| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 4.41 GPa | 640 ksi | ASTM D790 |
|
PolyOne Maxxam™ DC-818.G001-8000 Polypropylene, Unspecified (PP, Unspecified)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
|
|||
| Flexural Modulus | 4.41 GPa | 640 ksi | Tangent; ASTM D790 |
|
RheTech Products GC30P200-00 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural
Applications: Window frameHead lamp housingInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Flexural Modulus | 4.41 GPa | 640 ksi | Tangent; ASTM D790 |
|
RheTech Products GC30P200-01 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Window frameHead lamp housingInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Flexural Modulus | 4.41 GPa | 640 ksi | Tangent; ASTM D790 |
|
RheTech Products GC30P200-01UV 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, Black
Applications: Interior componentsStructural housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Flexural Modulus | 4.41 GPa | 640 ksi | Tangent; ASTM D790 |
|
RheTech Products GC30P200-523 30% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, UV Stabilized, (GM 167A) Ebony
Applications: Window frameHead lamp housingInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Flexural Modulus | 4.41 GPa | 640 ksi | ASTM D790 |
|
PolyOne Nymax™ GBF 1010 35 BLACK 13 Polyamide 6 (Nylon 6)
Information provided by PolyOne
|
|||
| Flexural Modulus | 4.41 GPa | 640 ksi | ASTM D790 |
|
Omni Plastics OmniTuff™ HPP GRC20 Homopolymer Polypropylene Glass Reinforced
Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni..
|
|||
| Flexural Modulus | 4.41 GPa | 640 ksi | ASTM D790 |
|
SABIC Innovative Plastics Lexan® BFL2015 PC (Asia Pacific)
Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only
|
|||
| Flexural Modulus | 4.41 GPa | 640 ksi | ASTM D790 |
|
SABIC Innovative Plastics Lexan® BFL2015HF PC (Asia Pacific)
Non-brominated, non-chlorinated flame retardant, glass reinforced PC. Opaque colors only. UL94 V0 1.5 mm for BLACK; V1 1.5 mm for OTHER Color.
|
|||
| Flexural Modulus | 4.41 GPa | 640 ksi | ASTM D790 |
|
SABIC Innovative Plastics Lexan® LGN1500 PC (Asia Pacific) |
|||
| Flexural Modulus | 4.41 GPa | 640 ksi | DIN 53452; ASTM D790 |
|
Kolon SPELLOY® KB133G15 PC + PBT Alloy Resin
(discontinued **)
SPELLOY® is a new technology of thermoplastic Polymer alloys developed to provide unique combination of excellent mechanical properties.High impact resistance (at low temperature), good dimensional..
|
|||
| Flexural Modulus | 4.41 GPa | 640 ksi | ASTM D790 |
|
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA)
(Unverified Data**)
Amodel AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin. Th..
|
|||
| Flexural Modulus | 4.41 GPa | 640 ksi | ASTM D790 |
|
Kolon KOCETAL® TC704 Mineral Reinforced Acetal Resin
Whisker reinforced, improved wear and dimensional property. Applications: Dimensionally precise products. Information provided by API-Kolon.
|
|||
| Flexural Modulus |
4.41
GPa @Thickness 3.20 mm |
640
ksi @Thickness 0.126 in |
1.3mm/min; ASTM D790 |
|
LG Chemical LUMID GP2130AE PA6+GF13%, General Purpose
Feature: Injection Molding, PA6+GF13%, General PurposeApplication: Industrial MaterialCAS No. 25038-54-4 and 65997-17-3Information provided by LG Chemical
|
|||
| Flexural Modulus | 4.41 GPa | 640 ksi | ASTM D790 |
|
LG Chemical LUPOS GP-2106F General Purpose ABS, 10% Glass Fiber Reinforced, Weather Resistant, Flame Retardant
LUPOS resins are glass fiber reinforced styrene copolymers. LUPOS have improved strength, rigidity and dimensional stability. They offer excellent heat resistance, minimal mold shrinkage and have ..
