| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 0.740 GPa | 107 ksi | Compression Molded; ASTM D790 |
|
NOVA Chemicals Surpass® RMs539-U Octene sMDPE Rotational Molding Film
Features: Octene copolymerExceptional low temperature impact propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Stan..
|
|||
| Flexural Modulus | 0.740 GPa | 107 ksi | Compression Molded; ASTM D790 |
|
NOVA Chemicals Surpass® RMs539-UG Octene sMDPE Rotational Molding Film
Features: Octene copolymerExceptional low temperature impact propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Stan..
|
|||
| Flexural Modulus | 0.735 GPa | 107 ksi | ASTM D790 |
|
PolyMirae Moplen EP200R Injection Molding Grade Polypropylene
Moplen EP200R is the reactor TPO manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP200R is a super impact copolymer particularly suitable for injection molding of..
|
|||
| Flexural Modulus | 0.740 GPa | 107 ksi | ASTM D790 |
|
BASF Capron® 8200 NL Nylon 6 (Conditioned)
(discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
|
|||
| Flexural Modulus | 0.740 GPa | 107 ksi | ASTM D790 |
|
BASF Capron® 8202 NL Nylon 6 (Conditioned)
(discontinued **)
Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
|
|||
| Flexural Modulus | 0.735 GPa | 107 ksi | ASTM D790 |
|
Hyosung Topilene C500H PP
C500H Butene Random CopolymerApplications: FilmCharacteristics:Excellent transparency & glossLow sealing temperatureHigh hot-tack strengthGood stiffnessInformation provided by Hyosung Corporation
|
|||
| Flexural Modulus | 0.735 GPa | 107 ksi | ASTM D790 |
|
Hyosung Topilene C600H2 PP
C600H2 Butene Random CopolymerApplications: FilmCharacteristics:Excellent transparency & glossLow sealing temperatureHigh hot-tack strengthGood stiffnessInformation provided by Hyosung Corporation
|
|||
| Flexural Modulus | 0.735 GPa | 107 ksi | Olsen Stiffness; ASTM D747 |
|
Global F-8000 High Density Polyethylene
Description-good mechanical strengthApplications-blown wide film applications producing liner film & industrial filmInformation provided by Global Polymers Corporation.
|
|||
| Flexural Modulus | 0.735 GPa | 107 ksi | ASTM D790 |
|
LG Chemical LUTENE-H ME5000 HDPE
Description: LUTENE-H ME5000 is mainly intended for injection molding of containers and bottle cap. It has good stress cracking resistance and high impact strength.Applications: Containers, dust bin..
|
|||
| Flexural Modulus | 0.741 GPa | 107 ksi | |
|
Kuraray SEPTON® PM2 Polypropylene Modified Plastic
Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. using its isoprene technology. SEPTON® resins are a series of hydrogenated styrenic blo..
|
|||
| Flexural Modulus |
0.735
GPa <br>@Thickness 6.40 mm
|
107
ksi <br>@Thickness 0.252 in
|
10mm/min; ASTM D790 |
|
LG Chemical LUPOL TE5007B PP+Rubber, High Impact
Description: Injection Molding, PP+Rubber, Low Density, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia , Rear Bumper Step)Information provided by LG Chemical
|
|||
| Flexural Modulus | 0.738 GPa | 107 ksi | ASTM D790 |
|
Techmer ES HiFill® PA6 L UV (Conditioned)
Availability: North AmericaForms: PelletsAdditive: Lubricant and UV StabilizerFeatures: Lubricated and Good UV ResistanceInformation provided by TP Composites, Inc.
|
|||
| Flexural Modulus |
0.740
GPa <br>@Strain <=0.250 %
|
107
ksi <br>@Strain <=0.250 %
|
ISO 178 |
|
Total MDPE HT 514 Medium Density Polyethylene, Blown Film
MDPE HT 514 is a medium density polyethylene produced by slurry loop low pressure process with hexene as co-monomer.MDPE HT 514 is a semi-high molecular weight polyethylene giving excellent mechanic..
|
|||
| Flexural Modulus | 0.740 GPa | 107 ksi | 2% Secant - 16:1 span:depth, 0.5 in/min; ASTM D-790 |
|
Chevron Phillips Marlex® HMN TR-945/945G Polyethylene; HDPE
High density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and excellent flowLong-term UV stabilizationGood impact stren..
|
|||
| Flexural Modulus | 0.740 GPa | 107 ksi | ASTM Test |
|
BASF Ultramid® 8202 HS PA6 (Conditioned)
Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab..
|
|||
| Flexural Modulus | 0.740 GPa | 107 ksi | ASTM Test |
|
BASF Ultramid® 8202 PA6 (Conditioned)
Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult..
|
|||
| Flexural Modulus |
0.740
GPa <br>@Temperature 120 °C
|
107
ksi <br>@Temperature 248 °F
|
ASTM Test |
|
BASF Ultramid® HPN 9362 40% Mineral Filled PA6 (Conditioned)
Ultramid HPN 9362 is a 40% mineral reinforced, impact modified nylon 6 injection molding compound. It is one of the High Productivity Nylon series having improved surface appearance while reducing c..
|
|||
| Flexural Modulus | 0.738 GPa | 107 ksi | ASTM D790 |
|
Total Lumicene® mPE BM359 SG Metallocene Medium Density High Gloss Blow Molding Resin
Metallocene Medium Density High Gloss Blow Molding ResinCharacteristics:Outstanding glossGood flexibilityExcellent impact strengthGood ESCRUSP Class VI compliantFDA CompliantApplications:Coextruded ..
|
|||
| Flexural Modulus | 0.740 GPa | 107 ksi | |
|
Reliance Industries Reclair Crosslinked R35042
Crosslinkable R35042 is a polyethylene grade that has increased service temperature and toughness, and improved ESCR over Reclair R35042. Crosslinkable R35042 applications include fuel tanks and ch..
|
|||