| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
|
PolyOne Geon™ Vinyl Rigid Molding M4300 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
|
PolyOne Geon™ Vinyl Rigid Molding M5100 Natural Polyvinyl Chloride, Rigid (PVC, Rigid)
NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of..
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | Tangent; ASTM D790 |
|
RheTech Products G13P100-00UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, Natural
Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
|
PolyOne Nymax™ 623 Zip 5 HS Black 13 Polyamide 6 Alloy (Nylon 6 Alloy)
The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials..
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
|
Polymer Resources NY6-GP1-[color]H Nylon, General Purpose, Heat Stabilized (DAM)
Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Nylon grades are tested dry as molded (DAM).Information provide..
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
|
Quadrant EPP Quadrant LSG PSU, Extruded, Unfilled, Polysulfone (ASTM Product Data Sheet) |
|||
| Flexural Modulus | 2.76 - 9.00 GPa | 400 - 1310 ksi | Average value: 5.00 GPa Grade Count:14 |
|
Overview of materials for Nylon 66, Mineral Filled, Impact Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Mineral Filled, Impact Grade". Each property range of values reported is minimum and maximum v..
|
|||
| Flexural Modulus | 2.76 - 3.45 GPa | 400 - 500 ksi | Average value: 3.07 GPa Grade Count:11 |
|
Overview of materials for Nylon 612, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of..
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
|
Techmer ES Electrafil® PC-50/EC/VO Polycarbonate, Conductive Carbon Filled
Conductive Carbon, Powder Modified with Flame Retardant
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | tangent; ASTM D790 |
|
Spartech PP5130 Talc Filled Homopolymer
Offers an excellent balance of processing improvement and high levels of stiffness and heat deflection temperatureInformation provided by Spartech
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
|
Techmer ES Plastiblend® PA6/6 M L Nylon 66
Availability: North AmericaForms: PelletsAdditive: LubricantFeatures: Fast Molding Cycle, Low Viscosity and LubricatedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D 790 |
|
SABIC Innovative Plastics LNP Thermocomp KB002 Acetal Copoly
LNP* Thermocomp* KB002 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region.
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
|
Techmer ES Statiblend® POM CO
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified FillerReinforFeature: ConductiveTPCI# 9962114Information provided by TP Composites, Inc.
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
|
A. Schulman POLYFORT™ FPP 1607 Talc Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 1607 is a 30% talc filled homopolymer polypropylene compound. Information provided by A. Schulman.
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
|
A. Schulman POLYFORT™ FPP 1607 Talc Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 1607 is a 30% talc filled homopolymer polypropylene compound. Information provided by A. Schulman.
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D-790 |
|
Axiall CL-7053 Rigid PVC, Molding
Georgia Gulf CL-7053 is a clear, high flow vinyl compound designed for a variety of end-use molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | 0.1 in/min; ASTM D790 |
|
Ineos Nova 8047 High Performance Styrenic Enhanced Polystyrene
(discontinued **)
High flow, Special additives can be incorporate to improve properties such as coefficient of friction and static dissipation, Custom colorsApplications: Injection molding, Designed for thin wall app..
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D-790 |
|
Axiall 3240 Rigid PVC, Extrusion
Georgia Gulf 3240 is a special purpose rigid powder blend PVC compound designed for applications requiring the following properties: WeatherabilityGlossImpact Strength & ToughnessFlame RetardantChe..
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
|
PolyOne Edgetek® UR-20GF/000 Natural Thermoplastic Polyurethane (Ether-Based), 20% Glass Fiber Reinforced
(di
Information provided by PolyOne™ Corporation
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
|
PolyOne LubriOne™ ATH-000/10T 2S Acetal (POM) Homopolymer
(discontinued **)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
|
|||