Polymer Property : Flexural Modulus = 210 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Modulus 1.45 GPa
210 ksi
Plastcom SLOVALEN PC 63 T 15-1M PP, 15% mineral filling
FeaturesModified PP copolymer for injection moulding with the content of 15 % mineral filler, uv stabilized, good scratch resistance, low odor and very good flowability with good dimensional stabili..
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790
PolyOne Maxxam™ PP CS 75 Polypropylene, Unspecified (PP, Unspecified)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Flexural Modulus 1.45 GPa
210 ksi
ISO 178
Polimeri Europa Eraclene® MP 90 C High Density Polyethylene - Injection Molding
Eraclene MP 90 C is a gas phase high density polyethylene resin (HDPE) with antioxidants, suitable for injection molding application.This grade has a narrow molecular weight distribution and a high ..
Flexural Modulus 1.45 GPa
210 ksi
0.05 in/min; ASTM D790
S&E Specialty Polymers TufTech™ 12-041 PVC Compound
Application: A PVC based semi-rigid compound designed for general purpose use in extruded form, including piping applications.Information provided by S&E Specialty Polymers
Flexural Modulus 1.45 GPa
210 ksi
ISO 178
Polimeri Europa Eraclene® MP 90 High Density Polyethylene - Injection Molding
Eraclene MP 90 is a high density polyethylene homopolymer resin (HDPE) with antioxidants, suitable for injection molding application.Eraclene MP 90 has a narrow molecular weight distribution and a h..
Flexural Modulus 1.45 GPa
210 ksi
1% Secant; ASTM D790
Flint Hills P4C5B-076 Homopolymer Polypropylene
Homopolymer, and FDA compliant.Features: Nucleated, antistat, and controlled rheology.Applications: Injection molding: cutlery and closuresFormer Huntsman polypropylene products are now produced by ..
Flexural Modulus 1.45 GPa
210 ksi
after 16 hours in 50°C water
Malvern Minerals Nylon with Novakup® L-337 Silane-Treated Quartz Filler
Product data demonstrates the effect of the Novakup® (lamellar quartz surface treated with A-1100) filler. A separate entry demonstrates the effect of untreated Novacite® filler in nylon. Th..
Flexural Modulus 1.45 GPa
210 ksi
ISO 178
Iran Petrochemical (PCC) S 30 S Polypropylene
This grade is for general injection molding applications.Applications: textile bobbins ,wheels ,fittings ,closures ,caps.Information provided by Iran Petrochemical Commercial Co.
Flexural Modulus 1.45 GPa
210 ksi
1% Secant; ASTM D790
IRPC Polimaxx Polene 2346NC Polypropylene Block Copolymer
CHARACTERISTICS: HIGH STIFFNESS, HIGH IMPACT, MEDIUM FLOW, HEAT STABILITY CONTAIN ANTISTATIC AND UV STABILIZER ADDITIVEAPPLICATIONS: INJECTION MOLDING FOR ELECTRICAL APPLIANCES, AUTOPARTS
Flexural Modulus 1.45 GPa
210 ksi
1% Secant, 0.05 in/min; ASTM D790
LyondellBasell Pro-faxâ„¢ SC973 Polypropylene Copolymer
Description: Pro-faxâ„¢ Ultra SC973 fully formulated (antistatic, nucleated, slip modified), very high melt flow, impact polypropylene reactor copolymer resin is designed for injection molding ap..
Flexural Modulus 1.45 GPa
210 ksi
ISO 178
Iran Petrochemical (PCC) S 30 G Polypropylene
The grade has combined excellent process ability with high stiffness.Applications: bags, mats, packing twines and ropes, drinking beakers packaging for dairy products.Information provided by Iran Pe..
Flexural Modulus 1.45 GPa
210 ksi
1% Secant; ASTM D790
IRPC Polimaxx Polene 1126NK Polypropylene Homopolymer
CHARACTERISTICS: GOOD EXTRUDABILITY, LOW GEL CONTAIN HIGH SLIP AND ANTIBLOCK ADDITIVES APPLICATIONS: TUBULAR BLOW FILM WATER QUENCH FOR GENERAL PURPOSE FILM, FOOD AND PACKAGING BAGS, GARMENT BAGS
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790
LyondellBasell Hifaxâ„¢ HSBMR246 Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ HSBMR246 medium high melt flow, 1,500 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an outstanding balance of physical pro..
