Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 4.00 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Modulus 4.00 GPa
580 ksi
Plastcom SLOVAMID 6 T 10 PA6, mineral filling
FeaturesDecreased shrinkage against the BT types, increased heat application up to 170°C. Increased modulus in tension - strength of the material. PA matrix reduction. Application eg. for tools, fi..
Flexural Modulus 4.00 GPa

@Temperature 23.0 °C
580 ksi

@Temperature 73.4 °F
ISO 178
Polykemi AB POLYblend 45V GF10 PC/ABS-blend, Flame Retardant
Information provided by Polykemi AB
Flexural Modulus 4.00 GPa
580 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Cycoloy® XCM840 PC+ABS
High stiffness PC/ABS blend offering practical impact, low CTE, high heat resistance, with good aesthetics suitable for injection molding
Flexural Modulus 4.00 - 6.00 GPa
580 - 870 ksi
Compression; ISO 178
Raschig Group RALUPOL® 5000 UP Polyester
Glass-fiber reinforced polyester molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, excellent heat resistance, good mechanical strength. This product meets the all..
Flexural Modulus 4.00 GPa

@Temperature 150 °C
580 ksi

@Temperature 302 °F
ISO 178
Solvay Specialty Polymers Amodel® A-1133 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel A-1133 HS is a 33% glass reinforced, heat stabilized polyphthalamide (PPA) with a high heat deflection temperature, high flexural modulus and high tensile strength. Excellent creep resistance..
Flexural Modulus 4.00 - 10.6 GPa
580 - 1540 ksi
Average value: 5.66 GPa Grade Count:8
Overview of materials for Glass Reinforced, Modified SMA
This property data is a summary of similar materials in the MatWeb database for the category "Glass Reinforced, Modified SMA". Each property range of values reported is minimum and maximum values of..
Flexural Modulus 4.00 GPa
580 ksi
Lehmann & Voss LUVOCOM® 1105-8264 PEEK, with CNT
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Electrically conductive, suitable for continuous discharging of statically generated elect..
Flexural Modulus 4.00 GPa
580 ksi
Lehmann & Voss LUVOCOM® 1301-8290 PPS, linear, with aramid reinforcement
Applications: Automotive industry, textile-and office machinery, medical- and precision engineering.Improved friction and wear behaviour. Emergency running property.Low warpage.dynamic stressInforma..
Flexural Modulus 4.00 - 4.50 GPa
580 - 653 ksi
ASTM D790
Loxim 820 01 HBCC Polypropylene Compound, 20% Chemically Coupled, Flame Retardant
Information provided by Loxim Industries
Flexural Modulus 4.00 GPa
580 ksi
Lehmann & Voss LUVOCOM® 1105-7023/GY PEEK, with glass fiber
Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Chemical and hydrolysis resistance parts, non flammable.High dimension..
Flexural Modulus 4.00 GPa
580 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP RA004 PA 66 (Europe-Africa-Middle East)
LNP* Lubricomp* RA004 is a compound based on Nylon 66 resin containing Aramid Fiber.
Flexural Modulus 4.00 GPa
580 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 (Europe-Africa-Middle East)
Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the E..
Flexural Modulus 4.00 GPa
580 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA
NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an..
Flexural Modulus 4.00 GPa
580 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics NORYL GTX GTX975 PPE+PA (Asia Pacific)
NORYL GTX975 is a 18% mineral filled material especially designed for in- or on-line painted exterior automotive trim part, e.g. tankflaps and corner panels. This material combines high stiffness an..
Flexural Modulus 4.00 GPa
580 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 (Asia Pacific)
Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A..
Flexural Modulus 4.00 GPa
580 ksi
ISO 178
Wellman Wellamid® GS25-66 22L-N, 25% Glass Sphere Filled Nylon 66, Lubricated
Typical Applications: Potentiometer liners, electrical coil forms, automotive window lift and power door lock switch bodies, gears, thick wall section moldings, emission control valves.Data provided..
Flexural Modulus 4.00 GPa
580 ksi
DIN EN ISO 178
Wolf Kunststoff ZEDEX® ZX-324 A3A PEEK
Main Characteristics: Hard; Stiff; Tough; High fatigue strength; Good water resistance; Sufficient UV and weather resistance; Flame retardant; Good machinability; FDA compliant LABS; PTFE and Silico..
Flexural Modulus 4.00 GPa
580 ksi
ASTM D790
Toyobo VYLOPET® CA5310 PC/PBT Polymer Alloy, High Rigidity, Impact Resistant
Applications: Lamp partsHome electric appliance partsFeatures: Fine appearanceHigh rigidityImpact resistantInformation provided by Toyobo.
Flexural Modulus 4.00 GPa
580 ksi
ASTM-D790
Polyram PlusTek PD300G4 Nylon 12, 20% Glass Fiber
20% glass-fiber reinforced polyamide 12 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Flexural Modulus 4.00 GPa
580 ksi
ASTM-D790
Polyram PlusTek RA307G4 Nylon 6.6, 20% Glass Fiber
20% glass fiber reinforced heat stabilized polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
Flexural Modulus 4.00 GPa
580 ksi
ASTM-D790
Polyram RamSter PF300G2 PBT, 10% Glass Fiber
10% Glass-Fiber reinforced PBT for injection molding applicationsInformation provided by Polyram Ram On Ind.
Flexural Modulus 4.00 GPa
580 ksi
ISO Data
BASF Ultraform N 2320 U03 UNC Q600 POM
Ultraform N2320 U03 UNC Q600 is a rapidly freezing UV stabilized general-purpose injection molding grade.
Flexural Modulus 4.00 GPa
580 ksi
ASTM D790
Beijing Chemical Industry KAIFA® 301-G10 PBT Resin
10% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group)
Flexural Modulus 4.00 GPa
580 ksi
ASTM D790
A. Schulman ComAlloy Hiloy® 419 Polyester - PBT, Mineral Reinforced
Data provided by the manufacturer, ComAlloy International Company.40% Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Flexural Modulus 4.00 GPa

@Temperature 23.0 °C
580 ksi

@Temperature 73.4 °F
ISO 178
Polykemi AB POLYfill PPH T20040 Polypropylene Homopolymer, Mineral Reinforced
Information provided by Polykemi AB
Flexural Modulus 4.00 GPa
580 ksi
ISO 178
BASF Ultramid® B3M6 Grey 22319 Q94 30% Mineral Filled PA6 (Dry)
Description: 30% Mineral-filled injection molding grade for high impact industrial items having very high dimensional stability, such as automobile wheel covers.Information provided by BASF
Flexural Modulus 4.00 GPa
580 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics Lexan® ML3260 PC (Europe-Africa-Middle East)
LEXAN ML3260 is a medium viscosity, 15% glass reinforced, flame retardant grade especially designed for applications like computer cartridges.
Copyright © lookpolymers.com All Rights Reserved