| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 3.80 GPa | 551 ksi | ISO 178, ASTM D790 |
|
Nilit Nilamid A3 H G3 ZB 13% Glass Reinforced High Impact PA66
Description: Nilamid A3 H G3 ZB (13% Glass Reinforced) was developed for applications that require a combination of high stiffness and good elongation or impact resistance. It is widely used for app..
|
|||
| Flexural Modulus |
3.80
GPa <br>@Temperature 90.0 °C
|
551
ksi <br>@Temperature 194 °F
|
ISO 178, ASTM D790 |
|
Nilit Nilamon B3 H7 GK 35 15% Glass Fiber, 25% Mineral Reinforced PA6
Description: Nilamon B3 H7 GK 35 provides a combination between low warpage and high stiffness, while retaining a good impact strength. It has a high heat aging resistance, so that it is suitable fo..
|
|||
| Flexural Modulus | 3.80 GPa | 551 ksi | ISO 178 |
|
Nilit FRIANYL A63 H-KV30 Nylon 6.6 for injection molding, 30% glass ball reinforced
Nylon 6.6 for injection molding, heat stabilized (dark natural color).Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Flexural Modulus |
3.80
GPa <br>@Temperature 23.0 °C
|
551
ksi <br>@Temperature 73.4 °F
|
ISO 178 |
|
Polykemi AB POLYfill PPH T8040 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Flexural Modulus | 3.80 GPa | 551 ksi | ISO 178 |
|
Nilit FRIANYL B63 H-KV30 Nylon 6 for injection molding, 30% glass ball reinforced
Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Flexural Modulus | 3.80 GPa | 551 ksi | ASTM D790 |
|
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)
(Unverified Data**)
KetaSpire KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire PEEK is produced to the highest industry standards and is characterized by a dist..
|
|||
| Flexural Modulus |
3.80
GPa <br>@Temperature 23.0 °C
|
551
ksi <br>@Temperature 73.4 °F
|
ISO 178 |
|
Polykemi AB POLYfill PPH GF5020 PD1 VT2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled, Heat Stabilized
Information provided by Polykemi AB
|
|||
| Flexural Modulus |
3.80
GPa <br>@Temperature 23.0 °C
|
551
ksi <br>@Temperature 73.4 °F
|
ISO 178 |
|
Polykemi AB POLYfill PPH T1040 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Flexural Modulus |
3.80
GPa <br>@Temperature 23.0 °C
|
551
ksi <br>@Temperature 73.4 °F
|
ISO 178 |
|
Polykemi AB POLYfill PPH T2040 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Flexural Modulus | 3.80 GPa | 551 ksi | ISO 178 |
|
Victrex® PEEK 450G General Purpose
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, FDA food contac..
|
|||
| Flexural Modulus | 3.80 GPa | 551 ksi | ISO 527 |
|
Victrex® PEEK 450PF Fine Powder Grade
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression molding, standard flow, FDA food contact complia..
|
|||
| Flexural Modulus | 3.80 GPa | 551 ksi | 2 mm/min; ISO 178 |
|
Ineos ABS Lustran® SAN C Injection Molding Grade |
|||
| Flexural Modulus | 3.80 GPa | 551 ksi | ISO 178 |
|
MRC Polymers NAXALOYâ„¢ 770 GF10 ABS+PC Alloy, 10% Glass Fiber Filled
Can be UV StabilizedInternal and external lubricant can be addedInformation provided by MRC Polymers Inc.
|
|||
| Flexural Modulus | 3.80 GPa | 551 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics NORYL V02570 PPE+HIPS (Asia Pacific)
Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t..
|
|||
| Flexural Modulus | 3.80 GPa | 551 ksi | ASTM D790 |
|
Solvay Specialty Polymers KetaSpire® KT-880FP Polyetheretherketone (PEEK)
KetaSpire® KT-880FP is the high-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural color fine powder form for compression molding and other uses that can benefit from th..
|
|||
| Flexural Modulus | 3.80 GPa | 551 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics Valox® 4012G PBT (Europe-Africa-Middle East)
VALOX 4012G is a 10% glass fibre reinforced PBT injection moulding resin with excellent mechanical properties. Applications: connectors. This grade is a 4012 with improved cycle time and ductility.
