| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 2.05 GPa | 297 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS (Asia Pacific)
High impact PC+ABS material designed for local Pacific Automotive applications
|
|||
| Flexural Modulus | 2.05 GPa | 297 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Lexan® BFL4000U PC (Europe-Africa-Middle East)
Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo..
|
|||
| Flexural Modulus | 2.05 GPa | 297 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer
Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul..
|
|||
| Flexural Modulus | 2.05 GPa | 297 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer (Asia Pacific)
Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul..
|
|||
| Flexural Modulus | 2.05 GPa | 297 ksi | ISO 178 |
|
Total Lacqrene® 1235 High Impact Polystyrene
(discontinued **)
LACQRENE® 1235 is a high gloss, high impact polystyrene used in injection molding and co-extrusion. This grade produces articles with a surface gloss level equivalent to that of certain grades of ..
|
|||
| Flexural Modulus |
2.05
GPa @Temperature 90.0 °C |
297
ksi @Temperature 194 °F |
ISO 178, ASTM D790 |
|
Nilit Nilamid B3 H G3 15% Glass Fiber Reinforced PA6
Description: Nilamid B3 H G3 is a general purpose, 15% glass fiber reinforced NYLON 6. These products combine good overall mechanical performance and impact strength with ease of processing. Key cha..
|
|||
| Flexural Modulus | 2.05 - 3.21 GPa | 297 - 466 ksi | Average value: 2.66 GPa Grade Count:47 |
|
Overview of materials for PVC, High Impact
This property data is a summary of similar materials in the MatWeb database for the category "PVC, High Impact". Each property range of values reported is minimum and maximum values of appropriate M..
|
|||
| Flexural Modulus | 2.05 GPa | 297 ksi | 2 mm/min; ISO 178 |
|
Ineos ABS Lustran® M210TF ABS Pellets
Lustran® ABS M210TF is used in general applications for toy and food contact. It meets European standard EN 71, part 3 and ASTM F 963. It has standard impact strength, high gloss, and is easy flo..
|
|||
| Flexural Modulus | 2.05 GPa | 297 ksi | 2 mm/min; ISO 178 |
|
Inno-Comp INNOPOL® CS 3-9230 KAR YU UV-Stabilized, 26% Mineral-Filled Compound Blend Of Polypropylene Homopolymer And Block-Copolymer
INNOPOL® CS 3-9230 KAR YU is a yellow colored, UV-stabilized, 26% mineral-filled compound based on a blend of polypropylene homopolymer and block-copolymer.INNOPOL® CS 3-9230 KAR YU is develop..
|
|||
| Flexural Modulus | 2.05 GPa | 297 ksi | ASTM D790 |
|
Hannam Chemical Hanalac 740 ABS, Super High Impact Grade
Superior impact strength, even at low temperature. Applications: helmets, shoe heels, bobbins, roller skates, bags, pipes, radiator grills, auto parts, appliance wheels.
|
|||
| Flexural Modulus | 2.05 GPa | 297 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Valox® IQ357 PBT+PC
Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified.
|
|||
| Flexural Modulus | 2.05 GPa | 297 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Valox® IQ357M PBT+PC
Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release.
|
|||
| Flexural Modulus | 2.05 GPa | 297 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Valox® IQ357U PBT+PC
Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin.
|
|||
| Flexural Modulus | 2.05 GPa | 297 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Xenoy® CL100 PBT+PC
Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom..
|
|||
| Flexural Modulus | 2.05 GPa | 297 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Europe-Africa-Middle East)
Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom..
|
|||
| Flexural Modulus | 2.05 GPa | 297 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Asia Pacific)
Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing..
|
|||
| Flexural Modulus | 2.05 GPa | 297 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics LNP STAT-KON SD000 PA12
LNP* STAT-KON* SD000 is an unfilled Nylon 12 compound. Added feature of this grade is: Electrically Conductive.
|
|||
| Flexural Modulus | 2.05 GPa | 297 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Xylex X8419 PC+POLYESTER
Low-medium flow, suitable for blow molding, injection molding, extrusion.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Flexural Modulus | 2.05 GPa | 297 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics XYLEX X8419 PC+POLYESTER (Europe-Africa-Middle East)
Low-medium flow, suitable for blow molding, injection molding, extrusion.
|
|||
| Flexural Modulus | 2.05 GPa | 297 ksi | 3-point, 2 mm/min; ISO 178 |
|
Styron MAGNUMâ„¢ 3416 SLG Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: The mass (continuous process) ABS technology of Styron ensures an ABS resin that combines excellent processability with a stable light base color providing an ideal resin for self coloring..
|
|||
| Flexural Modulus | 2.05 GPa | 297 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA (Europe-Africa-Middle East)
NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin..
|
|||
| Flexural Modulus | 2.05 GPa | 297 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
|
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Asia Pacific)
NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq..
|
|||
| Flexural Modulus | 2.05 GPa | 297 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
|
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Europe-Africa-Middle East)
NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq..
|
|||
| Flexural Modulus | 2.05 GPa | 297 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
|
SABIC Innovative Plastics NORYL NWP100 PPE+HIPS (Asia Pacific)
PPO/HIPS Unfilled high impact extrusion grade
|
|||
| Flexural Modulus | 2.05 GPa | 297 ksi | ASTM D 790 |
|
SABIC Innovative Plastics Noryl EBN9003 PPE+HIPS (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Flexural Modulus | 2.05 GPa | 297 ksi | ASTM D790 |
|
SABIC Innovative Plastics NORYL EXT115 PPE+PS (Asia Pacific)
PPE+PS, Auto exterior grade, wax remover resistant
|
|||
| Flexural Modulus | 2.05 GPa | 297 ksi | 2mm/min; ASTM D790 |
|
Denka TH-23 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene
"TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a..
|
|||
| Flexural Modulus | 2.05 GPa | 297 ksi | ISO 178 |
|
Eurostar Star L POM D51 POM, Injection Molded
Star L POM D51 is a PTFE Lubricated, POM Copolymer Injection Molding ResinInformation provided by Eurostar.
|
|||
| Flexural Modulus | 2.05 GPa | 297 ksi | ISO 178 |
|
Clariant Renol PA1SP0003 Nylon 66, PE Modified
Reduced Coefficient of FrictionData provided by Clariant Masterbatches
|
|||
| Flexural Modulus | 2.05 GPa | 297 ksi | ASTM D 790 |
|
SABIC Innovative Plastics Noryl EUN1240 PPE+HIPS (Asia Pacific)
This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||