| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 9.70 GPa | 1410 ksi | ASTM D790 |
|
Premix Premi-Glas® 1100V-10 Fiberglass Reinforced Thermoset BMC
Premi-Glas® 1100V-10 is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regulator..
|
|||
| Flexural Modulus | 9.70 GPa | 1410 ksi | ASTM D790 |
|
Premix Premi-Glas® 1100V-15 Fiberglass Reinforced Thermoset BMC
Premi-Glas® 1100V-15 is a fiberglass reinforced thermoset bulk molding compound for electrical and flame retardant applications.Key features and benefits are:Non-Halogen FR technology for regulator..
|
|||
| Flexural Modulus |
9.70
GPa @Temperature 23.0 °C |
1410
ksi @Temperature 73.4 °F |
ISO 178 |
|
DuPont Performance Polymers Rynite® RE19051 BK507 PET
(Unverified Data**)
Rynite® RE19051 BK507 is a 40% glass and mineral reinforced, flame retardant, polyethylene terephthalate black resin.Information provided by DuPont Performance Polymers
|
|||
| Flexural Modulus | 9.70 GPa | 1410 ksi | ISO 178 |
|
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK)
(Unverified Data**)
AvaSpire AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 resin. ..
|
|||
| Flexural Modulus | 9.70 GPa | 1410 ksi | ASTM D790 |
|
Premix Premi-Glas® 2103-10 CRSX Polyester BMC
Premi-Glas® 2103-10 CR-SX is a 10% glass reinforced thermoset Sheet Molding Compound designed for electrical switchgear and industrial circuit breaker applications. Key features and benefits are:U..
|
|||
| Flexural Modulus | 9.70 GPa | 1410 ksi | cond., 2 mm/min; ISO 178-A |
|
Lanxess Durethan® BKV 50 000000 Nylon 6, Glass Fiber Reinforced
PA 6, 50% glass fibers, injection moldingInformation provided by LANXESS.
|
|||
| Flexural Modulus | 9.70 GPa | 1410 ksi | cond., 2 mm/min; ISO 178-A |
|
Lanxess Durethan® BKV 50 H EF DUS022 900116 Nylon 6, Glass Fiber Reinforced
PA 6, 50% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS.
|
|||
| Flexural Modulus | 9.70 GPa | 1410 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics LNP LUBRICOMP RFL159 PA 66
LNP* LUBRICOMP* RFL159 is a compound based on Nylon 66 resin containing 25% Glass Fiber, 5% PTFE. Added features of this material include: Wear Resistant, Flame Retardant
|
|||
| Flexural Modulus | 9.70 GPa | 1410 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP LUBRICOMP RFL36XXY PA 66
LNP* LUBRICOMP* RFL36XXY is a compound based on Nylon 66 containing 30% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant.
|
|||
| Flexural Modulus | 9.75 GPa | 1410 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics LNP LUBRICOMP RFL36XXZ PA 66 (Asia Pacific)
LNP Lubricomp is a compound based on PA66 resin containing glass fiber, PTFE. It is an internally lubricated compound that provide excellent chemical resistance, strength and wear/friction propertie..
|
|||
| Flexural Modulus | 9.75 GPa | 1410 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP LUBRICOMP RFN17SXS PA (Europe-Africa-Middle East)
LNP* Lubricomp* RFN17SXS is a compound based on Nylon 66 resin containing Glass Fiber, MOS2. Added features of this material include: Heat Stabilized
|
|||
| Flexural Modulus | 9.70 GPa | 1410 ksi | ISO 178 |
|
Solvay Specialty Polymers AvaSpire® AV-651 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber
AvaSpire® AV-651 GF30 is a 30% glass fiber reinforced polyaryletherketone (PAEK) that has been specifically formulated to provide higher mechanical strength and stiffness than unfilled AV-651 res..
|
|||
| Flexural Modulus | 9.70 GPa | 1410 ksi | ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP DE004ERP PC
LNP* Thermocomp* DE004ERP is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features include: Electrically Conductive, Easy Molding, Mold Release.
|
|||
| Flexural Modulus | 9.70 GPa | 1410 ksi | ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP DE004ERP PC (Asia Pacific)
LNP* Thermocomp* DE004ERP is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive, Easy Molding, Mold Release.
|
|||
| Flexural Modulus | 9.75 GPa | 1410 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics LNP THERMOCOMP EXTC8141 PC (Asia Pacific)
LNP* Thermocomp* EXTC8141 is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good ductility, No..
|
|||
| Flexural Modulus | 9.70 GPa | 1410 ksi | ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP JF006E PES
LNP* THERMOCOMP* JF006E is a compound based on Polyethersulfone resin containing 30% Glass Fiber. Added features of this material include: Easy Molding.
|
|||
| Flexural Modulus | 9.70 GPa | 1410 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics LNP THERMOCOMP RF006 PA 66
LNP* THERMOCOMP* RF006 is a compound based on Nylon 66 resin containing 30% Glass Fiber.
|
|||
| Flexural Modulus | 9.70 GPa | 1410 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics LNP THERMOCOMP RF006XXH PA 66
LNP* THERMOCOMP* RF006XXH is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added feature of this material is: Healthcare.
|
|||
| Flexural Modulus | 9.70 GPa | 1410 ksi | ISO 178-93 |
|
Wellman Wellamid® GF33A099-HRN Nylon 66, 33% Glass Reinforced, Hydrolysis Resistant
All information provided by Wellman Engineered Resins.
|
|||
| Flexural Modulus | 9.70 GPa | 1410 ksi | ASTM Test |
|
BASF Petra® 130 FR BK-112 30% Glass Filled PET
Petra 130 FR BK-112 is a 30% glass fiber reinforced, black pigmented, flame retardant injection molding compound based on post-consumer and post-industrial recycle polyethylene erephthalate feedstoc..
|
|||
| Flexural Modulus | 9.70 GPa | 1410 ksi | ASTM D790 |
|
Ashley Polymers Ashlene® 980LS-40G Nylon 612, 40% Glass Reinforced
A 40% glass reinforced, heat stabilized Nylon 612 resin.Data provided by the manufacturer
|
|||
| Flexural Modulus | 9.70 GPa | 1410 ksi | ASTM D790 |
|
A. Schulman ComAlloy Hiloy® 514 Polycarbonate, Glass Reinforced, UL
Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Flexural Modulus | 9.72 GPa | 1410 ksi | ASTM D790 |
|
LNP Thermocomp® JF-1006 Polyethersulfone, Glass Fiber Reinforcement
(discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..
|
|||
| Flexural Modulus | 9.70 GPa | 1410 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics LNP VERTON RV0079 PA 66
LNP VERTON* RV0079 is a compound based on Nylon 66 resin containing 35% Long Glasss Fiber. Added features of this material include: Flame Retardant, Structural.
|
|||