Polymer Property : Flexural Modulus = 2.60 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Modulus 2.60 GPa
377 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer
XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors.
Flexural Modulus 2.60 GPa
377 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer
XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors.
Flexural Modulus 2.60 GPa
377 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® XHT4143 PC Copolymer (Asia Pacific)
XHT4143 is a high flow, UV stabilized, high heat polycarbonate copolymer blend with an HDT/Af of 162C. It is available in a range of opaque and limited transparent colors.
Flexural Modulus 2.60 GPa
377 ksi
ISO 178
SABIC Innovative Plastics LNP Faradex DS0036IP PC (Europe-Africa-Middle East)
LNP* Faradex* DS0036IP is a compound based on Polycarbonate resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding, High Impact, Non-B..
Flexural Modulus 2.60 GPa
377 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP FARADEX KS002E Acetal Copolymer (Europe-Africa-Middle East)
LNP* FARADEX* KS002E is a compound based on Acetal Copolymer resin containing Stainless Steel Fiber. Added features include: EMI/RFI Shielding, Electrically Conductive, Easy Molding.
Flexural Modulus 2.60 GPa
377 ksi
STN EN ISO 178
Plastcom SLOVAMID 6 BT LS Polyamide 6, UV Stabilized
FeaturesPA 6 for injection moulding with the content of UV stabilizer predetermines products for external use, eg. seats for sport stadiums, covers of electrical appliances. Delivered in natural an..
Flexural Modulus 2.60 GPa
377 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® EXRL0627 PC Copolymer
EXRL0627 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and transparent colors.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.60 GPa
377 ksi
ASTM D790
Kolon KOCETAL® VT702 Anti-Static Grade Acetal Resin
Improved antistatic effects. Applications: Products for avoiding electric contamination. Information provided by API-Kolon.
Flexural Modulus 2.60 GPa
377 ksi
2 mm/min; ISO 178
Inno-Comp INNOPOL® CS 2-3120 20% Talc Filled Polypropylene Block-Copolymer
INNOPOL® CS 2-3120 is a 20% talc filled compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-3120 is developed for producing..
Flexural Modulus 2.60 GPa
377 ksi
d.a.m., 2 mm/min; ISO 178-A
Lanxess Durethan® B 31 FCS 000000 Nylon 6, Film Grade
PA 6, non-reinforced, extrusion, low viscosity, slip agentInformation provided by LANXESS.
Flexural Modulus 2.60 GPa
377 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL REN501 PPE+PS
Noryl REN501 resin is an unfilled Post Industrial Recycle (PIR) based injection moldable modified polyphenylene ether blend comprising up to 40% PIR content. Available in black only.
Flexural Modulus 2.60 GPa
377 ksi
ASTM D790
Solvay Specialty Polymers Veradel® 3000RP Polyethersulfone (PESU)
Veradel® 3000RP hydroxyl-functionalized polyethersulfones (r-PESU) is an amorphous, high-temperature sulfone polymer featuring reactive end groups to enhance solubility for dissolving or dispersi..
Flexural Modulus 2.60 GPa
377 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL PX1007 PPE+PS
Noryl* PX1007 is an unfilled non-chlorinated, non-brominated flame retardant PPE/HIPS grade.
Flexural Modulus 2.60 GPa
377 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA
Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be..
Flexural Modulus 2.60 GPa
377 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA (Europe-Africa-Middle East)
Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be..
Flexural Modulus 2.60 GPa
377 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL GTX GTX678 PPE+PA (Europe-Africa-Middle East)
Noryl GTX678 resin is a high performance blend of PPE/PA that exhibits an excellent balance on non-halogenated flame retardance, conductivity, ductility, and high-heat resistance. This grade can be..
Flexural Modulus 2.60 GPa
377 ksi
ASTM D790
Chase Plastics CP Pryme® AC100-27 Acetal Copolymer Molding Resin
Information provided by Chase Plastics.
Flexural Modulus 2.60 GPa
377 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 233 15% Mineral Reinforced Ionomer / Nylon Alloy
DescriptionFormion® FI 233 is an injection molding grade, 15% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. A..
Flexural Modulus 2.60 GPa
377 ksi
ISO 178-93
Wellman Wellamid® 42L-XE-N Nylon 6, Engineering Grade
All information provided by Wellman Engineered Resins.
Flexural Modulus 2.60 GPa
377 ksi
ASTM D 790
Cossa Polimeri ESTAPROP H 10100 BS Polypropylene, 50% Mineral Filled
PP homopolymer 50% mineral fillerExcellent surface appearance, high densityInformation provided by Cossa Polimeri S.r.l.
Flexural Modulus 2.60 GPa
377 ksi
dry; ISO 178
DSM Akulon® F-X9183 PA6
Low/Medium Viscosity
Flexural Modulus 2.60 GPa
377 ksi
ASTM D790
Aclo Accucomp ABS ABS892BL High Heat Grade
Flexural Modulus 2.60 GPa
377 ksi
ASTM D790
Aclo Accutech Polypropylene Copolymer CP0437M30CL Mica Reinforced Coupled
Flexural Modulus 2.60 GPa
377 ksi
ISO Data
BASF Ultraform W 2320 003 BK120 Q600 POM
Ultraform W 2320 003 BK120 Q600 is a pigmented black, very easy flowing and rapidly solidifying injection molding POM grade for use where processing is extremely difficult but mechanical properties ..
Flexural Modulus 2.60 GPa
377 ksi
ASTM D790
Ashley Polymers Ashlene® ABS Resin E213B
General purpose, black, utility grade for injection molding with medium gloss.Data provided by the manufacturer
Flexural Modulus 2.60 GPa
377 ksi
ASTM D790
A. Schulman ComAlloy Hiloy® 102 Polypropylene, Glass Reinforced
Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Modulus 2.60 GPa
377 ksi
ASTM Test
BASF Ultrason E 2010 PES
Ultrason E 2010 is an unreinforced, medium viscosity standard injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. It conforms to FDA req..
Flexural Modulus 2.60 GPa
377 ksi
ASTM D 790
Saint-Gobain Meldin® 2030 Bearing
General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca..
Flexural Modulus 2.60 GPa
<br>@Temperature 23.0 °C
377 ksi
<br>@Temperature 73.4 °F
ISO 178
DuPont Performance Polymers Delrin® FG100P NC010 Acetal Homopolymer &nbsp;(Unverified Data**)
Delrin® FG100P is a high viscosity acetal homopolymer, with improved thermal stability for use in easy to fill molds. It has been developed for consideration into applications such as parts for the..