| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
|
Multibase Multi-Pro® 1004 R Polypropylene
Features: Scratch Resistance, GoodHeat Resistance, HighStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | Tangent; ASTM D790 |
|
RheTech Products G13P100-00 13% Glass Fiber Reinforced Polypropylene, Natural
Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | Tangent; ASTM D790 |
|
RheTech Products G13P100-332UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, (GM 9772) Light Neutral
Applications: Interior trimAir ducts - distributionFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products.
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
|
PolyOne Novablend™ 2677 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
|
PolyOne Geon™ CPVC MC100 Polyvinyl Chloride, Chlorinated (CPVC)
Geon MC100 CPVC is an Injection molding fitting compound. It is listed under NSF Std 14 and 61 and meets or exceeds ASTM D-1784 Cell Class 23447. MC100 is designed for CTS applications where enhance..
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | 0.1 in/min; ASTM D790 |
|
Ineos Nova 271 High Performance Styrenic Enhanced Polystyrene
(discontinued **)
Excellent balance of stiffness, heat resistance, and impact properties, Custom colorsApplications: Injection molding and extrusion, Applications requiring strength and durability where custom colori..
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
|
PolyOne Lubri-Tech™ ATH-5KV/000 Acetal-Homopolymer, Aramid Fiber
(discontinued **)
Description/Features:Aramid Fiber ReinforcedInformation provided by PolyOne Corporation.
|
|||
| Flexural Modulus | 2.76 - 6.76 GPa | 400 - 980 ksi | Average value: 4.63 GPa Grade Count:11 |
|
Overview of materials for Polycarbonate/PET Polyester Blend, Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/PET Polyester Blend, Glass Reinforced". Each property range of values reported is minimum ..
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
|
Techmer ES Electrablend® PEI 04008 MB
Availability: North AmericaForms: PelletsFeatures: Conductive and CopolymerInformation provided by TP Composites, Inc.
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
|
Techmer ES HiFill® ABS E GM5 LE 5% Glass Filled
Availability: North AmericaFeatures: Low ExtractablesForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightInformation provided by TP Composites, Inc.
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
|
Techmer ES Luriblend® PA6/6 M/TL7 HS L Nylon 66
Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant, PTFE Lubricant and Molybdenum Disulfide LubricantFeatures: Lubricated and Heat StabilizerProcessing Method: Injection M..
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
|
Techmer ES Statiblend® PC FR BK
Availability: North AmericaForms: PelletsAntistaticFeatures: Flame Retardant and Semi ConductiveUL File Number: E157318Information provided by TP Composites, Inc.
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
|
Techmer ES Luriblend® POM HO TL20 Acetal
Availability: North AmericaForms: PelletsAdditive: PTFE Lubricant(20%)Features: Lubricated and HomopolymerInformation provided by TP Composites, Inc.
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP THERMOTUF VF1001S Super Tough Nylon
LNP* Thermotuf* VF1001S is a Super Tough Nylon containing glass fiber. Characteristics of this grade is Heat Stabilized.
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
|
Chase Plastics CP Pryme® N300L (DAM) Nylon 6 (Utility Grade), Internally Lubricant
Information provided by Chase Plastics.
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
|
Westlake Plastics Pomalux® CN-SS Acetal Copolymer (conductive)
Stainless-steel-fiber-filled, non-sloughing, dimensionally stable material HDT @ 264 psi of 225F. This material has relatively high chemical resistance, is extremely strong and stiff, and is an exc..
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
|
A. Schulman POLYFORT™ FPP 1607 Talc Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 1607 is a 30% talc filled homopolymer polypropylene compound. Information provided by A. Schulman.
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
|
Ensinger XP-130 Compression Molded PI Compound, 30% PTFE Filled
The XP-130 is an amorphous high performance thermoplastic with high permanent temperature and creep resistance as well as excellent bearing and wear properties, excellent long term thermal stability..
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | tangent; chs 0.05 in/min; ASTM D790 |
|
Diamond Polymers DIAMALOY 310 GF10 PC/Polyester Alloy, Impact Modified
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
|
|||
| Flexural Modulus | 2.76 - 2.90 GPa | 400 - 421 ksi | ASTM D790 |
|
3D Systems Accura® 45HC Plastic for SLA® Systems
A high speed material, with excellent thermal and moisture resistance for producing functional prototypes in 3D Systems' SLA 250 systems.ApplicationsHigh temperature testing:Automotive "under-the-ho..
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | 0.1 in/min; ASTM D790 |
|
Ineos Nova 8048 High Performance Styrenic Enhanced Polystyrene
(discontinued **)
Improved toughness, Custom colorsApplications: Designed for injection molding applications requiring clarity and toughnessPerformance grades of polystyrene are engineered to have specific properties..
|
|||
| Flexural Modulus | 2.76 GPa | 400 ksi | ASTM D790 |
|
PolyOne Edgetek® UR-20GF/000 Natural Thermoplastic Polyurethane (Ether-Based), 20% Glass Fiber Reinforced
(di