| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 2.96 GPa | 430 ksi | ASTM D790 |
|
Multibase Multi-Pro® 4615 X White Polypropylene
Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
|
|||
| Flexural Modulus | 2.96 GPa | 429 ksi | ASTM D790 |
|
PolyOne Geon™ Vinyl Rigid Extrusion 87416 Polyvinyl Chloride, Rigid (PVC, Rigid)
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
|
|||
| Flexural Modulus | 2.96 GPa | 429 ksi | ASTM D790 |
|
PolyOne Geon™ Vinyl Rigid Extrusion L7005 Polyvinyl Chloride, Rigid (PVC, Rigid)
Geon L7005 is recommended for whites and light pastel colors only.Note: Physical properties based on L7005 tan 3210 sample.Information provided by PolyOne
|
|||
| Flexural Modulus | 2.96 GPa | 429 ksi | ASTM D790 |
|
PolyOne LubriOne™ NN-000/10T Polyamide 66 (Nylon 66)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
|
|||
| Flexural Modulus | 2.96 GPa | 429 ksi | ASTM D790 |
|
PolyOne Nymax™ 600 A Zip 23 Natural 1 Polyamide 6 Alloy (Nylon 6 Alloy)
The Nymax® 600 Blend Series of nylon 6 materials are salt-and-pepper pelletized blends combining select nylon resins and process aids, performance modifiers, and color concentrates. These materials..
|
|||
| Flexural Modulus | 2.96 GPa | 429 ksi | ASTM D790 |
|
PTS Trimid® N66-100HL Heat Stabilized, Lubed Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Flexural Modulus | 2.96 GPa | 429 ksi | ASTM D790 |
|
PTS Trimid® N66-100NL Nucleated, Lubricated Nylon 6/6
Information provided by Polymer Technology and Services, LLC (PTS).
|
|||
| Flexural Modulus | 2.96 GPa | 430 ksi | Tangent; ASTM D790 |
|
RheTech Products M25P100-01 25% Mica Reinforced Polypropylene, Black
Applications: Underhood applicationsInternal I/P ComponentsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Flexural Modulus | 2.96 GPa | 430 ksi | ASTM D790 |
|
PolyOne Lubri-Tech™ ATH-000/2T Acetal-Homopolymer, PTFE Lubricated
(discontinued **)
Description/Features:PTFE LubricatedInformation provided by PolyOne Corporation.
|
|||
| Flexural Modulus | 2.96 GPa | 429 ksi | 2 mm/min; ISO 178 |
|
Lucite International Perspexâ„¢ GS IM Acrylic Cast Sheet OM14
PERSPEX cast sheet is made between sheets of high quality glass and produced in batches. It has a very high molecular weight making it strong, resilient and easy to handle and fabricate. The cast me..
|
|||
| Flexural Modulus | 2.96 GPa | 429 ksi | ASTM D790 |
|
SABIC Innovative Plastics LNP LUBRICOMP LL004E PEEK (Asia Pacific)
LNP* Lubricomp* LL004E is a compound based on Polyetheretherketone resin containing PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Flexural Modulus | 2.96 GPa | 429 ksi | ASTM D790 |
|
SABIC Innovative Plastics LNP LUBRICOMP RAL22 PA 66
LNP LUBRICOMP* RAL22 is a compound based on Nylon 66 resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant.
|
|||
| Flexural Modulus | 2.96 GPa | 429 ksi | ASTM D790 |
|
SABIC Innovative Plastics LNP LUBRICOMP RAL22 PA 66 (Asia Pacific)
LNP LUBRICOMP* RAL22 is a compound based on Nylon 66 resin containing Aramid, PTFE. Added features of this material include: Internally Lubricated.
|
|||
| Flexural Modulus | 2.96 GPa | 430 ksi | ASTM D790 |
|
Techmer ES Luriblend® POM HO TL2 Acetal
Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(2%)Features: Lubricated, Good Wear Resistance and HomopolymerInformation provided by TP Composites, Inc.
|
|||
| Flexural Modulus | 2.96 GPa | 429 ksi | ASTM D790 |
|
SABIC Innovative Plastics LNP THERMOCOMP KB003RXZ Acetal Copolymer
LNP THERMOCOMP* KB003RXZ is a compound based on Acetal Copolymer resin containing 15% Glass Bead. Added features of this material include: Easy Release.
|
|||
| Flexural Modulus | 2.96 GPa | 430 ksi | Tangent; ASTM D790 |
|
Washington Penn Homopolymer Polypropylene 50% Calcium Carbonate Filled
Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa..
|
|||
| Flexural Modulus | 2.96 GPa | 430 ksi | ASTM D790 |
|
Total PSC 529 Polystyrene
Polystyrene 529 is a medium flow crystal specially formulated for mar resistance. The easy to process crystal minimizes visual defects from ejection and automated part handling. Typical applications..
|
|||
| Flexural Modulus | 2.96 GPa | 430 ksi | ASTM D790 |
|
Total PSC 536 Polystyrene
Polystyrene 536 is a high melt flow; high heat crystal polystyrene. Designed for fast cycle injection molding and for high output, direct injection profile extrusion for foam applications.Informatio..
|
|||
| Flexural Modulus | 2.96 GPa | 430 ksi | ASTM D790 |
|
Asahi Kasei Thermylene® P6-20FG-1734 20% Glass Fiber Reinforced, High Impact
Information provided by Asahi Thermofil
|
|||
| Flexural Modulus | 2.96 - 9.65 GPa | 430 - 1400 ksi | Average value: 7.58 GPa Grade Count:11 |
|
Overview of materials for Nylon 46, Lubricated + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Lubricated + Glass Fiber Reinforced". Each property range of values reported is minimum and ma..
|
|||
| Flexural Modulus | 2.96 GPa | 429 ksi | ASTM D790 |
|
Ravago Manufacturing Americas Echo® RPC10G BK Polypropylene Homopolymer
Available in North America Filler: Glass Fiber Reinforcement, 10% Filler by weight Recycled Content: YesFeatures: Homopolymer Color: Black Form: Pellets Information provided by Ravago.
|
|||
| Flexural Modulus | 2.96 GPa | 430 ksi | ASTM D-790 |
|
Axiall 3101 Rigid PVC, Extrusion
Georgia Gulf 3101 is a powder blend designed for the extrusion of window, door and fence profiles where weatherability is of primary consideration.Information provided by Georgia GulfGeorgia Gulf be..
|
|||
| Flexural Modulus | 2.96 GPa | 430 ksi | ASTM D790 |
|
Techmer ES HiFill FR® PPO/HIPS MM20 IM FR 20% Mineral Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 20% Filler by WeightAdditive: Impact Modifier Features: Flame Retardant and Impact ModifiedInformation provided by TP C..
|
|||