Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 2900 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Modulus 20.0 - 22.0 GPa
2900 - 3190 ksi
ISO 178
Raschig Group EN 5007 Epoxy Molding Compound
Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo..
Flexural Modulus 20.0 - 23.0 GPa
2900 - 3340 ksi
Injection and Compression; ISO 178
Raschig Group EPOXIDUR® 3582 EP Epoxy
Glass-fiber reinforced and inorganically filled epoxy molding compound. Good mechanical strength, very good electrical isolation properties and dimensional stability even at high temperatures. Moldi..
Flexural Modulus 20.0 GPa
2900 ksi
ISO 178
Gharda Chemicals GATONE™ PEEK, 30% Carbon Fiber Reinforced  (discontinued **)
GATONE™ PEEK grades with carbon fiber reinforcements ranging from 10- 40 % are available in natural or desired color. Custom made grades can be developed to meet specific requirements.CHARACTERISTI..
Flexural Modulus 20.0 GPa
2900 ksi
ASTM D790
LATI LARPEEK 50 G/60 60% Glass Reinforced Polyetheretherketone (PEEK)  (discontinued **)
Larpeek polyetheretherketone (PEEK) is a high performance thermoplastic offering cost effective performance in difficult environments across all industries. PEEK is temperature resistant (up to 250°..
Flexural Modulus 20.0 GPa

@Temperature 23.0 °C
2900 ksi

@Temperature 73.4 °F
ISO 178
Victrex® PEEK 90HMF20 Polyetheretherketone (PEEK), 20% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 20% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, color black.T..
Flexural Modulus 20.0 GPa
2900 ksi
Lehmann & Voss LUVOCOM® 1105-7995 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
Flexural Modulus 20.0 GPa
2900 ksi
Lehmann & Voss LUVOCOM® 1-7791 Polyamide 66, with carbon fiber, PTFE, lubricant modified, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wear beh..
Flexural Modulus 20.0 GPa
2900 ksi
Lehmann & Voss LUVOCOM® 1800-8449 PET, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and stiff parts with low creep.Electrically conductive, suitable for continuous d..
Flexural Modulus 20.0 GPa
2900 ksi
Lehmann & Voss LUVOCOM® 204-8468 Polyphthalamide, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
Flexural Modulus 20.0 GPa
2900 ksi
Lehmann & Voss LUVOCOM® 20-7638 Polyphthalamide, with carbon fiber and PTFE
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
Flexural Modulus 20.0 GPa
2900 ksi
Lehmann & Voss LUVOCOM® 21-8015 Polyamide 6/6T, with carbon fiber
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive..
Flexural Modulus 20.0 GPa
2900 ksi
Lehmann & Voss LUVOCOM® 1105-0699-1 PEEK, with carbon fiber, PTFE, lubricant modified
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Improved friction and wea..
Flexural Modulus 20.0 GPa
2900 ksi
ASTM D790
Techmer ES HiFill® PA6 GF60 HS L 60% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformati..
Flexural Modulus 20.0 GPa
2900 ksi
ISO 178
SABIC Innovative Plastics LNP Thermocomp RF00CS PA 66
LNP* Thermocomp* RF00CS is a compound based on Nylon 66 resin containing Glass Fiber. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Americas re..
Flexural Modulus 20.0 GPa
2900 ksi
ASTM D790
Sumitomo Bakelite North America E 264H Long Glass Fiber Reinforced Epoxy
E 264H is a high strength, long fiberglass reinforced epoxy molding compound, which features improved flow in transfer molding.Information provided by Sumitomo Bak North America, Inc.
Flexural Modulus 20.0 GPa
2900 ksi
ASTM D790
Sumitomo Bakelite North America E 8354A-1 Short Glass Fiber Reinforced Epoxy
E 8354A-1 is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Sumito..
Flexural Modulus 20.0 GPa
2900 ksi
ASTM D790
Sumitomo Bakelite North America E 8354A-2 Short Glass Fiber Reinforced Epoxy
E 8354A-2 is a fiberglass and mineral reinforced epoxy molding compound, with excellent dimensional stability, good electrical insulation properties, and good strength.Information provided by Sumito..
Flexural Modulus 20.0 GPa
2900 ksi
ASTM D790
Sumitomo Bakelite North America RX® 3-1-530-P Long-Glass Reinforced Diallyl Phthalate
Long glass fiber reinforced, flame retardant, diallyl ortho-phthalate molding compound which meets the requirements of ASTM D5948 Type GDI-30F.Information provided by Vyncolit, a Sumitomo Bak Group
Flexural Modulus 20.0 GPa
2900 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP RF00CSXZ PA 66
LNP* THERMOCOMP* RF00CSXZ is a compound based on Recycled Nylon 66 resin containing 60% Glass Fiber. Added features of this material include: Heat Stabilized.
Flexural Modulus 20.0 GPa
2900 ksi
ISO 178
Sumitomo Bakelite North America RX® 865M Fiberglass Reinforced Phenolic Novolac
RX 865M is a fiberglass reinforced phenolic novolac compound, featuring dimensional stability, moderate impact resistance, and good strength and modulus.Information supplied by Sumitomo Bak North Am..
Flexural Modulus 20.0 GPa
2900 ksi
ASTM D790
PolyOne Lubri-Tech™ AM-30CF/15T Polyphthalamide (PPA), Carbon Fiber Reinforced, PTFE Lubricated  (discontinued
Description/Features:Carbon Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Copyright © lookpolymers.com All Rights Reserved