Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.55 GPa | 225 ksi | Tangent; ASTM D790 |
RheTech Products CC20P200-00 20% Calcium Carbonate Reinforced Polypropylene Copolymer, Natural Applications: Electrical housingsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
Polimeri Europa Sinkral® PD D 232/M4 ABS Resin Special very low gloss extrusion / co-extrusion grade, with good flow.Applications: Sinkral PD D 232/M4 is widely used in extrusion / co-extrusion of foils, when a very high matte appearance is req.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
Oxford Polymers 604-I Polycarbonate/Polybutylene Terephthalate (PBT) Alloy Polycarbonate/Polybutylene Terephthalate (PBT) AlloyInformation provided by Oxford Polymers. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 0.1 in/min; 0.250" thickness; ASTM D-790B |
Chevron Phillips EC6755 HIPS - High Impact Polystyrene
(discontinued **) Rubber modified high impact polystyrene.Applications:Containers and lidsPackaging for foods such as yot, sour cream, delicatessen salads and gravyCold temperature packagingPortion dairy containersFe.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
LATI LASTANE 50 G/25 25% Glass Fiber Reinforced Polyurethane (PUR)
(Unverified Data**) Description: Lastane thermoplastics are polyurethane (PUR) products. They exhibit good wear and impact resistance, even at low temperatures, noise inertness and excellent mould release. These proper.. |
|||
Flexural Modulus | 1.55 - 19.3 GPa | 225 - 2800 ksi | Average value: 2.35 GPa Grade Count:214 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Unreinforced". Each property range of values repor.. |
|||
Flexural Modulus | 1.55 GPa @Temperature 23.0 °C |
225 ksi @Temperature 73.4 °F |
ASTM D790A |
Ineos H20Z-00 Polypropylene Homopolymer This is a nucleated and antistatic homopolymer for injection molding applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.Appl.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 2 mm/min; ISO 178 |
Inno-Comp INNOPOL® CS 2-9000 MA B Polypropylene Copolymer INNOPOL® CS 2-9000 MA B is a black colored, high melt flow copolymer with antistatic additive.INNOPOL® CS 2-9000 MA B is developed for producing injection molded automotive components.All info.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 1% secant; ASTM D790-02 |
Ipiranga Petrochem PH 0361 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 1% secant; ASTM D790-02 |
Ipiranga Petrochem PH 1310 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
LyondellBasell Petrothene® LM600700 High Density Polyethylene (Blow Molding Grade) ApplicationsPETROTHENE LM 6007-00 resin exhibits very low taste and odor characteristics as well as good rigidity. Typical applications include water, and milk and juice bottles.Regulatory StatusLM.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 1% Secant; ASTM D790 |
IRPC Polimaxx Polene 1124NA Polypropylene Homopolymer CHARACTERISTICS: GOOD EXTRUDABILITY, LOW GEL CONTAIN LOW SLIP AND ANTIBLOCK ADDITIVES APPLICATIONS: CAST FILM AND TUBULAR BLOW FILM WATER QUENCH CPP FILM FOR FOOD PACKAGING, CPP FILM FOR LAMINATION |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Lubricomp FFL21 PE LNP* Lubricomp* FFL21 is a compound based on Polyethylene resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for t.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
Spartech Litho SP-2090 Polystyrene Sheet Description: Polystyrene SheetInformation provided by Spartech. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PPX PPX7110 PPE+PP (Asia Pacific) PPE+PP blend. High Impact, Good Heat Resistance |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL WCV072 PPE+PP Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | 1mm/min; ISO 527-2 |
Borealis HE125MO Polypropylene HE125MO is a polypropylene homopolymer intended for injection molding. This grade is characterized by good flow properties and high stiffness in and is specially suitable for high-speed injection mo.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ISO 178 |
Unipetrol PP MONSTEN® GB 005 Polypropylene Homopolymer Applications include injection molding, tapes, and thermoforming. Basic stabilization. Homopolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
Eastman Tritan MX710 Copolyester Eastman Tritan Copolyester MX710 is an amorphous product with excellent appearance and clarity. Eastman Tritan Copolyester MX710 has many outstanding features that include excellent toughness, hydr.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
Eastman Tritan MX711 Copolyester Eastman Tritan Copolyester MX711 is an amorphous product with excellent appearance and clarity. Eastman Tritan MX711 contains a mold release derived from vegetable based sources. Eastman Tritan Co.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
CPC - Vycom HITEC® HDPE High Density Polyethylene Hitec HDPE is a high impact, high density polyethylene sheet. It is ideally suited for the manufacture of chemical resistant products which come in direct contact with foodstuffs. Hitec meets the st.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790A |
CPC - Vycom PROTEC® Homopolymer Polypropylene Protec HP is a high corrosion resistant polypropylene material which exhibits excellent tensile strength and stiffness at elevated temperatures. Homopolymer polypropylene possesses excellent resista.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ISO 178 |
DuPont Performance Polymers Crastin® ST820 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Polybutylene Terephthalate with Excellent Impact Resistance Crastin ST820 NC010 is an unreinforced Super Tough polybutylene terephthalate resin for injection molding.Information provide.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
Entec Hypel® PEHD.7/.962 HDPE Available in North America Features: Food Contact Acceptable and High DensityAgency Ratings: FDA 21 CFR 177.1520RoHS Compliant Form: Pellets Information provided by Entec |
|||
Flexural Modulus | >= 1.55 GPa | >= 225 ksi | ASTM D790 |
Buckeye Polymers BP RPP 3015 T NAT Polypropylene, Talc Filled Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and .. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
Carmel Olefins CAPILENE® G 65 F Polypropylene Homopolymer Description: CAPILENE® G 65 F is a polypropylene homopolymer designed for the production of biaxially oriented polypropylene films (BOPP). It exhibits good processability, easy film stretchabilit.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
Multibase Multi-Flam™ 0103 HDPE NH Polyethylene Features:Flame RetardantHalogen Content, Low to None Forms:PelletsProcessing Methods:Injection MoldingCoextrusionExtrusionUses:TubingPipingInformation provided by Multibase |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ISO 178 |
Unipetrol PP MONSTEN® GB 107 Polypropylene Homopolymer Made for injection molding. Basic stabilization. Homopolymer.Information provided by Unipetrol RPA |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | tangent; ASTM D790 |
Spartech PP7240 Calcium Carbonate Filled High Impact Copolymer Provides the highest level of impact of all copolymers and are useful in applications where improved processing and stiffness are required versus unfilled copolymer materials.Information provided by.. |
|||
Flexural Modulus | 1.55 GPa | 225 ksi | ASTM D790 |
Teknor Apex Sinpolene CPP2030 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Calcium Carbonate Filler, 30% Filler by Weight Features: Copolymer Uses: Automotive Applications; Industrial Applicati.. |