Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 3.65 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Modulus 3.65 GPa
529 ksi
Plastcom SLOVAMID 66 C 15 MI PA66, 15% mineral filling
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0..
Flexural Modulus 3.65 GPa
529 ksi
Plastcom SLOVAMID 66 T 15 MI PA66, 15% mineral filling
FeaturesPA 66 with the content of 15 % chemically modified mineral filling and impact modified. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat produc..
Flexural Modulus 3.65 GPa
529 ksi
ASTM D790
Polymer Resources PPX-G10HF Modified-PPO, 10% Glass Reinforced, High Flow
Modified-Polyphenylene Oxide, 10% Glass Reinforced, High FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inf..
Flexural Modulus 3.65 GPa
529 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Cycoloy® CM8622 PC+ABS (Europe-Africa-Middle East)
CYCOLOY* CM8622 is a high heat PC/ABS blend offering high modulus, low CTE and good
Flexural Modulus 3.65 GPa
530 ksi
Tangent; ASTM D790
Fiberfil® PP-60/TC/40 Polypropylene Homopolymer, 40% Talc Filled
Information provided by FIBERFIL Engineered Plastics
Flexural Modulus 3.65 GPa
529 ksi
ISO 178
Solvay TECHNYL® B 50 H1 PA66/6, DRY
Description: TECHNYL® B 50H1 is an unreinforced melamine cyanurate flame retarded copolyamide 66/6. This product has been heat stabilized and is suitable for injection molding. This product is av..
Flexural Modulus 3.65 GPa
529 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP ZFL31XXC PPE+PS
LNP* LUBRICOMP* ZFL31XXC is a compound based on PPE+PS resin containing 5% Glass Fiber, 15% PTFE. Added features of this material include: Wear Resistant
Flexural Modulus 3.65 GPa
530 ksi
ASTM D790
Techmer ES Electrablend® PA6/6 IM C BK
Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/Reinfor.Additive: Impact ModifierFeatures: Conductive and Impact ModifiedAppearance: BlackInformation provided by TP..
Flexural Modulus 3.65 GPa
530 ksi
secant; ASTM D790
Spartech PP5420 Glass Fiber Reinforced Homopolymer
Provides the maximum strength and heat resistance among polypropylene compounds. Physical properties can approach those of more expensive engineering resins.Information provided by Spartech
Flexural Modulus 3.65 GPa
530 ksi
ASTM D790
Techmer ES HiFill® PA6/6 GF10 L 10% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by Weight Additive: LubricantFeatures: LubricatedInformation provided by TP Composites, Inc.
Flexural Modulus 3.65 GPa
530 ksi
ASTM D790
Techmer ES HiFill® PA6/6 GF6 HS BK 6% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 6% Filler by WeighAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance:..
Flexural Modulus 3.65 GPa
530 ksi
ASTM D790
Techmer ES Luriblend® PA6 GL15 Nylon 6
Availability: North AmericaForms: PelletsAdditive: Graphite Powder Lubricant(15%)Features: LubricatedInformation provided by TP Composites, Inc.
Flexural Modulus 3.65 GPa
530 ksi
0.125 in, injection molded, unannealed; ASTM D790
Styron EMERGEâ„¢ 4731-8 Polycarbonate
EMERGEâ„¢ PC 4702-15 advanced resin is formulated with 10% glass fiber and has an f1 rating by Underwriters Laboratories Inc. It provides good ignition resistance, rigidity, dimension stability ..
Flexural Modulus 3.65 GPa
529 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Valox® SHF4910 PBT (Europe-Africa-Middle East)
6.5% glass reinforced, Super High Flow, flame retardant PBT.
Flexural Modulus 3.65 GPa
529 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Valox® SHF4910 PBT (Europe-Africa-Middle East)
6.5% glass reinforced, Super High Flow, flame retardant PBT.
Flexural Modulus 3.65 GPa
529 ksi
ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP NF001 PC+ABS (Asia Pacific)
LNP* Thermocomp* NF001 is a compound based on PC+ABS Blend resin containing Glass Fiber.
Flexural Modulus 3.65 GPa

@Temperature 22.8 °C
530 ksi

@Temperature 73.0 °F
ASTM D790
Ensinger Tecapeek® Polyetheretherketone (PEEK)
TECAPEEK™ high performance polymer, made from Victrex PEEK polymer, has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's excepti..
Flexural Modulus 3.65 GPa
530 ksi
ASTM D790
Asahi Kasei Thermylene® P6-20FG-0153 20% Glass Fiber Reinforced, UV Stable
Information provided by Asahi Thermofil
Flexural Modulus 3.65 GPa
530 ksi
ASTM D790
Asahi Kasei Thermylene® P6-30FG-0877A 30% Glass Fiber Reinforced, UV Stabilized
Information provided by Asahi Thermofil
Flexural Modulus 3.65 GPa
530 ksi
ASTM D790
Asahi Kasei Thermylene® P6-40FB-Y947 40% Glass Fiber/Glass Bead, Heat Stabilized
Information provided by Asahi Thermofil
Flexural Modulus 3.65 GPa
530 ksi
ASTM D790
ScanTube PEEK Tubing
Information provided by ScanTube, Inc.
Flexural Modulus 3.65 - 11.4 GPa
530 - 1650 ksi
Average value: 9.18 GPa Grade Count:50
Overview of materials for Polyethylene Terephthalate (PET), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 30% Glass Reinforced". Specific grades with glass content between 25% ..
Flexural Modulus 3.65 - 5.03 GPa
530 - 730 ksi
Bulk Molding Compounds BMC T60-6006 Wear Resistant Molding Compound
BMC T60-6006 is a wear resistant molding compound specifically formulated for applications that require excellent abrasion resistance. Due to its low specific gravity it has substantial cost per cu..
Copyright © lookpolymers.com All Rights Reserved