Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 120 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Modulus 0.828 GPa
120 ksi
Method 1, Proc. B; ASTM D-790-95
Multibase Multi-Pro® 0710 C Brown Polypropylene
Data provided by Multibase.
Flexural Modulus 0.827 GPa
120 ksi
Tangent; ASTM D790
RheTech Products FT1002-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 0.827 GPa
120 ksi
Tangent; ASTM D790
RheTech Products FT1002-00A Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Step padsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 0.827 GPa
120 ksi
Tangent; ASTM D790
RheTech Products FT2600-677UV Thermoplastic Polyolefin, UV Stabilized, 0848 Black
Applications: Exterior trimStep pads and hitch padsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 0.827 GPa
120 ksi
Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790
Network Polymers NPP 20-2501 C/AS
Description: Random Copolymer Polypropylene, Clarified, with AntistatInformation provided by Network Polymers Inc.
Flexural Modulus 0.828 GPa
120 ksi
ISO 178/1A
Radici Heraflex® E 7722 TPC-ET Thermoplastic Elastomer
TPC-ET Thermoplastic Elastomer. High Modulus, Nominal Shore D/15s 69. Natural colorProcessing technology: Injection moldingInformation provided by Radici group.
Flexural Modulus 0.827 GPa
120 ksi
ASTM D790
Eastman Tenite Butyrate 513E3720008 Clear, Trsp Cellulose Acetate Butyrate  (discontinued **)
Plasticizer 23%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Flexural Modulus 0.827 GPa
120 ksi
ASTM D790
Honeywell Aegis™ PL165HS High Viscosity, Heat Stabilized, Flexible Nylon 6/66 Copolymer  (discontinued **)
Description: Aegis PL165HS is a high viscosity, heat stabilized, flexible nylon 6/66 copolymer. It possesses a balance of flexibility, toughness and abrasion resistance. Combined with its high melt ..
Flexural Modulus 0.827 GPa
120 ksi
ASTM D790
LTL Color Compounds ColorRxâ„¢ PP2-1002ARX Biocompatible Polypropylene Random Copolymer
A biocompatible approx. 10 melt injection molding grade of Polypropylene random copolymer for healthcare applications.All information provided by LTL Color Compounders, Inc.
Flexural Modulus 0.827 GPa
120 ksi
ASTM D790
Techmer ES HiFill FR® PP CO FR-N
Availability: North AmericaForms: PelletsFeatures: Flame Retardant, High Impact Resistance and CopolymerInformation provided by TP Composites, Inc.
Flexural Modulus 0.827 GPa
120 ksi
ASTM D790
Techmer ES Plastiblend® LDPE E FR V-2
Availability: North AmericaForms: PelletsFeatures: Flame RetardantProcessing Method: ExtrusionInformation provided by TP Composites, Inc.
Flexural Modulus 0.827 GPa
120 ksi
2% secant; ASTM D790
A. Schulman LP544-01 High-Density Copolymer Polyethylene
DescriptionLP 544-01 is a high-density copolymer polyethylene with exceptional ESCR and crush strength combined with good processability for applications including telecommunication ducting, thermof..
Flexural Modulus 0.827 GPa
120 ksi
2% secant; ASTM D790
A. Schulman LP544-01 High-Density Copolymer Polyethylene
DescriptionLP 544-01 is a high-density copolymer polyethylene with exceptional ESCR and crush strength combined with good processability for applications including telecommunication ducting, thermof..
Flexural Modulus 0.827 GPa
120 ksi
2% secant; ASTM D790
A. Schulman LP544-01 High-Density Copolymer Polyethylene
DescriptionLP 544-01 is a high-density copolymer polyethylene with exceptional ESCR and crush strength combined with good processability for applications including telecommunication ducting, thermof..
Flexural Modulus 0.827 GPa
120 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 512 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 512 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi..
Flexural Modulus 0.827 GPa
120 ksi
ASTM D882
A. Schulman LP477-01 High-Density Polyethylene
DescriptionLP 477-01 is a high-density polyethylene possessing excellent impact strength for blow molded bleach and detergent bottles, thermoformed industrial parts, tote boxes, trays, liners and ph..
