| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus |
8.80
GPa @Temperature 23.0 °C |
1280
ksi @Temperature 73.4 °F |
ISO 178 |
|
Polykemi AB SCANAMID 66.6 C12^F30 Nylon 66/6, Glass Fiber, Reinforced
Information provided by Polykemi AB
|
|||
| Flexural Modulus |
8.80
GPa @Temperature 23.0 °C |
1280
ksi @Temperature 73.4 °F |
ISO 178 |
|
Polykemi AB SCANMID 6 B12^ F30 Nylon 6, Glass Fiber Reinforced
Information provided by Polykemi AB
|
|||
| Flexural Modulus | 8.82 GPa | 1280 ksi | ASTM D790 |
|
SABIC Innovative Plastics Lexan® LGK4030 PC (Asia Pacific) |
|||
| Flexural Modulus | 8.83 GPa | 1280 ksi | ASTM D790 |
|
LG Chemical LUCON CP-4201F Conductive Thermoplastic, Flame Retardant
LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin..
|
|||
| Flexural Modulus |
8.83
GPa @Thickness 3.20 mm |
1280
ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
|
LG Chemical LUMID GP2251AF PA6+GF25%, Flame Retardant
Feature: Injection Molding, PA6+GF25%, Flame RetardantApplication: IT/OA (Micro Switch)CAS No. 25038-54-4, 65997-17-3, 88497-56-7, 1309-64-4 and 138265-88-0Information provided by LG Chemical
|
|||
| Flexural Modulus |
8.83
GPa @Thickness 6.40 mm |
1280
ksi @Thickness 0.252 in |
2.8mm/min; ASTM D790 |
|
LG Chemical LUMID GP2309A(W) PA6+GF30%, General Purpose
Feature: Injection Molding,PA6+GF30%, General PurposeApplication: Automotive (Cooling Fan)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
|
|||
| Flexural Modulus |
8.83
GPa @Thickness 3.20 mm |
1280
ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
|
LG Chemical LUMID GP2330A(W) PA6+GF33%, General Purpose
Feature: Injection Molding, PA6+GF33%, General PurposeApplication: Automotive (Cooling Fan), E&E (Bobbin)CAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
|
|||
| Flexural Modulus |
8.83
GPa @Thickness 3.20 mm |
1280
ksi @Thickness 0.126 in |
10mm/min; ASTM D790 |
|
LG Chemical LUPOS GP2305A SAN+GF30%, General Purpose
Feature: Injection Molding, SAN+GF30%, General PurposeApplication: Electric & Electronic (Housing, Components)CAS No. 9003-56-9 and 65997-17-3Information provided by LG Chemical
|
|||
| Flexural Modulus | 8.80 GPa | 1280 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP LUBRICOMP EFL36E PEI (Europe-Africa-Middle East)
LNP* Lubricomp* EFL36E is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Easy Molding.
|
|||
| Flexural Modulus | 8.80 GPa | 1280 ksi | ISO 178 |
|
Solvay TECHNYL® R CR 218 V30 Nylon 6, 30% glass fiber, DRY
TECHNYL® CR 218 V30 is a polyamide 6, reinforced with 30% glass fiber, heat stabilized, for injection molding. It contains recycled raw materials. This product is available in black color.Benefit..
|
|||
| Flexural Modulus | 8.80 GPa | 1280 ksi | ISO 178 |
|
SABIC Innovative Plastics LNP Thermocomp DF0069E PC
LNP* Thermocomp* DF0069E is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.This data was supplied by SABIC..
|
|||
| Flexural Modulus | 8.83 GPa | 1280 ksi | ISO 178 |
|
SABIC Innovative Plastics LNP Thermocomp IF006S PA 6/12 (Asia Pacific)
LNP* Thermocomp* IF006S is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Paci..
