| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 1.03 GPa | 150 ksi | Tangent; ASTM D790 |
|
RheTech Products FT4200-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Body side moldingsGrillesElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Flexural Modulus | 1.03 GPa | 150 ksi | Tangent; ASTM D790 |
|
RheTech Products P250-00UV Polypropylene Copolymer, UV Stabilized, Natural
Applications: ConsolesConsumer goodsInterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Flexural Modulus | 1.03 GPa | 150 ksi | Tangent; ASTM D790 |
|
RheTech Products P252-670UV Polypropylene Copolymer, UV Stabilized, 134B Stone
Applications: Interior trimElectrical housingsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Flexural Modulus | 1.03 GPa | 150 ksi | Test Method I, Procedure B (chs speed 0.05 in/min), Secant; ASTM D790 |
|
Network Polymers NPP 25-3502
Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc.
|
|||
| Flexural Modulus | 1.03 GPa | 150 ksi | 0.05 in/min; 1% secant; Procedure A; ASTM D790 |
|
Phillips 66 COPYLENE® CR750CL-02 Polypropylene, Random Copolymer, NX-8000 based
COPYLENE™ CR750CL-02 is an easy molding, high melt flow random copolymer that has good see-through and contact clarity in injection molding applications and is formulated with advanced technology. ..
|
|||
| Flexural Modulus | 1.03 GPa | 150 ksi | 0.05 in/mm, 1% Secant, Procedure A; ASTM D790 |
|
Phillips 66 COPYLENE® CR750CLS Polypropylene Random Copolymer
Description: COPYLENE® CR750CLS is a clarified random copolymer specially designed and formulated for clear injection molding applications and is formulated with antistat and lube for excellent mol..
|
|||
| Flexural Modulus | 1.03 GPa | 150 ksi | Tangent; ASTM D790 |
|
RheTech Products HP513-00A High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Interior trimI/P componentsCenter consolesInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
|
Ravago Manufacturing Americas Echo® RPPC 20/6 BK Polypropylene Copolymer
Available in North America Recycled Content: Yes Features: CopolymerColor: Black Form: Pellets Information provided by Ravago
|
|||
| Flexural Modulus | 1.03 GPa | 150 ksi | 2% Secant-Method 1; ASTM D790 |
|
Ineos TUB 121 HDPE
TUB 121 (aka ELTEX® TUB 121, ELTEX® TUB 121 N2025, and ELTEX® TUB 121 N3000) is a black high density bimodal polyethylene copolymer designed for extrusion of potable water, natural gas, ind..
|
|||
| Flexural Modulus | 1.03 GPa | 150 ksi | 2% Secant-Method 1; ASTM D790 |
|
Ineos TUB 121N HDPE
TUB121N is a natural high density bimodal polyethylene copolymer designed for extrusion of potable water, natural gas, industrial, and mining pipe. When blended with an approved black concentrate, t..
|
|||
| Flexural Modulus | 1.03 GPa | 150 ksi | 1% Secant at 0.05 in/min; ASTM D790A |
|
Ineos R05C-00 Polypropylene Random Copolymer
Random copolymer R05C-00 is an antistatic, clarified polypropylene random copolymer produced by a unique catalyst technology. It is designed as a high gloss resin and exhibits good stiffness and imp..
|
|||
| Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
|
Techmer ES HiFill FR® HDPE 8904 FR UV GY
Availability: North AmericaForms: PelletsAdditive: UV StabilizerFeatures: Flame Retardant and Good UV ResistanceAppearance: GrayInformation provided by TP Composites, Inc.
|
|||
| Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
|
Techmer ES HiFill® PA6 GF30 HS BK 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc..
|
|||
| Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
|
Techmer ES HiFill® PA6 GF30 HS L BK 30% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearanc..
|
|||
| Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
|
Techmer ES HiFill FR® PP CO E FR
Availability: North AmericaForms: PelletsFeatures: Flame Retardant and CopolymerProcessing Method: ExtrudedInformation provided by TP Composites, Inc.
