Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 2.34 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Cycolac® FR15U ABS
Flame retardant ABS with excellent indoor UV properties and excellent processing. UL94 V-0/5VA rated. Elevated UL RTI rating (90-85-90) for all colors except for blue and green colors (60-60-60).
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® 134 PC
Nonhalogenated. 3.5 MFR. FDA food contact compliant in limited colors.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® 135 PC
General purpose low flow polycarbonate powder gradeThis data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® 223 PC
17.5 MFR, for small, intricate parts. Improved flame retardance. UV stabilized.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® 223R PC
17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. UV stabilized.
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® FXD103 PC (Asia Pacific)
FXD103 is a Light Diffusion effect, part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace.This data was supplied by SABIC-IP for the ..
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Ravago Manufacturing Americas Hylex® P1307L Polycarbonate
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente..
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® HP8REU PC (Europe-Africa-Middle East)
Very low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains mold..
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® IR2840 PC
7.0 MFR, for thicker sections without sinks. Internal mold release. FDA food contact compliant, natural only.Effective January 15th, 2007 this grade will no longer be supported with biocompatibilit..
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® LUX2414G PC (Asia Pacific)
10 MFR. Improved flame retardance. Internal mold release. UV stabilized.
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® OQ2320 PC
Ophthalmic/safety lens market. OQ2xxx series in all transparent tints. Dedicated equipment, stringent quality production control.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® OQ4320R PC (Asia Pacific)
Optical grade with UV cut-off up to 400 nm; greater optical purity than standard grades. For sunglass and sunvisor markets. Internal mold release.
Flexural Modulus 2.34 GPa
<br>@Thickness 3.17 mm
340 ksi
<br>@Thickness 0.125 in
ASTM D790
PTS Tristar® PC-10FRNH 12 MFI Non-Bromine Non-Chlorine Flame Retardant Polycarbonate With Release
Information provided by Polymer Technology and Services, LLC (PTS).
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
PolyOne Lubri-Tech™ AT-000/8T Acetal-Copolymer, PTFE Lubricated &nbsp;(discontinued **)
Description/Features:PTFE LubricatedInformation provided by PolyOne Corporation.
Flexural Modulus 2.34 GPa
339 ksi
ASTM D790
Ineos ABS Cadon® 127 SMA General Purpose, High Heat &nbsp;(discontinued **)
Information provided by Bayer Corporation, Plastics DivisionLANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a JV with La..
Flexural Modulus 2.34 GPa
339 ksi
ASTM D790
Hannam Chemical Hanalac 770 ABS, Extrusion Grade
FDA Approved. Excellent mechanical strength, high rigidity, and high impact strength. Good thermoformability. Applications: Refrigerators liners, bathtubs, automobile interiors, portable bags, n..
Flexural Modulus 2.34 GPa
339 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP ZX07421 PPO
LN:* LUBRICOMP* ZX07421 is a compound based on PPO resin containing proprietary fillers. Added feature of this grade is: Wear Resistant.
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® HX312C PBT (Europe-Africa-Middle East)
Unreinforced PBT with release. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant. EtO and stea..
Flexural Modulus 2.34 GPa
<br>@Thickness 3.17 mm
340 ksi
<br>@Thickness 0.125 in
ASTM D790
Samsung Cheil Industries Starex® MP-0160RD Metal Plating Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL PN275 PPE+PS
PPE+PS with low mineral loading. High heat, platable applications.
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL PN275F PPE+PS
PPE+PS with low mineral loading. High heat, platable applications. NSF approved for water contact applications.
Flexural Modulus 2.34 GPa
<br>@Thickness 3.20 mm
339 ksi
<br>@Thickness 0.126 in
Injection Molded; ASTM D790
Styron PULSEâ„¢ 2100 LG PC/ABS Engineering Resin
Overview: PULSE 2100LG Engineering Resin is designed to provide top performance in tough applications, from single piece items to intricate components. Ideal for energy management solutions, it can ..
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
A. Schulman COMTUF® 506 Polycarbonate
Information provided by A. Schulman.
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
PlastxWorld CEVIAN® LMW48 Laser Markable Grade ABS
White MarkingThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc.
Flexural Modulus 2.34 GPa
340 ksi
Tangent; ASTM D790
Washington Penn Homopolymer Polypropylene 30% Calcium Carbonate Filled
Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa..
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Ensinger Hydel® PC-7 Polycarbonate (PC)
A polycarbonate based material with a proprietary carbon filler component. The highly dispersed filler imparts outstanding electrical consistency to minimize any hot spots. The material has good r..
Flexural Modulus 2.34 GPa
340 ksi
ASTM D790
Polymer Resources PPX-FR6 Modified PPO, UL 94 V-0 with HDT of 300 F &nbsp;(Unverified Data**)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation.
Flexural Modulus 2.34 GPa
340 ksi
2.0 in/min; ASTM D790
LTL Color Compounds ColorFast® FRPC300 Polycarbonate, Flame-Retarded
V2-rated polycarbonateAll information provided by LTL Color Compounders, Inc.
Flexural Modulus 2.34 GPa
339 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® HP4NR PC (Asia Pacific)
Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no m..
Copyright © lookpolymers.com All Rights Reserved