| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 15.0 - 20.0 GPa | 2180 - 2900 ksi | Injection and Compression; ISO 178 |
|
Raschig Group EPOXIDUR® 3581 T-1 EP Epoxy, Molded, Glass Fiber Filler
Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Very ..
|
|||
| Flexural Modulus | 15.0 GPa | 2180 ksi | |
|
Cookson Group Plaskon® PPF-165A Molding Compound
(discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.A conventional molding compound specifically formulated for semiconductor devices which are molded with preplated leadframes. Lo..
|
|||
| Flexural Modulus | 15.0 GPa | 2180 ksi | ASTM D790 |
|
Solvay Specialty Polymers Ryton® R-4-230BL Polyphenylene Sulfide Compound
(Unverified Data**)
Black Polyphenylene Sulfide CompoundRyton® R-4-230BL is an advanced 40% fiberglass reinforced polyphenylene sulfide compound which provides reduced flash and improved processability compared to oth..
|
|||
| Flexural Modulus | 15.0 GPa | 2180 ksi | ASTM D790 |
|
Solvay Specialty Polymers Ryton® BR42B Polyphenylene Sulfide Compound
(Unverified Data**)
Natural Color Polyphenylene Sulfide CompoundRyton® BR42B is a 40% fiberglass reinforced polyphenylene sulfide compound specially formulated to have a low coefficient of friction for use in low surf..
|
|||
| Flexural Modulus | 15.0 GPa | 2180 ksi | ASTM D790 |
|
Chevron Phillips Ryton® BR42C Polyphenylene Sulfide Compound
(discontinued **)
Black Polyphenylene Sulfide CompoundRyton® BR42C is a 40% fiberglass reinforced polyphenylene sulfide compound specially formulated to have a low coefficient of friction for use in low surface fric..
|
|||
| Flexural Modulus | 15.0 GPa | 2180 ksi | |
|
Lehmann & Voss LUVOCOM® 1105-7442 PEEK, with carbon fiber, easy flowing
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts.High chemical resistance parts, hydrolysis resi..
|
|||
| Flexural Modulus | 15.0 GPa | 2180 ksi | |
|
Lehmann & Voss LUVOCOM® 1114-8364 PAEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Good friction and wear behaviour especially at increased temperatures.Electrically conduct..
|
|||
| Flexural Modulus | 15.0 GPa | 2180 ksi | |
|
Lehmann & Voss LUVOCOM® 1301-7293/GN PPS, linear, with glass fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Strong, stiff parts.High continuous use and heat distortion temperature. Non flammable.High chemic..
|
|||
| Flexural Modulus | 15.0 GPa | 2180 ksi | |
|
Lehmann & Voss LUVOCOM® 1-8490 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.High dimensionally stab..
|
|||
| Flexural Modulus | 15.0 GPa | 2180 ksi | ASTM D790 |
|
IDI Composites E-207 Thermoset Polyester, Sheet
ELECTRICAL - U.L. recognized (E53587). Versatile family of compounds designed to meet the most demanding electrical and electronic applications. Excellent dielectric properties and arc/track resista..
|
|||
| Flexural Modulus | 15.0 GPa | 2180 ksi | ASTM D790 |
|
Kuraray Genestarâ„¢ GW2458HF Nylon, 45% Glass Filled
Low Warpage, High Flow V-0 Grade. It is suited for low warpage and high flow applications, making it well suited for card connectors.
|
|||
| Flexural Modulus | 15.0 GPa | 2180 ksi | |
|
Lehmann & Voss LUVOCOM® 1106-8374 Polyether imide, with carbon fiber and PTFE
Applications: High-strength and high-stiff parts; low coefficient of expansion.High continuous use and heat distortion temperature. Non flammable.Dynamic stressed parts at high movement velocity.Hig..
|
|||
| Flexural Modulus | 15.0 GPa | 2180 ksi | ISO 178 |
|
SABIC Innovative Plastics LNP LUBRICOMP KCL34A Acetal Homopolymer
LNP* LUBRICOMP* KCL34A is a compound based on Acetal Homopolymer resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Electrically Conductive.
|
|||
| Flexural Modulus | 15.0 GPa | 2180 ksi | ISO 178 |
|
Solvay Specialty Polymers Omnix® 4050 Polyamide, High Performance (HPPA) (Dry)
Omnix® 4050 is a 50% glass-fiber reinforced, high-performance polyamide (HPPA). It is particularly suited for replacing die-cast metal in a variety of mechanical applications and components used ..
|
|||
| Flexural Modulus | 15.0 GPa | 2180 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP VERTON RV00AEU PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RV00AEU is a compound based on PA 66 resin containing Long Glass Fiber. Added features include : Easy Molding, UV Stabilized.
|
|||
| Flexural Modulus | 15.0 GPa | 2180 ksi | ISO 178 |
|
Unitika RUN35-C25 PA6, Dry
High modulus and low warpage nylonInformation provided by Unitika Ltd.
|
|||
| Flexural Modulus | 15.0 GPa | 2180 ksi | ASTM-D790 |
|
Polyram PlusTek PA303G50 Nylon 6.6, 50% Glass Fiber
50% glass fiber reinforced, heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Flexural Modulus | >= 15.0 GPa | >= 2180 ksi | IEC 1212-2 5.2 |
|
Hippe EP GM 203 Glass Mat Reinforced Epoxy Resin - Sheet |
|||
| Flexural Modulus | 15.0 GPa | 2180 ksi | DIN 53 457 |
|
Albis Plastics Tedur® L 9511 PPS, 45% Glass Fiber
High Strength, High Rigidity Standard Grade. Incandescent wire resistance (2 mm) is 960°C per VDE 0471 T1.2.Applications: Fixture Elements, HousingsProcessing: Injection Molding (Melt Temperature:..
|
|||
| Flexural Modulus | 15.0 GPa | 2180 ksi | ISO 178 |
|
Vyncolit Neopreg Kinel® SK60 L8G Glass Fiber Reinforced Molding Compound
High flow, epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particularly suited fo..
|
|||
| Flexural Modulus | 15.0 - 20.0 GPa | 2180 - 2900 ksi | Compression; ISO 178 |
|
Raschig Group RALUPOL® 8605 UP Polyester
Glass fiber reinforced polyester molding compound. Resistant to hydrolysis. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU dire..
|
|||
| Flexural Modulus | 15.0 GPa | 2180 ksi | ISO 178 |
|
Hexion Bakelite™ PF 4111 Phenolic Formaldehyde Resin, Improved Electrical Properties, Ammonia Free, Resistant to High Temperatures, Low Shrinkage, High Arc Resistance, UL Listed, Acetic Acid Free, Copper Adhesive
Phenolic molding compound, inorganically filled, glass fiber reinforced, ammonia and acetic acid free, electrically high grade, high temperature stability, high mechanical strength, copper-adhesive,..
|
|||
| Flexural Modulus | 15.0 GPa | 2180 ksi | ASTM D790 |
|
Solvay Specialty Polymers Ryton® R-4-200NA Polyphenylene Sulfide Compound
(Unverified Data**)
Natural Color Polyphenylene Sulfide CompoundRyton® R-4-200NA is an advanced 40% fiberglass reinforced polyphenylene sulfide compound developed to provide high strength, fast cycles, and low mainten..
|
|||
| Flexural Modulus | 15.0 GPa | 2180 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP VERTON RX06097 PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RX06097 is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding, UV-Stabilized.
|
|||