|
|||
| Flexural Modulus | 3.80 GPa | 551 ksi | 2mm/min; ISO 178 |
|
Teijin Multilon DN-3510F Filler Reinforced Type, Halogen-Free Flame Resistant PC/ABS Polymer Alloy
Halogen-free flame retardant PC/ABS polymer alloy, and is also antimony-free. It has improved stiffness through the addition of 10 % filler. Improved stiffness and high fluidity realizes a thin wall..
|
|||
| Flexural Modulus | 3.80 GPa | 551 ksi | ISO 178 |
|
Wellman Wellamid® GFT13-66 XE-N 13% Impact Modified Glass Reinforced Nylon 66/6, Lubricated & Heat Stabilized
Typical Applications: Machinery gear trains and linkage, conveyor belt links, fasteners, auto under hood and door parts, automotive door handles, appliance parts, sporting goods, lawn and garden equ..
|
|||
| Flexural Modulus | 3.80 GPa | 551 ksi | |
|
Hexcel® HexPly® M34 75°C (167°F) Curing Epoxy Matrix
HexPly® M34 is an epoxy system, specifically developed for low temperature curing of large structural components, particularly in industrial markets. HexPly® M34 is a self-extinguishing system, pr..
|
|||
| Flexural Modulus | 3.80 GPa | 551 ksi | ISO 178 |
|
Polyram RamOfin PPH343T8 Polypropylene, 40% Mineral Filled
40% Mineral filled polypropylene for injection molding applications.Information provided by Polyram.
|
|||
| Flexural Modulus | 3.80 GPa | 551 ksi | ASTM-D790 |
|
Polyram RamShine PV102 ABS, General Purpose
General purpose ABS for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Flexural Modulus | 3.80 GPa | 551 ksi | ASTM D 790 |
|
Cossa Polimeri ESTAPROP HK 1280 T8 Polypropylene, 40% Mineral Filled
PP homopolymer 40% mineral fillerExcellent physical and mechanical characteristics, good surface appearanceInformation provided by Cossa Polimeri S.r.l.
|
|||
| Flexural Modulus | 3.80 GPa | 551 ksi | ASTM D790 |
|
Aclo Accutech Polypropylene CP0437T40V Copolymer Talc Reinforced
Approved to GMP.PP.079 Black A12566
|
|||
| Flexural Modulus | 3.80 GPa | 551 ksi | ASTM D790 |
|
Adell AJ-33 Nylon 66, 15% Glass Reinforced; High Impact
Data provided by Adell Plastics, Inc.
|
|||
| Flexural Modulus |
3.80
GPa <br>@Temperature 23.0 °C
|
551
ksi <br>@Temperature 73.4 °F
|
ISO 178 |
|
Polykemi AB POLYfill PPH T5040DS Polypropylene Homopolymer, Mineral Reinforced, Detergent Resistant
Information provided by Polykemi AB
|
|||
| Flexural Modulus | 3.80 - 24.1 GPa | 551 - 3500 ksi | Average value: 9.61 GPa Grade Count:155 |
|
Overview of materials for Polyetheretherketone, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum..
|
|||
| Flexural Modulus | 3.80 GPa | 551 ksi | ISO 178 |
|
Polyplastics Duracon® GB-25 Acetal Co-polymer (POM), Low warpage, GB 25% filling
DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O)..
|
|||
| Flexural Modulus | 3.80 GPa | 551 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics NORYL GTX GTX6203 PPE+PA (Europe-Africa-Middle East)
NORYL GTX6203 is a 20% talc filled material with superior dimensional stability, excellent processability and surface appearance.
|
|||
| Flexural Modulus | 3.80 GPa | 551 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics NORYL PX2391 PPE+HIPS (Europe-Africa-Middle East)
PX2391 is a 10% glass fiber reinforced, heat stabilized, low odor and low emission NORYL(R) grade for interior automotive applications, especially instrument panels
|
|||
| Flexural Modulus |
3.80
GPa <br>@Temperature 23.0 °C
|
551
ksi <br>@Temperature 73.4 °F
|
ISO 178 |
|
Polykemi AB POLYfill PPH T5040 FC VT Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
|
|||