| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 9.50 GPa | 1380 ksi | ASTM D790 |
|
Premix Premi-Glas® 1200-10 Fiberglass Reinforced Thermoset SMC
Premi-Glas® 1200-10 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st..
|
|||
| Flexural Modulus | 9.50 GPa | 1380 ksi | ISO 178 |
|
Hexion Bakelite™ PF 2736 Phenolic Formaldehyde Resin, Improved Electrical Properties, Low Shrinkage, UL Listed
&nbs
Phenolic molding compound, inorganically/organically filled, increased tracking resistance, UL listed molding compound 0.46 mm/V-0 (BK, Suffix "H"), 0.81 mm/V-0 (NC, GN, BK), 1.5 mm/V-0 (ALL).Applic..
|
|||
| Flexural Modulus | 9.50 GPa | 1380 ksi | ASTM D790 |
|
Plenco Valite 4100 Novolac Phenolic, Granular, Compression Molded
(discontinued **)
This Valite product has been replaced by Plenco 4100. Data provided by Plenco.VALITE 4100 is a black two stage, medium heat resistant phenolic molding compound. It has excellent moldability charac..
|
|||
| Flexural Modulus | 9.50 GPa | 1380 ksi | |
|
Lehmann & Voss LUVOCOM® 1850/GF/30/TF/13/SI/2 PBT, with glass fiber, PTFE, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.High dimensionally stable prec..
|
|||
| Flexural Modulus | 9.50 GPa | 1380 ksi | ISO 178 |
|
Grupo Repol Dinalon® B1S25 G35 35% Glass Fiber Reinforced Nylon 6
Mechanical properties are for dry as molded samples.Information provided by Grupo Repol.
|
|||
| Flexural Modulus | 9.50 GPa | 1380 ksi | ISO 178 |
|
Solvay TECHNYL® A 218G V33 Black 34N PA66, 25% glass fiber, DRY
Description: Polyamide 66, reinforced with 25% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. Avail..
|
|||
| Flexural Modulus | 9.50 GPa | 1380 ksi | ISO 178 |
|
Solvay TECHNYL® A 30 H1 V30 PA66, 30% glass fiber, DRY
Description: TECHNYL® A 30H1 V30 is a brominated flame retardant polyamide 66, reinforced with 30% of glass fiber, for injection molding. This product is available in natural & black color.Benefi..
|
|||
| Flexural Modulus | 9.50 GPa | 1380 ksi | ISO 178 |
|
Solvay Technyl® C 216 Nylon 6, 30% Glass Fiber, EH0
Polyamide PA6, reinforced with 30% of glass fiber, for injection molding.It has good mechanical properties. It is used in all sectors of industry, offering an excellent combination between thermal ..
|
|||
| Flexural Modulus | 9.50 GPa | 1380 ksi | ISO 178 |
|
Solvay TECHNYL® C 216 V30 PA6, 30% glass fiber, DRY
Description: Polyamide PA6, reinforced with 30 % of glass fiber, for injection molding.Available in: Asia Pacific and Latin AmericaProduct Applications: It has good mechanical properties, it is used..
|
|||
| Flexural Modulus | 9.50 GPa | 1380 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics ULTEM 2410EPR PEI (Asia Pacific)
40% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release for enhanced electroplatability. ECO Conforming, UL94 V0 listing.
|
|||
| Flexural Modulus | 9.50 GPa | 1380 ksi | ISO 178 |
|
SABIC Innovative Plastics LNP STAT-KON DEL339XF PC
LNP* STAT-KON* DEL339XF is a compound based on Polycarbonate resin containing 15% Carbon Fiber, 15% PTFE. Added features include: Electrically Conductive, Flame Retardant, Wear Resistant.
