| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 2.06 GPa | 299 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Cycolac® MG34LG ABS
Automotive: Low gloss ABS for unpainted interior applications.
|
|||
| Flexural Modulus | 2.06 GPa | 299 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer
Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in ..
|
|||
| Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D 790 |
|
SABIC Innovative Plastics LNP Colorcomp D10009 PC
LNP* Colorcomp* D10009 is a compound based on Polycarbonate resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant.This data was supplied ..
|
|||
| Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D790 |
|
SABIC Innovative Plastics LNP LUBRICOMP AL003 ABS (Europe-Africa-Middle East)
LNP LUBRICOMP* AL003 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Flexural Modulus |
2.06
GPa @Thickness 6.40 mm |
299
ksi @Thickness 0.252 in |
10mm/min; ASTM D790 |
|
LG Chemical LUMID HI5003A PA6/PO, High Impact, High Flow, Good Paintablility
Feature: Injection Molding, PA6/PO, High Impact, High Flow, Good PaintablilityApplication: Automotive Exterior PartsCAS No. 25038-54-4, 9010-79-1, 9003-07-0 and 14807-96-6Information provided by LG ..
|
|||
| Flexural Modulus |
2.06
GPa @Thickness 6.40 mm |
299
ksi @Thickness 0.252 in |
5mm/min; ASTM D790 |
|
LG Chemical Lupox® TE5000SP PBT+PC
Description: Injection Molding, PBT+PC, Low Gloss, Good WeatherabilityApplication: Automotive (Roof Rack)CAS No. 137050-02-03, 24968-12-5 and 103598-77-2Information provided by LG Chemical
|
|||
| Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D790 |
|
SABIC Innovative Plastics LNP LUBRICOMP DP003EH PC (Asia Pacific)
LNP LUBRICOMP* DP003EH is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Easy Molding.
|
|||
| Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D790 |
|
SABIC Innovative Plastics LNP LUBRICOMP IL004 PA 6/12 (Asia Pacific)
LNP* Lubricomp* IL004 is a compound based on Nylon 6/12 resin containing PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D790 |
|
SABIC Innovative Plastics LNP LUBRICOMP KL004 Acetal Copolymer (Asia Pacific)
LNP Lubricomp* KL004 is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. This grade was previously found under the LNP* Fu..
|
|||
| Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D790 |
|
SABIC Innovative Plastics LNP LUBRICOMP KL004 Acetal Copolymer (Europe-Africa-Middle East)
LNP* LUBRICOMP* KL004 is a compound based on Acetal Copolymer containing PTFE. Added features include Internally Lubricated.
|
|||
| Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D790 |
|
SABIC Innovative Plastics LNP LUBRICOMP KL004U Acetal Copolymer (Asia Pacific)
LNP Lubricomp* KL004U is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated. This grade was previously found under the LNP* F..
|
|||
| Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D790 |
|
SABIC Innovative Plastics LNP LUBRICOMP KP002 Acetal Copoly
LNP* LUBRICOMP* KP002 is a compound based on Acetal Copolymer resin containing 10% PTFE/Silicone. Added feature of this material is: Wear Resistant.
|
|||
| Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D790 |
|
SABIC Innovative Plastics LNP LUBRICOMP KP002 Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KP002 is a compound based on Acetal Copolymer resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.
|
|||
| Flexural Modulus | 2.06 GPa | 299 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NWR5810 PPE+PS
LNP* Lubricomp* Noryl_NWR5810 compound is a 10% PTFE filled PPE+PS. High flow and good impact. Applications requiring wear resistance/lubricity. Electronics.
|
|||
| Flexural Modulus | 2.06 GPa | 299 ksi | |
|
Shinil Chemical SHINSTAT PMMA Electrostatic Control Polymer Injection Grade
SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for ..
