Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 360 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Modulus 2.48 GPa
360 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Cycoloy® C1950 PC+ABS
Low viscosity injection molding resin.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.48 GPa
360 ksi
6.4 mm; ASTM D790
SABIC Innovative Plastics FL405 PC
Various weight reductions at 0.250"" (6.38 mm) wall. Impact resistant, superior processing, excellent surface. UL94 V-0 at 0.120
Flexural Modulus 2.48 GPa
360 ksi
ASTM D790
Ravago Manufacturing Americas Hybrid B3030U Polycarbonate + PBT Alloy
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Flexural Modulus 2.48 GPa
360 ksi
ASTM D790
Quadrant EPP Semitron® CMP LL5 Polyester (ASTM Product Data Sheet)
Enhanced semi-crystalline polyester product for extended service in CMP retaining rings. Superior performance, especially in oxide processes, and cost effective relative to standard ring materials. ..
Flexural Modulus 2.48 GPa
360 ksi
ASTM D790
Quantum Modified PPO - Noryl®
Information provided by Quantum Advanced Engineering Plastics
Flexural Modulus 2.48 GPa
360 ksi
6.4 mm; ASTM D790
SABIC Innovative Plastics Lexan® FL405 PC
Various weight reductions at 0.250"" (6.38 mm) wall. Impact resistant, superior processing, excellent surface. UL94 V-0 at 0.120
Flexural Modulus 2.48 GPa
360 ksi
ASTM D790
KYDEX® 152WG Capped Wood Grain Thermoplastic Sheet
Features:Super tough, durableHigh extensibility, rigidity, abrasion resistance and fire retardancyMore rigid than most thermoplastics, parts deform less when loadedOutstanding resistance to breakage..
Flexural Modulus 2.48 GPa
360 ksi
ASTM D790
KYDEX® XD MB 3D Laminate Thermoplastic 3D Laminate for Flat Lamination and Membrane Pressed Uses with Microban®
Features:Tough and extremely durableResistant to cracking and chippingSolid, integral color4,000+ custom colorsResistant to a wide range of chemicalsAbrasion resistantFire retardantVery low moisture..
Flexural Modulus 2.48 GPa
360 ksi
ASTM D790
KYDEX® T MB High Impact Fire Rated Thermoforming Sheet with Microban® Antimicrobial Product
Features:Substitute for FR-ABS sheet with competitive pricing but superior cost/performanceHigher breakage resistanceStandard thicknesses from 0.71 mm to 2.36 mmAmong the most rigid of thermoforming..
Flexural Modulus 2.48 GPa
360 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP DX96651 PC
LNP LUBRICOMP* DX96651 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Wear Resistant.
Flexural Modulus 2.48 GPa
360 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR6300 AES+PC+SAN (Asia Pacific)
Wear resistant PC+SAN, with proprietary lubricant, for business equipment applications.
Flexural Modulus 2.48 GPa
360 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON DX11408 PC
LNP* STAT-KON* DX11408 is a compound based on Polycarbonate containing Carbon Powder. Added features of this material include: Electrically Conductive, Improved Ductility
Flexural Modulus 2.48 GPa
360 ksi
ASTM D790
Techmer ES HiFill® PA11 GB7 HS L 7% Glass Bead Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 7% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformation provided by T..
Flexural Modulus 2.48 GPa
360 ksi
secant; ASTM D790
Spartech EP5140 Talc Filled Homopolymer
Provides the highest level of stiffness and heat resistance of filled olefins. Talc filled grades offer the highest strength properties. Typical applications include extrusion/thermoformed food cont..
Flexural Modulus 2.48 GPa
360 ksi
ASTM D790
Techmer ES Luriblend® PA6/6 LX Nylon 66
Availability: North AmericaForms: PelletsFeatures: Good Wear Resistance and Low FrictionInformation provided by TP Composites, Inc.
Flexural Modulus 2.48 GPa
360 ksi
ASTM D790
Techmer ES Plastiblend® PC/ABS 1000
Availability: North AmericaForms: PelletsInformation provided by TP Composites, Inc.
Flexural Modulus 2.48 GPa
360 ksi
1.3 mm/min; ASTM D790
Styron MAGNUMâ„¢ 8391 Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ 8391 ABS combines an excellent glossy appearance with high flow and medium impact performance. The mass continuous process) ABS technology of Styron ensures an ABS resin that ..
Flexural Modulus 2.48 GPa
360 ksi
1.3 mm/min; ASTM D790
Styron Magnumâ„¢ 8391 MED Acrylonitrile Butadiene Styrene (ABS) Resin
Overview: MAGNUMâ„¢ MED ABS combines an excellent glossy appearance with high flow and medium impact performance. The mass (continuous process) ABS technology of Styron ensures an ABS resin that ..
Flexural Modulus 2.48 GPa
360 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp YF006 TPEE
LNP THERMOCOMP* YF006 is a compound based on TPEE resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 2.48 GPa
360 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics Xenoy® X5300WX PBT+PC (Asia Pacific)
Unreinforced, opaque PBT+PC alloy. Chemical resistance and good mechanical performance. UV-stabilized. Excellent weatherability.
Flexural Modulus 2.48 GPa
360 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Xenoy® X5600WX PC+POLYESTER (Europe-Africa-Middle East)
Unreinforced, opaque Polyester+PC alloy. Chemical resistance, dimensional stability and mechanical performance. UV Stabilized. Mold ReleaseThis data was supplied by SABIC-IP for the Europe-Africa-Mi..
Flexural Modulus 2.48 GPa
360 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL GTX GTX674PC PPE+PA6 (Europe-Africa-Middle East)
A conductive PPE/PA blend designed to have improved surface appearance and elevated heat resistance for powder coating. The material is suitable for injection molding. The material is only availab..
Flexural Modulus 2.48 GPa
360 ksi
ASTM D790
Chase Plastics CP Pryme® AC300 Acetal Copolymer, Recycled Content
Features: Recycled contentForm: PelletsInformation provided by Chase Plastics.
Flexural Modulus 2.48 GPa
360 ksi
ASTM D790
Total PSI 825EX Polystyrene
Polystyrene 825EX is a high impact polystyrene designed for high stiffness in extrusion/thermoforming applications. The balance of high stiffness and impact properties allow for light weighting of t..
Flexural Modulus 2.48 GPa
360 ksi
ASTM D790
A. Schulman POLYFORT™ FPP 1200 Calcium Carbonate-Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 1200 is a 40% calcium carbonate-filled homopolymer polypropylene. Information provided by A. Schulman.
Flexural Modulus 2.48 GPa
360 ksi
ASTM D790
Entec Hylex® P1017FR Polycarbonate
Information provided by Ravago.
Flexural Modulus 2.48 GPa
360 ksi
ASTM D790
Asahi Kasei Thermofil P-40TC-2767 40% Talc Reinforced, Heat Stabilized
Information provided by Asahi Thermofil
Copyright © lookpolymers.com All Rights Reserved