| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 16.0 - 18.0 GPa | 2320 - 2610 ksi | Injection; ISO 178 |
|
Raschig Group 2557 AMC Polyester
Glass fiber reinforced polyester molding compound. Very good mechanical strength, very good electrical properties and dimensional stability, exceptional processability with short cycle time and low ..
|
|||
| Flexural Modulus | 16.0 - 20.0 GPa | 2320 - 2900 ksi | Compression; ISO 178 |
|
Raschig Group RALUPOL® 4566 UP Polyester
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, good electrical values, excellent heat resistance, outstanding pourability. This product meets the allowed u..
|
|||
| Flexural Modulus | 16.0 GPa | 2320 ksi | ASTM D790 |
|
Resinoid 1370 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
|
|||
| Flexural Modulus | 16.0 - 18.0 GPa | 2320 - 2610 ksi | Compression; ISO 178 |
|
Raschig Group RESINOL® 87120 EPF Phenolic
Glass-fiber reinforced phenolic molding compound. Excellent heat resistance, low mould shrinkage and post-shrinkage, good chemical resistance and very good mechanical properties. This product meets ..
|
|||
| Flexural Modulus | 16.0 - 19.0 GPa | 2320 - 2760 ksi | Injection; ISO 178 |
|
Raschig Group SURAPLAST UPA 63 UP
Glass fiber reinforced polyester molding compound. Minimal mold shrinkage and post-shrinkage, very good arc resistance, very good mechanical strength. This product meets the allowed upper limits for..
|
|||
| Flexural Modulus | 16.0 GPa | 2320 ksi | ASTM D790 |
|
LNP Stat-Kon® EC-1004 Polyetherimide, Carbon Fiber Reinforcement
(discontinued **)
Features: Electrically ConductiveForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades..
|
|||
| Flexural Modulus | 16.0 GPa | 2320 ksi | |
|
Cookson Group Plaskon® 3300SH Mineral Filled Epoxy Molding Compound
(discontinued **)
Test specimens were transfer molded and post cured 4 hours at 175°C.Exhibits exceptional reliability, excellent moldability, good release characteristics and low flash. This compound is especially..
|
|||
| Flexural Modulus | 16.0 GPa | 2320 ksi | ISO 178 |
|
Chevron Phillips Xtel® XK2760BL Polyphenylene Sulfide Alloy
(discontinued **)
Xtel® XK2760BL is a high performance, glass fiber and mineral filled PPS based alloy developed to provide excellent mechanical strength with a unique blend of toughness, rigidity, and low flash cha..
|
|||
| Flexural Modulus | 16.0 GPa | 2320 ksi | |
|
Lehmann & Voss LUVOCOM® 1301/CF/20 PPS, linear, with carbon fiber
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High continuous use and heat distortion temperature. Non flammable.High-strength and stiff parts w..
|
|||
| Flexural Modulus | 16.0 GPa | 2320 ksi | |
|
Lehmann & Voss LUVOCOM® 20-8368 Polyphthalamide, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Low influence from moisture and temperature to measures and electrical prop..
|
|||
| Flexural Modulus | 16.0 GPa | 2320 ksi | |
|
Lehmann & Voss LUVOCOM® 80-7727 Polyacetal-copolymer, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts; low thermal coefficient of expansion.Electrically conductive, suitable for..
|
|||
| Flexural Modulus | 16.0 GPa | 2320 ksi | |
|
Lehmann & Voss LUVOCOM® 80-7752 Polyacetal-copolymer, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita..
|
|||
| Flexural Modulus | 16.0 GPa | 2320 ksi | ASTM D790 |
|
Solvay TECHNYLSTARâ„¢ AFX 218S V50 PA6, 50% glass filled, DRY
Description: High stiffness materials TECHNYLSTAR Polyamide 66, reinforced with 50% of glass fiber, heat stabilized for injection molding. Characterized by a high fluidity of the melt. Available in:..
