| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 22.0 GPa | 3190 ksi | ISO 178 |
|
PolyOne OnForce™ LFT SF-40LCF/000 Black Polyphenylene Sulfide (PPS)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
|
|||
| Flexural Modulus | 22.0 GPa | 3190 ksi | ISO 178 |
|
Solvay Specialty Polymers Ixef® GS-1022 Polyarylamide (PARA)
(Unverified Data**)
Ixef GS-1022 is a 50% glass-fiber reinforced grade of polyarylamide (PARA) available in several colors. Parts molded from these colored resins can withstand high-energy gamma radiation without signi..
|
|||
| Flexural Modulus | 22.0 GPa | 3190 ksi | |
|
Lehmann & Voss LUVOCOM® 1105-8513 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Flexural Modulus | 22.0 GPa | 3190 ksi | |
|
Lehmann & Voss LUVOCOM® 1301-7449 PPS, linear, with carbon fiber and PTFE
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.High-strength and stiff parts with low creep.Improved friction and wear behaviour. Emergency runni..
|
|||
| Flexural Modulus | 22.0 GPa | 3190 ksi | |
|
Lehmann & Voss LUVOCOM® 20-8283 Polyphthalamide, with carbon fiber, lubricant modified
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Low influence from moisture an..
|
|||
| Flexural Modulus | 22.0 GPa | 3190 ksi | |
|
Lehmann & Voss LUVOCOM® PEKK-7299 Polyether ketone, with carbon fiber, easy flowing
Applications: Automotive industry, mechanical- and precision engineering.Improved strength and stiffnes at elevated temperatures.Suitable for discharging of statically generated electricity.Thermic,..
|
|||
| Flexural Modulus | 22.0 GPa | 3190 ksi | ASTM D790 |
|
Gharda Chemicals G-PAEKâ„¢ 1230CF Ultra High Performance PEK Polymer
Product Details: Ultra High Performance Thermoplastic material, 30% carbon fiber reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection molding, easy flow, Black in ..
|
|||
| Flexural Modulus | 22.0 GPa | 3190 ksi | |
|
Lehmann & Voss LUVOCOM® 1/CF/40 Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Flexural Modulus | 22.0 GPa | 3190 ksi | |
|
Lehmann & Voss LUVOCOM® 1105-7781 PEEK, with carbon fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at..
|
|||
| Flexural Modulus | 22.0 GPa | 3190 ksi | |
|
Lehmann & Voss LUVOCOM® 1-7893/GY Polyamide 66, with carbon fiber, heat stabilized
Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp..
|
|||
| Flexural Modulus | 22.0 GPa | 3190 ksi | ISO 178 |
|
Solvay Specialty Polymers Ixef® GS-1022 Polyarylamide (PARA), 50% Glass Fiber (Dry)
Ixef® GS-1022 is a 50% glass-fiber reinforced grade of polyarylamide (PARA) available in several colors. Parts molded from these colored resins can withstand high-energy gamma radiation without s..
|
|||
| Flexural Modulus | 22.0 GPa | 3190 ksi | 0° |
|
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, E-glass Balanced fabric 300 g/m2
Information provided by HexCel
|
|||
| Flexural Modulus | >= 22.0 GPa | >= 3190 ksi | IEC 1212-2 5.2 |
|
Hippe PI GC 301 Woven Glass Cloth Reinforced Phenolic Sheet
Used in electrical and mechanical applications. Very good mechanical and electrical properties at high temperature.Information provided by Hippe.
|
|||
| Flexural Modulus | 22.0 GPa | 3190 ksi | ASTM D790 |
|
A. Schulman ComAlloy Hiloy® 758 Carbon Fiber Reinforced, Flow Enhanced, PPS Alloy
Data provided by the manufacturer, ComAlloy International Company.40% Carbon Fiber Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has b..
|
|||
| Flexural Modulus | 22.0 GPa | 3190 ksi | ASTM D790 |
|
Sumitomo Bakelite North America Epiall® 1914A Short Glass Fiber Reinforced Epoxy
Epiall 1914A is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation properties.Information provided by..
|
|||