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790
Techmer ES HiFill FR® PA6/6,6 GF NAT
Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: Natural ColorProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790
Techmer ES Statiblend® HIPS E
Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: Antistatic and ConductiveAppearance: Natural ColorProcessing Method: ExtrusionInformation provided by TP Composites, Inc.
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790
A. Schulman PP 1255-01 Polypropylene General Purpose Homopolymer Polypropylene
DescriptionPolypropylene PP 1255-01 Natural is a general purpose molding grade, with UL 94 HB approval, homopolymer polypropylene. ApplicationPolypropylene PP 1255-01 meets FDA Regulation 21 CFR 177..
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790
A. Schulman PP 1255-01 Polypropylene General Purpose Homopolymer Polypropylene
DescriptionPolypropylene PP 1255-01 Natural is a general purpose molding grade, with UL 94 HB approval, homopolymer polypropylene. ApplicationPolypropylene PP 1255-01 meets FDA Regulation 21 CFR 177..
Flexural Modulus 1.45 GPa
210 ksi
ISO 178-93
Wellman Wellamid® XT1867-BK1 High Impact Nylon 66
Description: High Impact Nylon 66Information provided by Wellman.
Flexural Modulus 1.45 GPa
210 ksi
ISO 527-2
Total PPH 7069 Polypropylene, Homopolymer
ATOFINA Polypropylene PPH 7069 is homopolymer.ApplicationATOFINA Polypropylene PPH 7069 is characterized by medium fluidity for extrusion of continuous filament (CF) and bulk continuous filament (BC..
Flexural Modulus 1.45 GPa
210 ksi
ASTM D 790
Total PPC 4944WZ Polypropylene, Impact Copolymer
ATOFINA 4944 polypropylene is a nucleated and controlled rheology impact copolymer. 4944WZ is characterized by improved stiffness and impact resistance, as well as low shrinkage and low warpage. I..
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790
A. Schulman POLYFORT™ FPP 1182E Talc Filled, Extrusion Grade Copolymer Polypropylene
DescriptionPolyfort® FPP 1182E is a 20% talc-filled, extrusion grade copolymer polypropylene. It had a good balance of flexural modulus, low temperature impact, and appearance properties. Informat..
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790M
DSM Somos® 9110 Epoxy Photopolymer
DescriptionDSM Somos® 9110 is a liquid photopolymer that produces robust, functional and accurate parts using stereolithography machines. The material offers superior chemical resistance, a wide p..
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790
Ensinger Tecaform™ SD Acetal (POM)
Ensinger-Hyde static dissipative acetal contains no carbon fibers or powders and is generally accepted for clean room use. With its surface resistivity of 109 to 1011 ohm/square and its excellent b..
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790
Ensinger TECAPRO™ MT Medical Grade Polypropylene (PP)
TECAPRO™ MT is an FDA approved homopolymer polypropylene based material with exceptionally low residual stress to facilitate the fabrication of dimensionally stable parts with varying cross section..
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790
Americas Styrenics EB6755 High Impact Polystyrene
Product CharacteristicsGood Environmental Stress Crack Resistance (ESCR)Good practical toughnessDeep draw thermoforming capableGood low temperature impactFood Contact CompliantTypical ApplicationsPa..
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790
Carmel Olefins CAPILENE® HU 75 AV Polypropylene Impact Copolymer
Description: CAPILENE® HU 75 AV is a nucleated and antistatic controlled rheology impact copolymer for injection molding. It is characterized by improved stiffness and medium impact resistance. ..
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790
Asahi Kasei Thermofil P-9900-0576 Unreinforced, Flame Retardant, Heat Stabilized
Information provided by Asahi Thermofil
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790
Aaron Industries AAROPRENE® CFIPP 2010 High Impact Calcium Carbonate Filled Polypropylene
AAROPRENE® CFIPP 2000 Series Reinforced CompoundsMelt flow index may be specified. Color may be specified.
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790A
Ineos H07D-00 Polypropylene Homopolymer
Grade H07D-00 is a polypropylene homopolymer for cast film applications that require slip and antiblock additives. This resin meets the requirements of the Food and Drug Administration as specified ..
Flexural Modulus 1.45 GPa
210 ksi
ASTM D790A
BP Amoco Acctuf® 3432 Impact Copolymer Polypropylene  (discontinued **)
Suggested fabrication methods: Injection moldingFeatures: Nucleated, AntistaticComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded samples.