|
|||
| Flexural Modulus | 4.41 GPa | 640 ksi | ASTM D790 |
|
Kotec Carbotex KGN-15MRA Polycarbonate, Flame Retardant, 15% Glass Fiber Reinforced
Features: Glass fiber 15% reinforced, Mold release, Translucent, Dimensional stability, Flame retardant, High rigidityApplications: OA equipment, Communications, Precision parts, Machineries, E & E ..
|
|||
| Flexural Modulus | 4.41 GPa | 640 ksi | ASTM D790 |
|
SABIC Innovative Plastics LNP LUBRICOMP RA004 PA 66 (Asia Pacific)
LNP LUBRICOMP* RA004 is a compound based on Nylon 66 resin containing Aramid. Added features of this material include: Internally Lubricated.
|
|||
| Flexural Modulus | 4.41 GPa | 640 ksi | ASTM D790 |
|
Solvay Specialty Polymers Amodel® AT-6115 HS Polyphthalamide (PPA), 15% Glass Fiber (Dry)
Amodel® AT-6115 HS is a 15% glass-fiber reinforced, toughened grade of polyphthalamide (PPA) resin designed to possess more elongation than other 15% glass-fiber reinforced grades of Amodel resin..
|
|||
| Flexural Modulus | 4.41 GPa | 640 ksi | ASTM D790 |
|
SABIC Innovative Plastics LNP STAT-KON DDF029 PC (Asia Pacific)
LNP STAT-KON* DDF029 is a compound based on Polycarbonate resin containing Carbon Powder, Flame Retardant, Glass Fiber. Added features of this material include: Electrically Conductive.
|
|||
| Flexural Modulus | 4.41 GPa | 640 ksi | ASTM D790 |
|
Techmer ES HiFill FR® ABS GF15 FR-2 15% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 15% Filler by WeightFeatures: Flame RetardantInformation provided by TP Composites, Inc.
|
|||
| Flexural Modulus | 4.41 GPa | 640 ksi | ASTM D790 |
|
Samyang Tribit® 1500G20 PBT, Reinforced General Purpose
Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1500G20 is a reinforced, general purpose gr..
|
|||
| Flexural Modulus | 4.41 GPa | 640 ksi | ASTM D790 |
|
Samyang Trirex® 3025G15 Polycarbonate, 15% Glass Reinforced
TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec..
|
|||
| Flexural Modulus | 4.41 GPa | 640 ksi | 2.8 mm/min; ASTM D790 |
|
Samsung Cheil Industries Infino® NH-3204G PC, Glass Filled FR
Information provided by Samsung Cheil Industries.
|
|||
| Flexural Modulus | 4.41 GPa | 640 ksi | 2.8 mm/min; ASTM D790 |
|
Samsung Cheil Industries Infino® NH-3204G PC, Glass Filled FR
Information provided by Samsung Cheil Industries.
|
|||
| Flexural Modulus | 4.41 GPa | 640 ksi | ASTM D790 |
|
Chase Plastics CP Pryme® N330GL (COND, 50% RH) Nylon 6 (Utility Grade), 30% Glass Fiber Reinforced, Internally Lubricated
Information provided by Chase Plastics.
|
|||
| Flexural Modulus | 4.41 GPa | 640 ksi | Tangent; ASTM D790 |
|
Washington Penn Homopolymer Polypropylene 27% Glass Reinforced
Fiberglass & mineral-reinforced polypropylene compounds provide excellent tensile and impact properties. Mold shrinkage is similar to ABS and polystyrene. Compounds also have dimensional stability. ..
|
|||
| Flexural Modulus | 4.41 GPa | 640 ksi | 2.8mm/min; ASTM D790 |
|
Asia International Enterprise (Hong Kong) 60T6F Nylon 66, 30% Filled
Information provided by Asia International Enterprise (Hong Kong) Ltd.
|
|||