|
|||
| Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D790 |
|
SABIC Innovative Plastics LNP THERMOCOMP KZ001L Acetal Copoly (Asia Pacific)
LNP* Thermocomp* KZ001L is a compound based on Acetal Copolymer resin containing Glass Fiber. Added features of this material include: Low Extractible.
|
|||
| Flexural Modulus | 2.06 GPa | 299 ksi | 2.8 mm/min; ASTM D790 |
|
Samsung Cheil Industries Starex® SD-0150U ABS, Unreinforced
Information provided by Samsung Cheil Industries.
|
|||
| Flexural Modulus | 2.06 GPa | 299 ksi | 2.8 mm/min; ASTM D790 |
|
Samsung Cheil Industries Infino® EN-1052 PC, FR
Non-halogen flame-retardant material with high heat resistance that can be used in battery chargerInformation provided by Samsung Cheil Industries.
|
|||
| Flexural Modulus | 2.06 GPa | 299 ksi | 2.8 mm/min; ASTM D790 |
|
Samsung Cheil Industries Infino® HN-1064 PC, Unreinforced FR
PC material that is applied to other resin for mobile phone chargersInformation provided by Samsung Cheil Industries.
|
|||
| Flexural Modulus | 2.06 GPa | 299 ksi | 2.8 mm/min; ASTM D790 |
|
Samsung Cheil Industries Infino® HP-1000H PC/ABS, Unreinforced
Information provided by Samsung Cheil Industries.
|
|||
| Flexural Modulus | 2.06 GPa | 299 ksi | 2.8 mm/min; ASTM D790 |
|
Samsung Cheil Industries Starex® NH-0925U ABS, Unreinforced FR
Information provided by Samsung Cheil Industries.
|
|||
| Flexural Modulus | 2.06 GPa | 299 ksi | 2.8 mm/min; ASTM D790 |
|
Samsung Cheil Industries Starex® SD-0150U ABS, Unreinforced
Information provided by Samsung Cheil Industries.
|
|||
| Flexural Modulus | 2.06 GPa | 299 ksi | 2.8 mm/min; ASTM D790 |
|
Samsung Cheil Industries Starex® SF-0505HWR MABS, Unreinforced Scratch Resistant
Information provided by Samsung Cheil Industries.
|
|||
| Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D790 |
|
Samyang Trirex® 3022A Polycarbonate
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
|
|||
| Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D 790 |
|
SABIC Innovative Plastics LNP Thermotuf U1000AIS PPA (Asia Pacific)
LNP* Thermotuf* U1000AIS is a compound based on Polyphthalamide resin. Added features of this material include: High Impact, Heat Stabilized.This data was supplied by SABIC-IP for the Asia Pacific ..
|
|||
| Flexural Modulus | 2.06 GPa | 299 ksi | ISO 178 |
|
DuPont Performance Polymers Delrin® 500TE NC010 Acetal (POM)
(Unverified Data**)
Toughened Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500TE NC010 (formerly DE20560) is a medium viscosity toughened acetal homopolymer with very low VOC emissions. Processing..
|
|||
| Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D790 |
|
SABIC Innovative Plastics LNP THERMOTUF V1000SU PA (Asia Pacific)
LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized.
|
|||
| Flexural Modulus | 2.06 GPa | 299 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics LNP LUBRICOMP DL004XXC PC
LNP* LUBRICOMP* DL004XXC is a compound based on Polycarbonate containing 20% PTFE. Characteristics of this grade are: Interrnally Lubricated.
|
|||
| Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D790 |
|
SABIC Innovative Plastics LNP STAT-KON MFD02 PP (Asia Pacific)
LNP* Stat-kon* MFD02 is a compound based on Polypropylene resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive.
|
|||
| Flexural Modulus | 2.06 GPa | 299 ksi | ASTM D790 |
|
Samyang Trimma® SD6350T PMMA, Opaque
High scratch resistance; stability against weak acids, strong acids, weak alkalis and inorganic salts.Information provided by Samyang.
|
|||