| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 3.90 GPa | 566 ksi | ISO 178 |
|
Nilit FRIANYL A63 SG40 Nylon 6.6 for injection molding, 40% mineral filled
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Flexural Modulus | 3.90 GPa | 566 ksi | ISO 178 |
|
Nilit FRIANYL B63 AL40 Nylon 6.6 for injection molding, 40% aluminum filled
Nylon 6.6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Flexural Modulus | 3.90 GPa | 566 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP FARADEX DX92079 PC (Europe-Africa-Middle East)
LNP* Faradex* DX92079 is a compound based on Polycarbonate resin containing Glass Fiber, Glass Bead, Stainless Steel Fiber. Added features of this material include: EMI/RFI Shielding, Mold Release...
|
|||
| Flexural Modulus | 3.90 GPa | 566 ksi | ISO 178 |
|
Nilit FRIANYL B63 GV10 Nylon 6 for injection molding, 10% glass fiber reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Flexural Modulus | 3.90 GPa | 566 ksi | ISO 178 |
|
Victrex® PEEK 150PF Easy Flow
Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, fine powder for compression molding, easy flow, FDA food contact compliant, ..
|
|||
| Flexural Modulus |
3.90
GPa <br>@Temperature 23.0 °C
|
566
ksi <br>@Temperature 73.4 °F
|
ISO 178 |
|
Victrex® PEEK 150XF Polyetheretherketone, Unreinforced
Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, fine powder for compression moulding, easy flow, FDA food contact compliant, ..
|
|||
| Flexural Modulus |
3.90
GPa <br>@Temperature 60.0 °C
|
566
ksi <br>@Temperature 140 °F
|
ASTM D790 |
|
LATI LATAN 13 G/15 15% Glass Fiber Reinforced Polyoxymethylene Copolymer (POM)
(discontinued **)
Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea..
|
|||
| Flexural Modulus | 3.90 GPa | 566 ksi | |
|
Lehmann & Voss LUVOCOM® 3-8363 Polyamide 6, unreinforced
Applications: Automotive industry, textile machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteristics.Reduce..
|
|||
| Flexural Modulus | 3.90 GPa | 566 ksi | |
|
Lehmann & Voss LUVOCOM® 19-7745 Polyamide 46, with PTFE, improved wear resistance
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Isotropic shrinkage characteristics.Good friction and wear behaviour especially at increased te..
|
|||
| Flexural Modulus | 3.90 GPa | 566 ksi | 2 mm/min, 64mm span; ISO 178 |
|
SABIC Innovative Plastics SABIC STAMAX 20YK270 PP
SABIC® STAMAX 20YK270 is a 20% long glass fiber reinforced polypropylene with improved impact and flow properties. The glass fibers are chemically coupled to the PP matrix, resulting in high stif..
|
|||
| Flexural Modulus | 3.90 GPa | 566 ksi | ASTM D790 |
|
Solvay Specialty Polymers KetaSpire® KT-851 NL Polyetheretherketone (PEEK)
KetaSpire® KT-851 NL resin is a depth-filtered grade of polyetheretherketone (PEEK) supplied in non-lubricated, natural-color pellet form and is specially designed for use in extruded wire insula..
|
|||
| Flexural Modulus | 3.90 GPa | 566 ksi | ISO 178 |
|
Solvay Specialty Polymers KetaSpire® KT-880 Polyetheretherketone (PEEK)
KetaSpire® KT-880 is a high flow grade of unreinforced polyetheretherketone (PEEK) supplied in pellet form. KetaSpire® PEEK is produced to the highest industry standards and is characterized b..
|
|||
| Flexural Modulus | 3.90 GPa | 566 ksi | ISO 178 |
|
Solvay Specialty Polymers KetaSpire® KT-880FP Polyetheretherketone (PEEK)
KetaSpire® KT-880FP is the high-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural color fine powder form for compression molding and other uses that can benefit from th..
|
|||
| Flexural Modulus | 3.90 GPa | 566 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP Thermocomp AF0029 ABS (Europe-Africa-Middle East)
LNP* THERMOCOMP* AF0029 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant. Added features include: Flame Retardant.This data was supplied by SABIC-..
