Mechanical Properties Metric English Comments
Flexural Modulus 1.24 GPa
180 ksi
Tangent; ASTM D790
RheTech Products RCC233-01 33% Calcium Carbonate Reinforced Polypropylene Copolymer, Black, Recycled Content
Applications: Fender linersSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products.
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
Quadrant EPP Proteus® PP, Black Homopolymer Polypropylene (ASTM Product Data Sheet)
High impact resistance strength Better resistance to cracking at low temperatures than Homopolymer Polypropylene More pliable than homopolymer Meets food handling guidelines Chemical- and corrosion..
Flexural Modulus 1.24 GPa
180 ksi
0.05 in/min; 1% secant; Procedure A; ASTM D790
Phillips 66 COPYLENE® CM500LN Polypropylene, Impact Copolymer, High Flow, Medium Impact, Nucleated, Lube, Injection Molding
COPYLENE™ CM500LN is a very high melt flow, medium impact polypropylene copolymer resin, designed for injection molding applications requiring a good balance of properties with faster cycling capab..
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
Formosa Plastics Formolene® HP5221 Pipe HDPE  (discontinued **)
High Density Hexene Copolymer Formolene® HP5221 is a high performance copolymer that is designed for the most demanding requirements of corrugated pipe applications. Formolene® HP5221 meets the re..
Flexural Modulus 1.24 GPa
180 ksi
0.05 in/mm, 1% Secant, Procedure A; ASTM D790
Phillips 66 COPYLENE® CM020N Polypropylene Impact Copolymer
COPYLENE® CM020N is a nucleated, medium impact copolymer with an excellent balance of stiffness and impact performance for extrusion and injection processes.Applications: Extrusion and Injection Mo..
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
Albis Plastics Cellulose Acetate Propionate CP800 (Base Grade), 10% Plasticizer  (discontinued **)
Amorphous Cellulose Acetate Propionate (CAP)Characteristics: Strength, Hardness, Stiffness, Weatherability and Dimensional StabilityApplications: Brush Handles, Safety Glasses, Optical Products and ..
Flexural Modulus 1.24 GPa
<br>@Temperature 23.0 °C
180 ksi
<br>@Temperature 73.4 °F
ASTM D790A
Ineos H36G-00 Polypropylene Homopolymer
This is a high flow rate homopolymer. This material is designed for fiber spinning and spun bonded processes. It meets the requirements of the U.S. Food and Drug Administration as specified in 21 ..
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
Multibase Multi-Flex® D 6500 TPO Thermoplastic Polyolefin Elastomer
Features: Chemical Resistance, Good PaintableOzone Resistant General PurposeDensity, LowTear Strength, GoodUV Resistance, Good Forms:PelletsProcessing Method:Blow Molding Uses: Automotive Applica..
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
Techmer ES HiFill® HDPE TM20 20% Talc Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Talc Filler, 20% Filler by WeightInformation provided by TP Composites, Inc.
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790-92
Lubrizol Stat-Rite® S-680 Static Control PETG Alloy
Stat-Rite® S-680 is a static dissipative PETG alloy. Stat-Rite® M-680 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protectio..
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
A. Schulman PP 828S-01 Polypropylene Medium Impact Molding Grade Polypropylene
DescriptionPolypropylene PP 828S-01 is a medium impact molding grade created for applications needing good impact and higher H.D.T., such as tote bins, automotive ducting and housings. Information p..
Flexural Modulus 1.24 GPa
180 ksi
5 mm/min, tangent; ASTM D790
A. Schulman PP 1621 Polypropylene Low Flow Homopolymer Polypropylene
DescriptionPolypropylene PP 1621 is a low flow homopolymer polypropylene primarily used for sheet strapping and profile extrusion applications.ApplicationPP 1621 meets FDA Regulation 21 CFR 177.1520..
Flexural Modulus 1.24 GPa
180 ksi
5 mm/min, tangent; ASTM D790
A. Schulman PP 1621 Polypropylene Low Flow Homopolymer Polypropylene
DescriptionPolypropylene PP 1621 is a low flow homopolymer polypropylene primarily used for sheet strapping and profile extrusion applications.ApplicationPP 1621 meets FDA Regulation 21 CFR 177.1520..
Flexural Modulus 1.24 GPa
180 ksi
1.3mm per min, 1% secant; ASTM D790
Formosa Plastics Formolene® 4101M Staple Fiber and Injection Molding Polypropylene
HomopolymerApplications: Staple Fiber and General Purpose Injection MoldingFormolene 4101M is a medium viscosity, highly isotactic polypropylene homopolymer designed for Staple Fiber and general pur..
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
Formosa Plastics Formolene® E602 Pipe HDPE
High Density Polyethylene High Molecular Weight Bi-Modal Resin for Non-Pressure Pipe Extrusion Applications Formolene® E602 is a high performance copolymer that is designed for the most demanding r..
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
A. Schulman PP 3052X-01 Polypropylene Impact Resistant Copolymer
DescriptionPolypropylene PP 3052X-01 is an extra high flow impact resistant copolymer with relatively high stiffness. Information provided by A. Schulman.
Flexural Modulus 1.24 GPa
180 ksi
1% secant, 0.05 in/min.; ASTM D790A
ExxonMobil ACHIEVE 1605 Exxpol Metallocene Grade for Injection Molding Applications
Product Description: A homopolymer resin based on Exxpol™ metallocene technology designed for medical, electronics and other applications requiring cleanliness. It provides lower, volatiles and ext..
Flexural Modulus 1.24 GPa
180 ksi
chs 0.05 in/min; tangent; ASTM D790
Diamond Polymers NPP30-3500F Homopolymer Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Flexural Modulus 1.24 GPa
180 ksi
1% Secant; molded and tested in accordance with ASTM D 4101; ASTM D790A
Dow 5D49 Polypropylene Resin
DOW 5D49 is intended for use fiber spinning processes. It is well suited for spunbond non-woven applications.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braske..
Flexural Modulus 1.24 GPa
180 ksi
CMW® ELKONITE® TC10 Tungsten Carbide Copper material
For wiping and arcing electrical contacts and projection welding tips.Information provided by CMW Inc.
Flexural Modulus 1.24 GPa
180 ksi
1% Secant; ASTM D790
Plastics Group Polifil® RP-PP Polypropylene, Molding Grade
Polifil® RP-PP reprocessed polypropylene has the highest stiffness of the commodity olefin resins, while retaining sufficient impact properties for many applications. Due to its low cost and low de..
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
Quadrant EPP Proteus® White Homopolymer Polypropylene (ASTM Product Data Sheet)
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
A. Schulman POLYTROPE™ TPP 518 Injection Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 518 is an injection grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal expansion i..
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
Albis Plastics Cellulose Acetate CA700 , Unreinforced, 37% Plasticizer &nbsp;(discontinued **)
Amorphous Cellulose Acetate (CA)Characteristics: Chemical Resistance, Toughness, Strength, Hardness, Gloss, Clarity and "Feel"Applications: Tool Handles, Optical Products, Toys and Sheet ProductsPro..
Flexural Modulus 1.24 GPa
180 ksi
1% Secant; ASTM D790
LyondellBasell Alathon® 9301 High Density Polyethylene
ApplicationsALATHON 9301is a high density resin designed for sheet extrusion and thermoforming. It exhibits very low sag and high stiffness.Regulatory StatusALATHON 9301 meets the requirements of F..