|
|||
| Flexural Modulus | 8.83 GPa | 1280 ksi | 2.8 mm/min; ASTM D638 |
|
Samsung Cheil Industries Infino® VB-5305G PBT, Glass Filled FR
Information provided by Samsung Cheil Industries.
|
|||
| Flexural Modulus | 8.81 GPa | 1280 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP RX96592 PA 66
LNP* Thermocomp* RX96592 is a compound based on Nylon 6/6 containing Proprietary Fillers.
|
|||
| Flexural Modulus | 8.82 GPa | 1280 ksi | ASTM D790 |
|
SABIC Innovative Plastics LNP LUBRICOMP JX91198 PES
LNP LUBRICOMP* JX91198 is a compound based on Polyethersulfone resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
|
|||
| Flexural Modulus | 8.80 GPa | 1280 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Valox® 830 PBT (Europe-Africa-Middle East)
VALOX 830 is a 30% glass fibre reinforced PBT+PET blend with excellent surface finish. Applications: hot air gun housing assemblies, industrial glue guns, appliance housings and handles.
|
|||
| Flexural Modulus | 8.80 GPa | 1280 ksi | ASTM D790 |
|
Plenco 2535 Phenolic, Granular, Compression Molded
PLENCO 02535 is a general purpose, organic filled phenolic molding compound offering optimized cure characteristics and excellent electrical properties. Type ASTM 5948 CFG, and UL recognized under c..
|
|||
| Flexural Modulus | 8.822 GPa | 1280 ksi | ASTM D790 |
|
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Flexural Modulus | 8.80 GPa | 1280 ksi | ASTM D790 |
|
Plenco 7500 Phenolic, Granular, Compression Molded
PLENCO 07500 is an organic reinforced phenolic molding compound, offering improved mechanical strength and excellent cosmetic characteristics. Type ASTM 5948 CFG and UL recognized under component fi..
|
|||
| Flexural Modulus | 8.822 GPa | 1280 ksi | ASTM D790 |
|
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Flexural Modulus | 8.80 GPa | 1280 ksi | ISO 178-93 |
|
Wellman Wellamid® GF33-66 XE-BKDX9 33% Glass Fiber Reinforced Nylon 66
Description: Glass Fiber Reinforced Nylon 66Information provided by Wellman.
|
|||
| Flexural Modulus | 8.822 GPa | 1280 ksi | ASTM D790 |
|
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Flexural Modulus | 8.822 GPa | 1280 ksi | ASTM D790 |
|
A. Schulman ComAlloy® E-13819 Heat Dissipative PPS
Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Flexural Modulus | 8.83 GPa | 1280 ksi | ISO Data |
|
BASF Petra® 7030 GY6128 30% Glass Filled PET
Petra 7030 GY6128 is a grey pigmented, high flow 30% glass fiber reinforced injection molding compound based on post-consumer and post-industrial recycled polyethylene terephthalate feedstock. It o..
|
|||
| Flexural Modulus | 8.83 GPa | 1280 ksi | 2.8mm/min; ASTM D790 |
|
Asia International Enterprise (Hong Kong) 60G7F Nylon 66, 35% Filled
Information provided by Asia International Enterprise (Hong Kong) Ltd.
|
|||
| Flexural Modulus | 8.83 GPa | 1280 ksi | ISO 178 |
|
SABIC Innovative Plastics LNP Thermocomp IF006S PA6.12
LNP* Thermocomp* IF006S is a compound based on Nylon 6/12 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas ..
|
|||
| Flexural Modulus | 8.83 GPa | 1280 ksi | ASTM D790 |
|
LNP Lubricomp® PDX-J-91198 Polyethersulfone, Proprietary Filler
(discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
|
|||
| Flexural Modulus | 8.83 GPa | 1280 ksi | 2.8 mm/min; ASTM D638 |
|
Samsung Cheil Industries Infino® VB-5300G PBT, Glass Filled FR
Information provided by Samsung Cheil Industries.
|
|||