| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 0.100 GPa | 14.5 ksi | ISO 178 |
|
Polimeri Europa Greenflex® ML 20 Ethylene Vinyl Acetate Copolymer - Injection Molding
Greenflex ML 20 is an ethylene vinyl acetate copolymer (EVA) for injection molding, when a good ESCR is required.Main Applications: Greenflex ML 20 is recommended for the production of flexible ite..
|
|||
| Flexural Modulus | 0.100 GPa | 14.5 ksi | ISO 178 |
|
Polimeri Europa Greenflex® ML 21 Ethylene Vinyl Acetate Copolymer - Injection Molding
Greenflex ML 21 is an ethylene vinyl acetate copolymer (EVA) for injection molding, when a good ESCR is required. Greenflex ML 21 contains additive waxes to obtain high production speed.Main Applic..
|
|||
| Flexural Modulus | 0.100 GPa | 14.5 ksi | ISO 178 |
|
Polimeri Europa Riblene® MY 00 Low Density Polyethylene - Injection Molding
Riblene MY 00 is a very high flowability low density polyethylene resin (LDPE).Main Applications: Riblene MY 00 is suitable for hot melts.Information provided by Polimeri Europa.
|
|||
| Flexural Modulus |
0.100
GPa @Temperature 23.0 °C |
14.5
ksi @Temperature 73.4 °F |
ISO 178 |
|
DuPont Performance Polymers Hytrel® HTR8685 BK022A TPC-ET
(Unverified Data**)
Hytrel® HTR8685 BK022A is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal hardness of 44D, is pigmented black with fine particle size carbon black,..
|
|||
| Flexural Modulus | 0.100 GPa | 14.5 ksi | ASTM D790 |
|
Rotuba M Cellulose Acetate
Property values at 50% RH.Data provided by the manufacturer.
|
|||
| Flexural Modulus | 0.100 GPa | 14.5 ksi | 1% Secant; ASTM D790 |
|
Multibase Multi-Flex® D 3204 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good P..
|
|||
| Flexural Modulus | 0.100 GPa | 14.5 ksi | 1% secant at 0.05 in/min; ASTM D790A |
|
LyondellBasell Astryn CA743GA Polypropylene Copolymer
Key Features: low melt flow, low modulus, UV-stabilized polypropylene copolymer with antiblock, good heat seamability, good puncture resistance, plasticizer-free, excellent low temperature impact re..
|
|||
| Flexural Modulus | 0.100 GPa | 14.5 ksi | Tangent, 0.5 in/min; ASTM D790 |
|
LyondellBasell Hifaxâ„¢ CA10GC Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ CA10GC fractional melt flow, 100 MPa flexural modulus, precolored, UV-stabilized, reactor grade, extrudable thermoplastic elastomeric olefin (TEO) resin combines good proces..
|
|||
| Flexural Modulus | 0.100 GPa | 14.5 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
|
SABIC Innovative Plastics NORYL WCA871A PPE
Flame retardant performance and mechanical properties capable of meeting UL VW-1 requirement and 105C temperature rating as defined UL1581. UL1581 tests conducted on 1.0mmD wire with AWG28 conductor..
|
|||
| Flexural Modulus | 0.100 GPa | 14.5 ksi | 12.5 mm/min; ISO 178 |
|
SABIC Innovative Plastics NORYL WCA871A PPE
Flame retardant performance and mechanical properties capable of meeting UL VW-1 requirement and 105C temperature rating as defined UL1581. UL1581 tests conducted on 1.0mmD wire with AWG28 conductor..
|
|||
| Flexural Modulus | 0.100 GPa | 14.5 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
|
SABIC Innovative Plastics NORYL WCA871A PPE (Asia Pacific)
Flame retardant performance and mechanical properties capable of meeting UL VW-1 requirement and 105C temperature rating as defined UL1581. UL1581 tests conducted on 1.0mmD wire with AWG28 conductor..