|
|||
| Flexural Modulus | 3.90 GPa | 566 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
|
SABIC Innovative Plastics Noryl GTX GTX965 PPE+PA66
NORYL GTX965 is a mineral reinforced PPE/PA blend. It offers excellent surface appearance, processability and dimensional stability at elevated temperatures. The best molding condition for good appe..
|
|||
| Flexural Modulus | 3.90 GPa | 566 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT (Asia Pacific)
LNP* Lubricomp* WBL36L is a compound based on Polybutylene Terephalate resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
|
|||
| Flexural Modulus | 3.90 GPa | 566 ksi | ISO 178 |
|
SABIC Innovative Plastics LNP LUBRICOMP WBL36L PBT (Asia Pacific)
LNP* Lubricomp* WBL36L is a compound based on Polybutylene Terephalate resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
|
|||
| Flexural Modulus | 3.90 GPa | 566 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Valox® 7062HP PBT (Europe-Africa-Middle East)
ENDURAN 7062HP is a 38% mineral filled & FDA compliance injection moulding resin.
|
|||
| Flexural Modulus | 3.90 GPa | 566 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP AW00A ABS (Europe-Africa-Middle East)
LNP* THERMOCOMP* AW00A is a compound based on Acrylonitrile Butadiene Styrene resin containing Wollastonite.
|
|||
| Flexural Modulus | 3.90 GPa | 566 ksi | 2mm/min; ISO 178 |
|
Borealis MD441U Polypropylene Compound, Mineral Filled
MD441U is a 40% mineral filled polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties and a medium melt flow rate. Applications: air cond..
|
|||
| Flexural Modulus | 3.90 GPa | 566 ksi | ISO 178 |
|
Wellman Wellamid® FR22F-N Flame Retardant Nylon 66, Lubricated
Typical Applications: Electrical terminal blocks, electric fan switch housings, coil forms, multi-pin electrical connectors, electric fan switch housings, TV tuner components, automotive switch hous..
|
|||
| Flexural Modulus | 3.90 GPa | 566 ksi | ISO 178-93 |
|
Wellman Wellamid® GS1857-BK1 Nylon 66, 15% Glass Sphere Reinforced
Developmental productAll information provided by Wellman Engineered Resins.
|
|||
| Flexural Modulus | 3.90 GPa | 566 ksi | DIN EN ISO 178 |
|
Wolf Kunststoff ZEDEX® ZX-324V2T A3F PEEK, PTFE Modified
Reduced friction; High wear resistance; High elasticity; Stress resistantApplications: Shipbuilding; Chemical Engineering; Automotive Technology; Machine ToolsInformation provided by Zedex
|
|||
| Flexural Modulus | 3.90 GPa | 566 ksi | ASTM D790 |
|
Cresset Powers Cress-Alon™ NF3020 2% Nano Clay Loaded, 3.0 r.v. Film Grade Nylon 6, Dry As Molded
Low density, high rigidity, high heat distortion temperature, high retention of mechanical properties under humid conditions, flame retardant, recyclable and environmentally friendly, less glass fib..
|
|||
| Flexural Modulus | 3.90 GPa | 566 ksi | ASTM D790 |
|
Clariant ABS4500G10BK ABS, 10% Glass Reinforced
Data provided by Clariant Masterbatches
|
|||
| Flexural Modulus | 3.90 GPa | 566 ksi | ASTM D790 |
|
A. Schulman ComAlloy Hiloy® 221 ABS, Glass Reinforced, UL
Data provided by the manufacturer, ComAlloy International Company.10% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Flexural Modulus | 3.90 GPa | 566 ksi | ASTM D 790 |
|
Saint-Gobain Meldin® 2021 Bearing
General Notes on Meldin 2000 Series Bearing Products:For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin 2000 Series ca..
|
|||
| Flexural Modulus | 3.90 GPa | 566 ksi | DIN 53452; ASTM D790 |
|
Kolon Kopa® KN173MS Nylon 6 Resin
KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c..
|
|||
| Flexural Modulus | 3.90 GPa | 566 ksi | ISO 178 |
|
Panjin Zhongrun Chemerize 021G Medium Viscosity CoPEEK
Information provided by Bieglo Gmbh.
|
|||