Flexural Modulus 0.827 GPa
120 ksi
2% secant; ASTM D790
A. Schulman LP544-01 High-Density Copolymer Polyethylene
DescriptionLP 544-01 is a high-density copolymer polyethylene with exceptional ESCR and crush strength combined with good processability for applications including telecommunication ducting, thermof..
Flexural Modulus 0.827 GPa
120 ksi
ASTM D790
Eastman Tenite Butyrate 485A2R30023 Natural, Trsp Cellulose Acetate Butyrate
Plasticizer 23%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Flexural Modulus 0.827 GPa
120 ksi
ASTM D790
Eastman Tenite Butyrate 565A3720023 Clear, Trsp Cellulose Acetate Butyrate
Plasticizer 23%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p..
Flexural Modulus 0.830 GPa
120 ksi
2% Secant; ASTM D790
Chevron Phillips Marlex® H525 High Density Polyethylene, Pressure Pipe Grade
This high performance PE 4710 HDPE is tailored for demanding pressure pipe applications that require:Good long-term hoop strengthGood resistance to slow crack growthExcellent resistance to slumpAddi..
Flexural Modulus 0.827 GPa
120 ksi
0.05 in/min; ISO 178
CTC X-PRO CTC PP 3020 Polypropylene Copolymer
X-PRO PP 3020 is a high melt polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC).
Flexural Modulus 0.827 GPa
120 ksi
1% Secant; molded and tested in accordance with ASTM D 4101; ASTM D790A
Dow 6D43 Polypropylene Resin
DOW 6D43 is intended for use fiber spinning processes.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braskem in July 2011.
Flexural Modulus 0.827 GPa
120 ksi
Dow HDPE 12450N High Density Polyethylene
DOW HDPE 12450N resin is a narrow molecular weight distribution copolymer designed to offer excellent impact strength and toughness with moderate stiffness. This resin has good processability over a..
Flexural Modulus 0.827 GPa
120 ksi
CMW® ELKONITE® 1060 Silver Tungsten Carbide Contact Material
Electrical contactor material for medium current ac applicationsInformation provided by CMW Inc.
Flexural Modulus 0.830 GPa
120 ksi
ASTM D790
Ashley Polymers Ashlene® D926 Nylon 12
A flexible Nylon 12 with exceptional toughness, excellent abrasion and chemical resistance, outstanding low temperature performance, dimensional stability and low moisture absorption. Also availabl..
Flexural Modulus 0.827 GPa
120 ksi
2% secant; ASTM D790
A. Schulman LP544-01 High-Density Copolymer Polyethylene
DescriptionLP 544-01 is a high-density copolymer polyethylene with exceptional ESCR and crush strength combined with good processability for applications including telecommunication ducting, thermof..
Flexural Modulus 0.825 GPa
120 ksi
ASTM D790
A. Schulman POLYFORT™ PP 1329 Medium Impact Copolymer Polypropylene
DescriptionPolyfort® PP 1329 is a medium impact copolymer polypropylene, available in matched automotive colors. Information provided by A. Schulman.
Flexural Modulus 0.827 GPa
120 ksi
1.3mm per min; ASTM D790
Formosa Plastics Formolene® L64220U Rotational Molding LLDPE  (discontinued **)
Linear Low Density Polyethylene Hexene Copolymer for Rotational Molding Formolene® L64220U is a general-purpose rotational molding linear low density resin made using the BP Gas Phase ProcessTM. Th..
Flexural Modulus 0.825 GPa
120 ksi
ASTM D790
A. Schulman POLYFORT™ PP 1329 Medium Impact Copolymer Polypropylene
DescriptionPolyfort® PP 1329 is a medium impact copolymer polypropylene, available in matched automotive colors. Information provided by A. Schulman.
Flexural Modulus 0.827 GPa
120 ksi
1.3mm per min, 1% secant; ASTM D790
Formosa Plastics Formolene® 2620A Impact Copolymer Polypropylene
Impact Copolymer for Compounding and Injection Molded Applications Formolene® 2620A is a high impact copolymer of polypropylene designed for applications such as automotive compounds and lawn & gar..