|
|||
| Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
|
A. Schulman POLYTROPE™ TPP 615 Olefinic Elastomer
DescriptionPolytrope TPP 615 is an olefinic elastomer developed to exhibit very low thermal expansion, high DOI on painted parts with good low temperature impact properties. ApplicationTPP 615 is de..
|
|||
| Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
|
A. Schulman PP 1817-01 Polypropylene Utility Grade Random Co-Polymer
DescriptionPolypropylene PP 1817-01 is a utility grade random co-polymer which can be used for general purpose injection molding, extrusion, or blow molding applications. It does not have a gel spe..
|
|||
| Flexural Modulus | 1.03 GPa | 150 ksi | 1.3mm per min, 1% secant; ASTM D790 |
|
Formosa Plastics Formolene® 3355E Random Copolymer Polypropylene
Random Copolymer for Containers, Totes and Bins, and Closures Formolene® 3355E is a high melt flow random copolymer with fast cycle time and good mold and denesting release. It is designed for inje..
|
|||
| Flexural Modulus | 1.03 GPa | 150 ksi | 1.3mm per min, 1% secant; ASTM D790 |
|
Formosa Plastics Formolene® 3355O Random Copolymer Polypropylene
Random Copolymer for Clear Storage Containers and Food and Beverage Containers Formolene® 3355O is a high melt flow random copolymer with fast cycle time and easy mold release. It is designed for i..
|
|||
| Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
|
Formosa Plastics Formolene® HB5502F Blow Molding HDPE
High Density Polyethylene Hexene Copolymer with Synthetic Antistat Formolene® HB5502F HDPE resin is designed for applications requiring excellent stiffness and stress crack resistance properties. I..
|
|||
| Flexural Modulus | 1.03 GPa | 150 ksi | |
|
TriStar TriSteel AT Metal Backed PTFE Bearing System
Ultraflon 601T (AT) POM bronze with PTFE, lined metal back bearing system, high PV, self lube, high speed. This liner will run with zero lubrication required. Most commonly used in clip bearings, li..
|
|||
| Flexural Modulus | 1.03 GPa | 150 ksi | 1.3mm per min, 1% secant; ASTM D790 |
|
Formosa Plastics Formolene® 3320B Random Copolymer Polypropylene
Random Copolymer for Storage Boxes, Pill Vials and Containers Formolene® 3320B is a high flow random copolymer with fast cycle time and easy mold release. It is designed for injection molding appli..
|
|||
| Flexural Modulus | 1.03 GPa | 150 ksi | 0.05 in/min; ISO 178 |
|
CTC X-PRO PP 2021 Polypropylene Impact Copolymer
X-PRO PP 2021 is an impact, polypropylene copolymer. It has general purpose applications.Data provided by Composite Technologies (CTC).
|
|||
| Flexural Modulus | 1.03 GPa | 150 ksi | Compression molded parts prepared according to ASTM D 1928, method 1, procedure B.; ASTM D790 |
|
Dow CONTINUUM™ DGDA-2490 NT Bimodal Polyethylene Resin
CONTINUUM™ DGDA-2490 NT is produced using UNIPOL™ II process technology. This product may be utilized for pipe applications where long term hydrostatic strength combined with outstanding resistan..
|
|||
| Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
|
Aaron Industries AVPP C 200-2 MELT 30 Clarified Virgin Polypropylene
A natural polypropylene copolymer resin specifically designed for injection molding applications - containing clarifiers.
|
|||
| Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D 790 |
|
Total XT10 N Natural HDPE, pipe
Applications: Potable water, industrial and mining, sewer and sewer relining, gas and oil gathering, general pipe relining, pipe coatingInformation provided provided by Total Petrochemicals.Total Pe..
|
|||
| Flexural Modulus | 1.03 GPa | 150 ksi | ASTM D790 |
|
PolyOne Edgetek® UR-20GF/000 Thermoplastic Elastomer - TPU, Glass Filled
(discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation.
|
|||