| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 0.896 GPa | 130 ksi | ASTM D790 |
|
Multibase Multi-Pro® 0612 CW Polypropylene
Calcium carbonate filler, 6% filer by weightForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
|
|||
| Flexural Modulus | 0.896 GPa | 130 ksi | ASTM D790 |
|
Ravago Manufacturing Americas Hylon® N1000THL Nylon 6/6 (DAM)
Information provided by Ravago.
|
|||
| Flexural Modulus | 0.894 - 3.54 GPa | 130 - 513 ksi | Average value: 2.61 GPa Grade Count:69 |
|
Overview of materials for Polystyrene, Molded, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
|
|||
| Flexural Modulus | 0.896 GPa | 130 ksi | 1% Secant; ASTM D 790 |
|
Chevron Phillips HiD® 9330 HDPE Natural Pipe Resin
(discontinued **)
Resin Type: gas phase linear hexane copolymer; ASTM D3350 Classification 335520A; ASTM D4976 Classification: PE 235, A 55701Applications: base resin for use in utility and conduit pipe applicationsI..
|
|||
| Flexural Modulus | 0.896 GPa | 130 ksi | 2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790 |
|
Eastman M3007-P Polyethylene
(discontinued **)
M3007-P is suggested for applications such as spiral-wound can linings, release paper, and photographic paper. M3007-P Has been found to exhibit good barrier properties, temperature resistance, and..
|
|||
| Flexural Modulus | 0.896 GPa | 130 ksi | 2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790 |
|
Eastman M3016-P Polyethylene
(discontinued **)
M3016-P is suggested for applications such as spiral-wound can linings, release paper, and photographic paper. M3016-P Has been found to exhibit good barrier properties, temperature resistance, and..
|
|||
| Flexural Modulus | 0.896 GPa | 130 ksi | ASTM D790 |
|
LNP Lubricomp® FL-4410 Polyetherimide, Silicone Lubricant Additive
(discontinued **)
Features: LubricatedForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still ac..
|
|||
| Flexural Modulus | 0.896 GPa | 130 ksi | Conditioned; ASTM D790 |
|
Ravago Manufacturing Americas Hylon® N1000THLUV2 Polyamide 66
(discontinued **)
Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Lubricated, Heat Stabilized and Good ToughnessRoHS CompliantAuto Specifications: GM GMP.PA66.079 Color: Bla..
|
|||
| Flexural Modulus | 0.897 GPa | 130 ksi | 2% Secant-Method 1; ASTM D790 |
|
Ineos TC46-25 HDPE
TC46-25 is a natural high density polyethylene copolymer designed specifically for telecommunications ducting to meet or exceed the material requirements in ASTM F2160, UL 651B and MEMA TC-7. TC46-..
|
|||
| Flexural Modulus | 0.896 GPa | 130 ksi | ASTM D790-90 |
|
Lubrizol Stat-Rite® X-5111 Static Control Polypropylene
Stat-Rite® X-5111 is a static dissipative Polypropylene alloy. Stat-Rite® X-5111 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ES..
|
|||
| Flexural Modulus | 0.896 GPa | 130 ksi | 1% secant; ASTM D790 |
|
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of..
|
|||
| Flexural Modulus | 0.897 GPa | 130 ksi | ASTM D790 |
|
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene
DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. ..
|
|||
| Flexural Modulus | 0.896 GPa | 130 ksi | ASTM D790 |
|
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene
DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman...
|
|||
| Flexural Modulus | 0.896 GPa | 130 ksi | |
|
Westlake MC2004 High Density Polyethylene Coating
Westlake MC2004 is a high density polyethylene designed for extrusion coating and lamination applications. MC2004 provides improved barrier properties, temperature resistance, stress crack resistanc..
|
|||
| Flexural Modulus | 0.896 GPa | 130 ksi | |
|
Westlake MC3016 High Density Polyethylene Coating
Westlake MC3016 is a high density polyethylene designed for extrusion coating and lamination applications. MC3016 provides improved barrier properties, temperature resistance, stress crack resistanc..
|
|||
| Flexural Modulus | 0.896 GPa | 130 ksi | ASTM D 790 |
|
Total PPC 5724 Polypropylene, Extra High Impact Copolymer
ATOFINA 5724 is characterized by a high fluidity offering a combination of processing and excellent impact properties in applications ranging from industrial to household.ApplicationATOFINA 5724 has..
|
|||
| Flexural Modulus | 0.896 GPa | 130 ksi | ASTM D790 |
|
A. Schulman PP 1498-01 Polypropylene Medium Impact Copolymer Polypropylene
DescriptionPolypropylene PP 1498-01 is a high flow, medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. Schulman...
|
|||
| Flexural Modulus | 0.897 GPa | 130 ksi | ASTM D790 |
|
A. Schulman POLYFORT™ PP 1498HU UV Stabilized, Medium Impact Copolymer Polypropylene
DescriptionPolyfort® PP 1498HU is a high flow UV stabilized medium impact copolymer polypropylene. It molds easily at low temperatures, pressures and mold cycle times. Information provided by A. ..
|
|||
| Flexural Modulus | 0.896 GPa | 130 ksi | ISO 178 |
|
ExxonMobil HDPE HMA 018 High Density Polyethylene Resin
Product Description: HMA 018 is an easy flow HDPE grade, characterized by high gloss and dimensional stability. Availability: Africa & Middle East, Asia Pacific and Europe Additive: Thermal Stabili..
|
|||
| Flexural Modulus | 0.896 GPa | 130 ksi | 1% Secant; ASTM D790 |
|
ExxonMobil HDP8660.29 Rotational Molding Resin
Product Description: HD 8660 series are high density hexane copolymers designed to offer superior toughness and stiffness. They are ideally suited for applications that require the optimum balance o..
|
|||
| Flexural Modulus | >= 0.896 GPa | >= 130 ksi | ASTM D790 |
|
Buckeye Polymers BP PPC 0220 BLK Polypropylene Copolymer
Product Information: Black Polypropylene Copolymer good for general purpose programs requiring moderate impact resistance.Product Features:Good impact resistanceGood UV resistanceGood chemical resis..
|
|||
| Flexural Modulus | 0.896 GPa | 130 ksi | 1% secant; ASTM D790 |
|
A. Schulman LP551-01 Narrow Molecular Weight Copolymer, High-Density Polyethylene
DescriptionLP551-01 is a narrow molecular weight copolymer, high-density polyethylene combining excellent impact strength with good environmental stress crack resistance. ApplicationApplications of..
|
|||
| Flexural Modulus | 0.896 GPa | 130 ksi | Tangent; ASTM D790 |
|
RheTech Products E204-00 High Density Polyethylene, Natural
Applications: Electrical housingsUnderhood componentsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Flexural Modulus |
0.896
GPa @Temperature 175 °C |
130
ksi @Temperature 347 °F |
ISO 178 |
|
Solvay Specialty Polymers Amodel® A-1240 L Polyphthalamide (PPA)
(discontinued **)
Amodel A-1240 L is a 40% mineral filled polyphthalamide (PPA) that offers low warpage and excellent dimensional stability. This resin also has a high deflection temperature, flexural modulus and ten..
|
|||
| Flexural Modulus | 0.896 - 2.30 GPa | 130 - 334 ksi | Average value: 1.52 GPa Grade Count:39 |
|
Overview of materials for Polypropylene, Sheet/Thermoforming Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Sheet/Thermoforming Grade". Each property range of values reported is minimum and maximum..
|
|||