| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 2.30 GPa | 334 ksi | STN EN ISO 178 |
|
Plastcom SLOVALEN PC 51 T 20 Polypropylene Copolymer, 20% Micronized Talc
FeaturesModified copolymer PP for injection moulding with the content of 20% micronized, floated, chemically modified talc. General application in all industry branches - packing material, garden f..
|
|||
| Flexural Modulus | 2.30 GPa | 334 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
|
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS (Asia Pacific)
High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra..
|
|||
| Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS (Asia Pacific)
High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra..
|
|||
| Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Lexan® 945ASR PC (Asia Pacific)
Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t..
|
|||
| Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Lexan® FXD123R PC (Europe-Africa-Middle East)
LEXAN FXD123R is a transparent/translucent low viscosity grade for light diffusion special effects. UV-stabilized. Color package may affect performance.
|
|||
| Flexural Modulus | 2.30 GPa | 334 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Lexan® HF1130R PC
PC, High Flow, Mold Release, UV-Stabilized
|
|||
| Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Lexan® HP2NR PC (Europe-Africa-Middle East)
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no..
|
|||
| Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Lexan® HP6REU PC (Europe-Africa-Middle East)
Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold ..
|
|||
| Flexural Modulus | 2.30 GPa | 334 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Lexan® PC2200R PC (Europe-Africa-Middle East)
PC2200R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
|
|||
| Flexural Modulus | 2.30 GPa | 334 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Lexan® PK2870 PC
LEXAN* PK2870 polycarbonate resin, global grade, MVR (300C/1.2kg) 2 cm3/10min, high viscosity, branched, blow molding, high melt strength, high impact resistance, Available in transparent colors onl..
|
|||
| Flexural Modulus | 2.30 GPa | 334 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Lexan® VR1820 PC (Europe-Africa-Middle East)
VR1820 resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
|
|||
| Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP LUBRICOMP DL0039E PC (Europe-Africa-Middle East)
LNP* LUBRICOMP* DL0039E is a compound based on Polycarbonate resin containing PTFE, Flame retardant. Added features include: Easy Molding, Internally Lubricated, Flame retardant.
|
|||
| Flexural Modulus | 2.30 GPa | 334 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
|
SABIC Innovative Plastics Cycoloy® EFX830ME PC (Asia Pacific)
Modified PC blend offering metallic look with minimal flow lines, flame retarded without using Chlorinated or Brominated additives.This data was supplied by SABIC-IP for the Asia Pacific region.
|
|||
| Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Lexan® 221R PC (Europe-Africa-Middle East)
LEXAN 221R is a low viscosity multi purpose grade and contains a release agent to ensure easy processing. This grade is UL94-V2 at 0.4 mm approved.
|
|||
| Flexural Modulus | 2.30 GPa | 334 ksi | 15 mm/min; ASTM D790 |
|
LG Chemical SF-510 Alphalac Polystyrene
(Unverified Data**)
Super flow, High gloss and high impact equivalent to ABS, Excellent mechanical properties compare with general HIPS, Meet requirements for cost and quality, Applications include TV cabinets, thin pa..
|
|||
| Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Lexan® BFL2000U PC
Lexan* BFL2000U Polycarbonat (PC) resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating. Lexan* BFL2000U is designed for hig..
|
|||
| Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Lexan® FXD164R PC (Europe-Africa-Middle East)
Transparent/translucent medium viscosity PC for light diffusion special effects, FDA compliant and mold release containing. The color package may affect performance.This data was supplied by SABIC-I..
|
|||
| Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
|
LG Chemical HF-350 ABS, High Flow, High Impact
Information Provided by LG Chem
|
|||
| Flexural Modulus | 2.30 GPa | 334 ksi | ISO 178 |
|
LyondellBasell Hostacomâ„¢ SP98F/94 Thermoplastic Polyolefin Elastomer
Description: Hostacomâ„¢ SP98F/94 Black medium melt flow, 2,300 MPa flexural modulus, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good combination of stiffness, impact ..
|
|||
| Flexural Modulus | 2.30 GPa | 334 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
|
SABIC Innovative Plastics PC0800 PC
PC0800 resin is a low flow (MFR = 8 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release.T..
|
|||
| Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics PC1000 PC (Europe-Africa-Middle East)
PC1000R resin is a medium-low flow (MFR = 10 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.
|
|||
| Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics PC1800 PC
PC1800 resin is a medium-high flow (MFR = 18 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold ..
|
|||
| Flexural Modulus | 2.30 GPa | 334 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
|
SABIC Innovative Plastics PC2200 PC (Europe-Africa-Middle East)
PC2200 resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release..
|
|||
| Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics PC2200R PC (Europe-Africa-Middle East)
PC2200R resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market.This data was supplied by S..
|
|||
| Flexural Modulus | 2.30 GPa | 334 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics PC2800 PC (Europe-Africa-Middle East)
PC2800 resin is a high flow (MFR = 28 at 300°C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release...
|
|||
| Flexural Modulus | 2.30 GPa | 334 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics NORYL FXN121BK PPE+HIPS
Noryl* FXN121BK is an unfilled modified polyphenylene ether resin suitable for injection molding. Designed to possess a unique low gloss surface appearance even when molded in polished tools, this r..
|
|||
| Flexural Modulus | 2.30 GPa | 334 ksi | tangent; ASTM D790 |
|
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound
Information provided by A. Schulman.
|
|||
| Flexural Modulus | 2.30 GPa | 334 ksi | ASTM D790 |
|
A. Schulman POLYFORT™ FXP 2600-3120 CaC02 Filled Homopolymer Polypropylene
DescriptionPolyfort® FXP 2600-3120 is a 20% GAC02 filled homopolymer polypropylene compound.Information provided by A. Schulman.
|
|||
| Flexural Modulus | 2.30 GPa | 334 ksi | ASTM D790 |
|
Covestro Makrolon® 2458 Polycarbonate, Injection Grade
Very easy flowing BgVV- and FDA injection molding grade with easy mold release, for food contact applications, better resistance to hot water.Information provided by Bayer.As of 1 September 2015, Ba..
|
|||
| Flexural Modulus | 2.30 GPa | 334 ksi | ISO 178 |
|
BASF Ultramid® B3L PA6 (Dry)
Ultramid B3L is an impact-modified, easy flowing injection molding PA6 grade for fast processing.
|
|||