| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 10.0 GPa | 1450 ksi | ASTM D790 |
|
Premix Premi-Glas® 1200-22 Fiberglass Reinforced Thermoset SMC
Premi-Glas® 1200-22 is a fiberglass reinforced thermoset sheet molding compound for general purpose applications requiring thermal stability and stiffness.Key features and benefits are:Excellent st..
|
|||
| Flexural Modulus | 10.0 GPa | 1450 ksi | ASTM D790 |
|
Premix Premi-Glas® 1201-20 Fiberglass Reinforced Thermoset SMC
Premi-Glas® 1201-20 is a fiberglass reinforced thermoset sheet molding compound for sanitary ware applications such as shower bases and surrounds, bathtubs and vanity tops.Key features and benefits..
|
|||
| Flexural Modulus | 10.0 GPa | 1450 ksi | ASTM D790 |
|
Premix Premi-Glas® 2143-24 CR-SX Fiberglass Reinforced Thick Molding Compound
Premi-Glas® 2143-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves..
|
|||
| Flexural Modulus | 10.0 GPa | 1450 ksi | ASTM D790 |
|
Premix Premi-Glas® 2207-20 CR-SX Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2207-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f..
|
|||
| Flexural Modulus | >= 10.0 GPa | >= 1450 ksi | DIN 53452 |
|
Qualchem Danamid AFCF-30 Polyamide 66, 30% Carbon Fiber
Reinforced with carbon fiber, antistatic and conductive.Information provided by Qualchem Zrt.
|
|||
| Flexural Modulus | 10.0 - 15.0 GPa | 1450 - 2180 ksi | Injection; ISO 178 |
|
Raschig Group 6552 DAIP
Glass-fiber reinforced diallyl isophthalate molding compound. Good mechanical strength together with retention of high electrical isolation properties under hot humid conditions, exceptional dimensi..
|
|||
| Flexural Modulus | 10.0 GPa | 1450 ksi | ASTM D 790 |
|
SABIC Innovative Plastics Lexan® LCG0820 PC (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Flexural Modulus | 10.0 GPa | 1450 ksi | |
|
Lehmann & Voss LUVOCOM® 1301-7508 PPS, linear, with glass spheres
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic..
|
|||
| Flexural Modulus | 10.0 GPa | 1450 ksi | |
|
Lehmann & Voss LUVOCOM® 20-0778/BK Polyphthalamide, with glass fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
|
|||
| Flexural Modulus |
10.0
GPa <br>@Temperature 22.0 °C
|
1450
ksi <br>@Temperature 71.6 °F
|
25 mm wide 100 mm long, flat samples; ISO 14125 |
|
Menzolit Menzolit® BMC 2500 Unsaturated Polyester UP
BMC 2500 is a special BMC for high voltage isolating applications. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. The fire retardanc..
|
|||
| Flexural Modulus |
10.0
GPa <br>@Temperature 22.0 °C
|
1450
ksi <br>@Temperature 71.6 °F
|
25 mm wide 100 mm long, flat samples; ISO 14125 |
|
Menzolit Menzolit® BMC 2800 Unsaturated Polyester UP
BMC 2800 is a high performance BMC for matching the demands of medium and high voltage applications in the electrical field especially in respect of RTI 160+ according to Underwriters Laboratories ..
|
|||
| Flexural Modulus |
10.0
GPa <br>@Temperature 22.0 °C
|
1450
ksi <br>@Temperature 71.6 °F
|
25 mm wide 100 mm long, flat samples; ISO 14125 |
|
Menzolit Menzolit® SMC 0300 Unsaturated Polyester UP
SMC 0300 is a low shrink standard SMC providing improved surface quality, reduced shrinkage and warpage. Typical fields of applications are mechanical engineering and electrical industry, where impr..
|
|||
| Flexural Modulus | 10.0 GPa | 1450 ksi | 1.3 mm/min; ASTM D790 |
|
Lavergne VYPET VNT 635A PET 35% Glass Reinforced
Vypet 635A is a 35 % glass reinforced PET injection molding compound designed for electrical and structural applications with a very glossy surface.Features: High temperature performance, Excellent..
|
|||
| Flexural Modulus | 10.0 GPa | 1450 ksi | ISO 178 |
|
Solvay TECHNYL® A 218HP V50 PA66, 35% glass fiber, Conditioned
Description: TECHNYL® A 218HP V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product off..
|
|||
| Flexural Modulus | 9.98 GPa | 1450 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP THERMOTUF IX02582 PA6.12
LNP* Thermotuf* IX02582 is a compound based on Nylon 6/12 resin containing Proprietary Filler(s). Added features of this material include: High Impact.
|
|||
| Flexural Modulus | 10.0 GPa | 1450 ksi | ASTM D790 |
|
Lubrizol Isoplast® 101LGF40NAT Engineering Thermoplastic Polyurethane Resin
Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009.
|
|||
| Flexural Modulus | 10.0 GPa | 1450 ksi | ASTM-D790 |
|
Polyram PlusTek PB300G7 Nylon 6, 35% Glass Fiber
35% glass-fiber reinforced, heat stabilized polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Flexural Modulus | 10.0 GPa | 1450 ksi | ASTM D790 |
|
Toyobo VYLOPET® EMC333 Injection Molding Polyester Resin, Hydrolysis Resistant
Applications: Electric rice cooker partsBathroom appliancesFeatures: Good hydrolysis resistanceInformation provided by Toyobo.
|
|||
| Flexural Modulus | 10.0 GPa | 1450 ksi | ISO 178 |
|
BASF Ultramid® B3EG7 BK 00564 35% Glass Filled PA6 (Dry)
Description: 35% Glass fiber reinforced injection molding grade for industrial articles and electrical insulating parts.Information provided by BASF
|
|||
| Flexural Modulus | 10.0 GPa | 1450 ksi | ASTM D790 |
|
Adell DR-18 40% Glass Reinforced Polycarbonate |
|||
| Flexural Modulus | 10.0 GPa | 1450 ksi | ASTM D790 |
|
Gharda Chemicals GATONE™ 5330GF Polyetheretherketone (PEEK)
(discontinued **)
Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric..
|
|||
| Flexural Modulus | 10.0 GPa | 1450 ksi | 2 mm/min; ISO 178-A |
|
Lanxess Pocan® BFN 4231 000000 PBT, 25% Glass Fiber
PBT, 25% glass fibers, injection molding, halogen free flame retardantInformation provided by LANXESS.
|
|||
| Flexural Modulus | 10.0 - 12.0 GPa | 1450 - 1740 ksi | ISO 178 |
|
Vyncolit 3520 CG Novolac Phenolic
Graphite filled phenolic molding compound with excellent dimensional stability. Self-lubricating and has a low coefficient of friction. Not suitable for electrical applications.USES: Gas meter par..
|
|||