|
|||
| Flexural Modulus | 16.0 GPa | 2320 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
|
SABIC Innovative Plastics LNP Stat-kon EX08308C PEI (Asia Pacific)
Stat-Kon* EX08308C is a high cleanliness Polyetherimide Compound reinforced with Carbon Fiber for use in applications requiring the highest level of cleanliness. This compound is compounded using LN..
|
|||
| Flexural Modulus | 16.0 GPa | 2320 ksi | ISO 178 |
|
Sumitomo Bakelite North America RX® 611 Fiberglass Reinforced Phenolic
RXÂ 611 is a fiberglass reinforced phenolic molding compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type MFH.Information supplied by Sumitomo..
|
|||
| Flexural Modulus | 16.0 GPa | 2320 ksi | ASTM D790 |
|
Toyobo Vylopet® EMC145 Glass Reinforced Polyester, Standard Grade
Key Feature: Flame retardant V-0 UL-94 classApplications: Ultra-precise componentsGeneral features of Vylopet® include heat resistance, good mechanical properties, high dielectric strength and trac..
|
|||
| Flexural Modulus | 16.0 GPa | 2320 ksi | ISO 178 |
|
Vyncolit A2990 Glass Fiber Reinforced Novolac Phenolic
Resole resin based, glass fiber reinforced. Good mechanical properties, combined with superior electrical insulation properties. Among others used for commutator applicationsInformation provided by ..
|
|||
| Flexural Modulus | 16.0 GPa | 2320 ksi | ISO 178 |
|
Vyncolit G865 Novolac Phenolic
Glass fiber filled phenolic molding compound with high mechanical, good thermal and electrical properties. USES: Asbestos-free replacement for die-cast automotive metal parts, e.g. reactors for aut..
|
|||
| Flexural Modulus | 16.0 GPa | 2320 ksi | tangent; chs 0.05 in/min; ASTM D790 |
|
Diamond Polymers Centrex® 833 Sheet Extrusion Grade
Centrex 833 resin is a high-gloss, high-impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, and it ..
|
|||
| Flexural Modulus | 16.0 GPa | 2320 ksi | ISO 178 |
|
Eurostar Star L PA66 30Y D51 PA66, Carbon Fiber Filled, Injection Molded
Star L PA66 30Y D51 is a PTFE Lubricated, Carbon Fiber Reinforced, Polyamide 66 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Flexural Modulus | 16.0 GPa | 2320 ksi | ISO 178 |
|
Ascend Performance Materials Vydyne® R550H Nylon 66, 50% Glass Reinforced, DAM
Vydyne® R550H is general-purpose, heat-stabilized, hydrolysis-resistant, 50% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of physic..
|
|||
| Flexural Modulus | 16.0 GPa | 2320 ksi | ASTM D790 |
|
A. Schulman ComAlloy E-16674B PPS, Electrically Conductive - Carbon Fiber Filled
Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Flexural Modulus | 16.0 GPa | 2320 ksi | ASTM D790 |
|
LATI LARPEEK 50 G/50 50% Glass Reinforced Polyetheretherketone (PEEK)
(discontinued **)
Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°..
|
|||
| Flexural Modulus | 16.0 GPa | 2320 ksi | ASTM D790 |
|
Resinoid 1329 Phenolic Molding, Glass Reinforced
Data provided by the manufacturer.The Resinoid 1300 and 7000 glass fiber reinforced series compounds feature mechanical strength, dimensional stability, electrical insulation, and heat resistance
|
|||
| Flexural Modulus | 16.0 GPa | 2320 ksi | ASTM D790 |
|
Sumitomo Bakelite North America Epiall® 1961B-1 Mineral and Glass Filled Electrical Encapsulation Grade Epoxy
Epiall 1961B-1 is a short glass fiber and mineral filled epoxy molding compound with excellent dimensional stability, good strength properties, and good electrical insulation properties.Information ..
|
|||