Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 1310 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Modulus 9.00 GPa
1310 ksi
ASTM D790
Premix Premi-Glas® 2200-20 CR-SX Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2200-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Pigmentable for molded-in c..
Flexural Modulus 9.00 GPa
1310 ksi
ASTM D790
Premix Premi-Glas® 2205-20 CRSX Polyester SMC
Premi-Glas® 2205-20 CR-SX is a 20% fiberglass reinforced Sheet Molding Compound formulated for condensate pan applications requiring chemical resistance, heat resistance, dimensional stability, we..
Flexural Modulus 9.00 GPa
1310 ksi
ASTM D790
Premix Premi-Glas® 3140-22 Fiberglass Reinforced Thermoset Thick Molding Compound
Premi-Glas® 3140-22 is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves glass..
Flexural Modulus 9.00 GPa
1310 ksi
ASTM D790
Premix Premi-Glas® 3200-20 Fiberglass Reinforced SMC
Description: Premi-Glas® 3200-20 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di..
Flexural Modulus 9.00 GPa
1310 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics EXTEM XH2315 TPI Resin (Europe-Africa-Middle East)
Extem XH2315 Resin
Flexural Modulus 9.00 GPa

@Temperature 23.0 °C
1310 ksi

@Temperature 73.4 °F
ISO 178
Polykemi AB SCANAMID 66 A13^ F30 Nylon 66, Glass Fiber Reinforced
Information provided by Polykemi AB
Flexural Modulus 9.04 GPa
1310 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP KONDUIT PX11311 PA 6 (Asia Pacific)
Thermally conductive mineral filled PA6 FR compound
Flexural Modulus 9.00 GPa
1310 ksi
ISO 178
PolyOne Nymax™ ND 1233 GF Black Polyamide 66 (Nylon 66)
The Nymax® GF 1200 Series of glass fiber-reinforced nylon 6/6 compounds have been specifically formulated for applications requiring high stiffness, tensile properties, heat resistance, and durabil..
Flexural Modulus 9.00 GPa
1310 ksi
Lehmann & Voss LUVOCOM® 1-8491 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.High dimensionally stab..
Flexural Modulus 9.00 GPa
1310 ksi
Lehmann & Voss LUVOCOM® 19-8094 Polyamide 46, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
Flexural Modulus 9.00 GPa
1310 ksi
Lehmann & Voss LUVOTECH® MR 1025 BK Polyamide 66, with mineral filler
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Low warpage.Isotropic shrinkage characteristics.Information provided by Lehmann & Voss & Co.KG
Flexural Modulus 9.00 GPa
1310 ksi
2mm/min; ASTM D790
Kingfa PBT-RG301 Flame Retardant, 30% Glass Fiber Reinforced PBT
Features:Flame retardantHigh mechanical strengthHigh heat resistanceGood electric propertiesNo bloomingApplications:Injection moldingHousehold appliance partsBobbinLighting partsRelayLinkerInformati..
Flexural Modulus 9.00 GPa

@Temperature 22.0 °C
1310 ksi

@Temperature 71.6 °F
25 mm wide 100 mm long, flat samples; ISO 14125
Menzolit Menzolit® SMC 0430 Unsaturated Polyester UP
SMC 0430 is a low emission Class-A SMC for on-line painted exterior body applications on passenger cars. These compounds mould to parts with excellent surface quality for on-line painted body panel..
Flexural Modulus 9.00 GPa
1310 ksi
Lehmann & Voss LUVOCOM® 1104-7452 Polyether ketone, with glass fiber, easy flowing
Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Improved fatigue properties.Thermic, mechanic and chemical highly str..
Flexural Modulus 9.00 GPa
1310 ksi
ASTM D790
Loxim 433 01HB Nylon 6,6
Information provided by Loxim Industries
Flexural Modulus 9.00 GPa
1310 ksi
Lehmann & Voss LUVOCOM® 1100-7890 Polyether sulfone, with carbon fiber
Applications: Apparatus- and precision engineering, film- and photo industry, sporting- and leisure goods, medical- and electrical enineering, aircraft- and aerospace industry.High dimensionally sta..
Flexural Modulus 9.06 GPa
1310 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® IQ507 PBT+PC (Europe-Africa-Middle East)
Valox iQ507 resin: Environmentally responsible, sustainable, and low carbon footprint resin that is 30% glass fiber reinforced PBT+PC alloy. Valox iQ507 offers good mechanical and thermal characte..
Flexural Modulus 9.00 GPa
1310 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP STAT-KON ZX08301 PPE (Asia Pacific)
Stat-Kon* ZX08301 compound is a high heat compounds with ESD safe and low warpage performance suitable for use in Semiconductor Packaging Applications.
Flexural Modulus 9.00 GPa
1310 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Thermocomp RF006XXP PA 66 (Europe-Africa-Middle East)
30% glass fibre reinforced Polyamide 66 injection moulding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Modulus 9.00 GPa
1310 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP Thermocomp RF007S PA 66 (Europe-Africa-Middle East)
LNP* THERMOCOMP* RF007S is a compound based on PA 66 resin containing Glass Fiber . Added features include: Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regi..
Flexural Modulus 9.00 GPa
1310 ksi
ISO 178
Borealis Nepol™ GB601HP Polypropylene, 40% Long Glass Fiber Reinforced w/BJ356MO
Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat..
Flexural Modulus 9.00 GPa
1310 ksi
DAM; ISO 178
DuPont Performance Polymers Zytel® HTN FR52G30NH NC010 Polyphthalamide (PPA)  (Unverified Data**)
30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide Zytel HTNFR52G30NH NC010 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin. It..
Flexural Modulus 9.00 GPa
1310 ksi
2 mm/min; ISO 178
Eurostar Staramide AG6K PA66, 30% Glass Filled, Injection Molded
AG6 is a Heat and Hydrolytically Stabilized, 30% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive suppli..
Flexural Modulus 9.00 GPa
1310 ksi
ASTM D790
E-Polymers TEKAMID® TA250G33 33% Glass Fiber Reinforced PA66, DAM
33% Glass Fiber Reinforced, Good surfaceInformation provided by E-Polymers Co. Ltd.
Flexural Modulus 9.00 GPa
1310 ksi
Longitudinal direction; ISO 178
Azdel Plus U421B02N 42% Directionalized Continuous Fiber Mat / PP Resin Matrix
AZDEL® U421B02N is a uni-directional fiber and random glass mat reinforced polypropylene composite material featuring excellent fiber distribution over long flow paths and complex part forms. This..
Flexural Modulus 9.00 GPa
1310 ksi
ASTM D790
Ashley Polymers Ashlene® 528L-33G Nylon 66, 33% Glass Reinforced
General purpose glass fiber reinforced Nylon 66, designed for parts requiring excellent thermal and dimensional stability and higher strength than conventional resins.Data provided by the manufactur..
Copyright © lookpolymers.com All Rights Reserved