|
|||
| Flexural Modulus | 9.50 GPa | 1380 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Valox® 420SE0 PBT (Europe-Africa-Middle East)
30% glass reinforced, UL94 V-0/5V rated. Numerous applications: edge trimmers, food mixer motor stator and commutator, cooling fan, connectors, bobbins, switches etc
|
|||
| Flexural Modulus | 9.50 GPa | 1380 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Valox® 420SE0U PBT
PBT, 30% Glass Reinforced, Flame Retardant UL94 V-0/5VA rated, UV-Stabilized
|
|||
| Flexural Modulus | 9.50 GPa | 1380 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP DF008ER PC (Europe-Africa-Middle East)
LNP* Thermocomp* DF008ER is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release.
|
|||
| Flexural Modulus | 9.53 GPa | 1380 ksi | ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP PF008S PA 6 (Asia Pacific)
LNP THERMOCOMP* PF008S is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.
|
|||
| Flexural Modulus | 9.50 GPa | 1380 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics NORYL GFN1740V PPE+PS
Noryl* GFN1740V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi..
|
|||
| Flexural Modulus | 9.50 GPa | 1380 ksi | ISO 178 |
|
SABIC Innovative Plastics LNP VERTON RX89047 PA 66
LNP* VERTON* RX89047 is a compound based on Nylon 66 resin containing Proprietary Fillers. Added feature of this grade is: Structural.
|
|||
| Flexural Modulus | 9.50 GPa | 1380 ksi | ASTM D790 |
|
Plenco 4414 Phenolic, Granular, Transfer Molded
PLENCO 04414 is a flock and mineral filled phenolic molding compound. It is formulated for use in electrical applications that require improved heat resistance, mechanical strength, and dimensional ..
|
|||
| Flexural Modulus | 9.50 GPa | 1380 ksi | ISO 178 |
|
Vyncolit 4523 XB Novolac Phenolic
Organic and inorganic filled phenolic molding compound with good mechanical and thermal properties. Improved heat resistance compared to organic filled compounds.USES: Fuse holders, brush holders, ..
|
|||
| Flexural Modulus | 9.50 GPa | 1380 ksi | ASTM D790 |
|
Plenco 4568 Phenolic, Granular, Compression Molded
PLENCO 04568 is a heat resistant, mineral and flock filled, phenolic molding compound, formulated to provide thermal oxidation stability along with excellent dimensional stability. 04568 is availabl..
|
|||
| Flexural Modulus | 9.50 GPa | 1380 ksi | ISO 178 |
|
Unitika TERRAMAC TE-7300 Polylactic Acid (PLA)
Heat-resisting grade, Injection grade. Bio-based materials produced from annually renewable raw materials.Information provided by Unitika Ltd.
|
|||
| Flexural Modulus | 9.50 GPa | 1380 ksi | DAM; ISO 178 |
|
DuPont Performance Polymers Zytel® 70G30HSL BK039B Nylon 66
(Unverified Data**)
30% Glass Reinforced Heat Stabilized Polyamide 66 Information provided by DuPont Performance Polymers
|
|||
| Flexural Modulus | 9.50 GPa | 1380 ksi | 2mm/min; ASTM D790 |
|
Kingfa JE2-R2G30 Glass Fiber Reinforced ABS/PBT Alloy
Features:High stiffness, high hardnessGood mechanical strengthGood chemical resistanceGood size stabilityGood heat stabilityLow tendency to warpApplications:Optical appliance (camera, video)Sports a..
|
|||
| Flexural Modulus |
9.50
-
11.0
GPa <br>@Temperature 80.0 - 80.0 °C
|
1380
-
1600
ksi <br>@Temperature 176 - 176 °F
|
Average value: 10.2 GPa Grade Count:4 |
|
Overview of materials for Polypropylene with 60% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 60% Glass Fiber Filler". Specific grades with glass content between 55% and 64% are i..
|
|||
| Flexural Modulus | 9.50 GPa | 1380 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics NORYL FE1740PW PPE+PS (Europe-Africa-Middle East)
Noryl* FE1740PW Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 40 % Glass Reinforced, injection moldable grade with improved hydrolytic stability and with a Tensile Modulus > 11000 MPa; thi..
|
|||