|
|||
| Flexural Modulus | 0.100 GPa | 14.5 ksi | 12.5 mm/min; ISO 178 |
|
SABIC Innovative Plastics NORYL WCA871A PPE (Asia Pacific)
Flame retardant performance and mechanical properties capable of meeting UL VW-1 requirement and 105C temperature rating as defined UL1581. UL1581 tests conducted on 1.0mmD wire with AWG28 conductor..
|
|||
| Flexural Modulus | 0.100 GPa | 14.5 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
|
SABIC Innovative Plastics NORYL WCA871A PPE (Europe-Africa-Middle East)
Flame retardant performance and mechanical properties capable of meeting UL VW-1 requirement and 105C temperature rating as defined UL1581. UL1581 tests conducted on 1.0mmD wire with AWG28 conductor..
|
|||
| Flexural Modulus | 0.100 GPa | 14.5 ksi | 12.5 mm/min; ISO 178 |
|
SABIC Innovative Plastics NORYL WCA871A PPE (Europe-Africa-Middle East)
Flame retardant performance and mechanical properties capable of meeting UL VW-1 requirement and 105C temperature rating as defined UL1581. UL1581 tests conducted on 1.0mmD wire with AWG28 conductor..
|
|||
| Flexural Modulus | 0.100 GPa | 14.5 ksi | 12.5 mm/min, 100 mm span; ASTM D790 |
|
SABIC Innovative Plastics NORYL WCD915 PPE-TPE (Asia Pacific)
Flexible and non-halogenated flame retardant extrusion grade intended for evaluation in applications such as insulation materials. Flame retardant performance capable of meeting UL 1581 VW-1 require..
|
|||
| Flexural Modulus | 0.100 GPa | 14.5 ksi | ASTM D790 |
|
Borealis Casico™ FR4807 Non-Halogen Flame Retardant Compound for Low Voltage Insulation and Jacketing
Casico FR4807 is a natural, thermoplastic polyolefin compound designed for flame retardant low voltage wire insulation and jacketing. As such, FR4804 offers a unique combination of good extrusion pr..
|
|||
| Flexural Modulus | 0.100 GPa | 14.5 ksi | ASTM D790 |
|
DuPont™ Surlyn® 8020 Ionomer Resin, Sodium
Surlyn® 8020 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu..
|
|||
| Flexural Modulus | 0.100 GPa | 14.5 ksi | ASTM D790 |
|
DuPont™ Surlyn® 9020 Ionomer Resin, Zinc
Surlyn® 9020 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with zinc ions. The resin contains an addit..
|
|||
| Flexural Modulus | 0.100 GPa | 14.5 ksi | ISO 178 |
|
DuPont Performance Polymers Hytrel® HTR8685 BK022A Polyester Elastomer TPC-ET
(Unverified Data**)
44 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Hytrel HTR8685 BK022A is designed for blow molding or processing techniques requi..
|
|||
| Flexural Modulus | 0.100 GPa | 14.5 ksi | ASTM D790 |
|
C.O.I.M. LARIPUR® LPR4525 Special Adipate Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
|
|||
| Flexural Modulus | 0.100 GPa | 14.5 ksi | ASTM D790 |
|
Buckeye Polymers BP Flex D0840 TPO
Replace Flex PVCTPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment. These resins have excellent UV resis..
|
|||
| Flexural Modulus | 0.100 GPa | 14.5 ksi | ASTM D790 |
|
Ashley Polymers Ashlene® R6020 Nylon 6
A medium viscosity extrusion grade resin with excellent melt stability and good melt strength, suitable for extrusion coating and film co-extrusion applications. Excellent grease resistance, toughn..
|
|||
| Flexural Modulus | 0.100 - 9.50 GPa | 14.5 - 1380 ksi | Average value: 2.15 GPa Grade Count:327 |
|
Overview of materials for Nylon 6, Unreinforced