Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 12.0 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Modulus 12.0 GPa
1740 ksi
ISO 178, ASTM D790
Nilit Nilamid A3 H G8 40% Glass Reinforced PA66
Description: Nilamid A3 H G8 is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance, even at elevated temper..
Flexural Modulus 12.0 GPa
1740 ksi
DIN 53 457
Albis Plastics Tedur® L V 9107-1 PPS, 40% Glass Fiber  (discontinued **)
Low Flash, Improved Impact and Burst Strength. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Pump Housings, Hollow Articles Under PressureProcessing: Injection Moldi..
Flexural Modulus 12.0 GPa
1740 ksi
Lehmann & Voss LUVOCOM® 1105-7828/GY PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Flexural Modulus 12.0 GPa
1740 ksi
Lehmann & Voss LUVOCOM® 1106-7622 Polyether imide, with carbon fiber
Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.High dimensionally stable precision parts.Electrical..
Flexural Modulus 12.0 GPa
1740 ksi
Lehmann & Voss LUVOCOM® 1700-7910 PPO, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
Flexural Modulus 12.0 GPa
1740 ksi
ASTM D790
IDI Composites A-203 Thermoset Polyester, Sheet
AUTOMOTIVE - Versatile family of compounds specifically designed for automotive structural applications. Low shrink characteristics, heat resistance, long-term dimensional stability, and corrosion r..
Flexural Modulus 12.0 GPa
1740 ksi
Haysite H258 Polyester Laminate
Solder Pallet and Work Holder Sheet A high temperature polyester laminate that exhibits excellent retention of mechanical properties and dimensional stability at elevated temperatures. Applications..
Flexural Modulus 12.0 GPa
1740 ksi
Lehmann & Voss LUVOCOM® 1/CF/20 Polyamide 66, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
Flexural Modulus 12.0 GPa
1740 ksi
Haysite HST-II Glass Reinforced Polyester Sheet, Electrical Grade
UL, Inc. has granted HST-II the highest thermal recognition ever achieved by any glass polyester laminate (U.L. File No. E81893). HST-II has a 220º C/210º C rating for 1/8" thick and heavier,..
Flexural Modulus 12.0 GPa
1740 ksi
Lehmann & Voss LUVOCOM® 1104-7598 Polyether ketone, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Improved fatigue properties.Thermic, mechanic and chemical highly str..
Flexural Modulus 12.0 GPa
1740 ksi
GB/T 9341-2008
Sichuan Deyang Haton® hGR302 PPS / F4 Polyphenylene Sulfide
Injection molding, anti-frictionInformation provided by Sichuan Deyang Chemical Co., LTD
Flexural Modulus 12.0 GPa
1740 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® V8280SF PBT+PET
High Modulus, PBT+PET, 40% Glass Reinforced, Mold Release, Super High Flow
Flexural Modulus 12.0 - 14.0 GPa
1740 - 2030 ksi
ISO 178
Vyncolit G885 Novolac Phenolic
Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties. Information provided by Vyncolit, a Sumitomo Bak Group
Flexural Modulus 12.0 - 14.0 GPa
1740 - 2030 ksi
ISO 178
Vyncolit X658 Novolac Phenolic
Glass fiber and mineral filled phenolic molding compound with excellent mechanical and thermal properties and a very good dimensional stability.USES: Complex precision parts.Information provided by ..
Flexural Modulus 12.0 GPa
1740 ksi
ISO 178
Vyncolit X7012 Glass Fiber Reinforced Novolac Phenolic
Novolac resin based, glass fiber and glass beads reinforced. High mechanical strength even at high temperatures in Long Life CoolantsInformation provided by Sumitomo Bak North America, Inc.
Flexural Modulus 12.0 GPa
1740 ksi
ASTM D790
Toyobo VYLOPET® EMC132-01 Injection Molding Polyester Resin, Flame Resistant
Applications: Relay partsFeatures: Excellent arc resistanceFlame resistanceInformation provided by Toyobo.
Flexural Modulus 12.0 GPa
1740 ksi
2 [mm/min]; ISO 178
Akro-Plastic Akromid® A3 GF 40 (1258) PA 6.6 Dry, 40% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Copyright © lookpolymers.com All Rights Reserved