Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 297 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Modulus 2.05 GPa
297 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS
High impact PC+ABS material designed for local Pacific Automotive applications
Flexural Modulus 2.05 GPa
297 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® BFL4000U PC (Europe-Africa-Middle East)
Lexan* BFL4000U Polycarbonate resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating and good impact/flow balance. Designed fo..
Flexural Modulus 2.05 GPa
297 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® FL3000 PC (Europe-Africa-Middle East)
FL3000 is an FR product with excellent low temperature impact, bromine and chlorine free, good retention of properties upon weathering.This data was supplied by SABIC-IP for the Europe-Africa-Middle..
Flexural Modulus 2.05 GPa
297 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer (Asia Pacific)
Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul..
Flexural Modulus 2.05 GPa
297 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Lexan® FXE1414L PC Copolymer (Europe-Africa-Middle East)
Opaque EXL, UV-Stabilized & light shielding capability (Wall thickness >0.8mm), for portable electronics device enclosure application. Only available in white, grey and limited pastel colors. Consul..
Flexural Modulus 2.05 GPa
297 ksi
2 mm/min; ISO 178
Inno-Comp INNOPOL® CS 3-9230 KAR YU UV-Stabilized, 26% Mineral-Filled Compound Blend Of Polypropylene Homopolymer And Block-Copolymer
INNOPOL® CS 3-9230 KAR YU is a yellow colored, UV-stabilized, 26% mineral-filled compound based on a blend of polypropylene homopolymer and block-copolymer.INNOPOL® CS 3-9230 KAR YU is develop..
Flexural Modulus 2.05 GPa
297 ksi
ASTM D790
SABIC Innovative Plastics NORYL STN15 PPE+HIPS (Asia Pacific)
PPE+HIPS Unfilled Auto Interior
Flexural Modulus 2.05 GPa
297 ksi
2 mm/min, 64mm span; ISO 178
SABIC Innovative Plastics SABIC PPCOMPOUND 7727 PP
SABIC® PPcompound 7727 is a mineral filled, impact modified polypropylene TPO. This material combines impact resistance, heat stability, and is used in injection molded applications. The IMDS ID..
Flexural Modulus 2.05 GPa
297 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® IQ357 PBT+PC
Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified.
Flexural Modulus 2.05 GPa
297 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Asia Pacific)
Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified.
Flexural Modulus 2.05 GPa
297 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® IQ357M PBT+PC
Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release.
Flexural Modulus 2.05 GPa
297 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® IQ357U PBT+PC
Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin.
Flexural Modulus 2.05 GPa
297 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® IQ357U PBT+PC (Asia Pacific)
Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin.
Flexural Modulus 2.05 GPa
297 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Europe-Africa-Middle East)
Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom..
Flexural Modulus 2.05 GPa
297 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® CL100 PBT+PC (Europe-Africa-Middle East)
Xenoy CL100 is an unfilled, impact modified, UV-stabilized PC/PBT blend with excellent solvent resistance and good low-temperature ductility. It has a proven track record in unpainted exterior autom..
Flexural Modulus 2.05 GPa
297 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Asia Pacific)
Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing..
Flexural Modulus 2.05 GPa
297 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Xenoy® HX5600HP PBT+PC (Europe-Africa-Middle East)
Xenoy HX5600HP is PBT based semi-crystalline blend with balanced flow and impact properties. Improved chemical resistance against lab disinfectants and chemicals for healthcare enclosure and housing..
Flexural Modulus 2.05 GPa
297 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Xylex X8419 PC+POLYESTER
Low-medium flow, suitable for blow molding, injection molding, extrusion.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.05 GPa
297 ksi
ISO 178
Styrolution Novodur® M210TF ABS
Novodur M210TF is medium impact, high gloss injection molding grade designed for toy application. M210TF is in compliance with food contact regulationsInformation provided by Styrolution
Flexural Modulus 2.05 GPa
297 ksi
ASTM Test
Styrolution Terluran® HI-10 ABS
Terluran HI-10 is an injection molding and extrusion grade of ABS with very high toughness and medium flow.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
Flexural Modulus 2.05 GPa
297 ksi
3-point, 2 mm/min; ISO 178
Styron MAGNUMâ„¢ 3416 SLG Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: The mass (continuous process) ABS technology of Styron ensures an ABS resin that combines excellent processability with a stable light base color providing an ideal resin for self coloring..
Flexural Modulus 2.05 GPa
297 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL GTX GTX974 PPE+PA (Europe-Africa-Middle East)
NORYL GTX974 is a material especially designed for in- or on-line painted bodypanels and fenders in particular. This material combines impact performance with conductivity for electro-static paintin..
Flexural Modulus 2.05 GPa
297 ksi
2.6 mm/min, 100 mm span; ASTM D790
SABIC Innovative Plastics NORYL NWP100 PPE+HIPS (Asia Pacific)
PPO/HIPS Unfilled high impact extrusion grade
Flexural Modulus 2.05 GPa
297 ksi
ASTM D790
SABIC Innovative Plastics NORYL GTX GTX600 PPE+PA6 (Asia Pacific)
Pa6 based unfilled GTX
Flexural Modulus 2.05 GPa
297 ksi
ISO 178
Polyplastics Duracon® WR-01 Acetal Co-polymer (POM), Chlorine water resistance
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
Flexural Modulus 2.05 GPa
297 ksi
2mm/min; ASTM D790
Denka TH-23 Transparent Resin Polymer (MBS resin) Polymethacrylate Butadiene Styrene
"TX Polymer" (methyl methacrylate styrene), MS resins as an alternative to acrylic resins, with low density, low moisture absorption, and good moldability, "TH Polymer/TP Polymer," MBS resins with a..
Flexural Modulus 2.05 GPa
297 ksi
ISO 178
Clariant Renol PA1SP0003 Nylon 66, PE Modified
Reduced Coefficient of FrictionData provided by Clariant Masterbatches
Flexural Modulus 2.05 GPa
297 ksi
DAM; ISO 178
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612  (Unverified Data**)
Unreinforced Polyamide 612Information provided by DuPont Performance Polymers
Flexural Modulus 2.05 GPa
297 ksi
ASTM D790
Ineos Nova Zylar® 631 Clear Impact Modified Acrylic Copolymer  (discontinued **)
Features:Outstanding practical toughness and ductilityStyrenic processing advantagesExcellent property retention after ETO and gamma sterilizationUSP Class VI compliantCustom colors and enhancement ..