephthalate (PBT), Glass Filled, PTFE Lubricated
(discontinued
Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||
| Flexural Modulus | 6.90 - 23.5 GPa | 1000 - 3410 ksi | Average value: 16.2 GPa Grade Count:4 |
|
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled". Each property range of values reported ..
|
|||
| Flexural Modulus | 6.89 GPa | 1000 ksi | ASTM D790 |
|
PolyOne Edgetek® AS-30GF/000 FRVO Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **)
Description/Features:Glass Fiber ReinforcedFlame RetardantUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
|
Plenco 201 Black General Purpose Woodflour/Mineral Filled Phenolic Molding Compound
(discontinued **)
Plaslok 201 is a two-stage, woodflour and mineral-filled phenolic molding compound formulated to have an excellent balance of molded properties. The material provides good electrical insulation val..
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
|
Plaslok 309 Black (INJ) Mineral/Fiber Filled Phenolic Molding Compound
(discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 309 is a two-stage, mineral and fiber..
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | |
|
Haysite ETS-FR-II Glass Reinforced Polyester Sheet, Electrical Grade (GPO2)
A NEMA GPO-2 glass mat reinforced thermoset polyester molded sheet. ETS-FR-II is UL recognized with a flame rating of 94V-0 and arc resistance of 185 seconds. This grade is an IEEE Thermal Class B, ..
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | DIN 53452; ASTM D790 |
|
Kolon Kopa® KN163G30 Nylon 6 Resin
KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c..
|
|||
| Flexural Modulus | 6.89 GPa | 1000 ksi | ASTM D790 |
|
Techmer ES HiFill® ABS 1067
Availability: North AmericaFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High DensityForms: PelletsProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
|
|||
| Flexural Modulus | 6.89 GPa | 1000 ksi | ASTM D790 |
|
Techmer ES HiFill® PA6 GB36 IM1 BK 36% Glass Bead Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 36% Filler by WeightAdditive: Lubricant Features: LubricatedAppearance: BlackInformation provided by TP Composites, Inc.
|
|||
| Flexural Modulus | 6.89 GPa | 1000 ksi | ASTM D790 |
|
Techmer ES HiFill® PA6 GF20 L BK 20% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by Weight Processing: Method: Injection MoldingInformation provided by TP Composites, Inc.
|
|||
| Flexural Modulus | 6.89 GPa | 1000 ksi | ASTM D790 |
|
Techmer ES HiFill® PA6/6 GF/M40 HS Up BK 40% Glass/Mineral Fiber Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by Weight and Mineral Filler, 40% Filler by WeightAdditive: Lubricant, UV Stabilizer and Heat Sta..
|
|||
| Flexural Modulus | 6.89 GPa | 1000 ksi | ASTM D790 |
|
Techmer ES Elastoblend® PA6/6 GF33 IM HS L BKN 33% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 33% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri..
|
|||
| Flexural Modulus | 6.89 GPa | 1000 ksi | ASTM D790 |
|
Techmer ES HiFill® PA6 0425
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforFeatures: High Specific GravityInformation provided by TP Composites, Inc.
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | ISO 178 |
|
Borealis Nepol™ GB601HP Polypropylene, 30% Long Glass Fiber Reinforced w/BJ356MO
Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat..
|
|||
| Flexural Modulus | 6.89 GPa | 1000 ksi | ASTM D790 |
|
Chase Plastics CP Pryme® PC330GR Polycarbonate (Utility Grade), 30% Glass Fiber Reinforced, Mold Release
Information provided by Chase Plastics.
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
|
Adell AT-37 Nylon 66, 35% Glass Reinforced; Impact Modified
Data provided by Adell Plastics, Inc.
|
|||
| Flexural Modulus | 6.89 GPa | 1000 ksi | Tangent; ASTM D790 |
|
Applied Composites 150 Polyester SMC
Industry Application: TransportationProduct Application: Engine CoversDistinct Features: Grey Pigments Only, Low DensityInformation provided by Applied Composites Corporation.
|
|||
| Flexural Modulus |
6.89
GPa <br>@Temperature 22.8 °C
|
1000
ksi <br>@Temperature 73.0 °F
|
ASTM D790 |
|
Quadrant EPP Duratron® PAI T7530, Compression Molded Carbon Fiber Reinforced Polyamide-Imide |
|||
| Flexural Modulus | 6.89 GPa | 1000 ksi | ASTM D790 |
|
Polymer Resources PPX-G30 Modified PPO, 30% Glass Reinforced
(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
|
|||
| Flexural Modulus | 6.90 GPa | 1000 ksi | ASTM D790 |
|
Plaslok 302 Black Impact Grade Woodflour/Flock Filled Phenolic Molding Compound
(discontinued **)
Plaslok Corporation was purchased by Plastics Engineering Company (maker of Plenco brand materials) in March 2000. The Plaslok name is no longer in use.Plaslok 302 is a two-stage, woodflour and flo..
|
|||