Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 479 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Modulus 2.70 - 3.30 GPa
392 - 479 ksi
ASTM D790-04
Proto3000 Objet Digital Materials™ DM_Dots_7513 Transparent Prototyping Polymer
Primary material: FullCure720Secondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide t..
Flexural Modulus 2.70 - 3.30 GPa
392 - 479 ksi
ASTM D790-04
Proto3000 Objet Digital Materials™ DM_Grid_7523 Transparent Prototyping Polymer
Primary material: FullCure720Secondary material: VeroBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide t..
Flexural Modulus 2.70 - 3.30 GPa
392 - 479 ksi
ASTM D790-04
Proto3000 Objet FullCure720 Transparent Prototyping Polymer
Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid ..
Flexural Modulus 3.30 - 3.30 GPa

@Temperature 60.0 - 60.0 °C
479 - 479 ksi

@Temperature 140 - 140 °F
Average value: 3.30 GPa Grade Count:2
Overview of materials for Polystyrene, Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Glass Filled". Each property range of values reported is minimum and maximum values of appr..
Flexural Modulus 3.20 - 3.30 GPa

@Temperature 60.0 - 120 °C
464 - 479 ksi

@Temperature 140 - 248 °F
Average value: 3.27 GPa Grade Count:1
Overview of materials for Polycarbonate, 20% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E..
Flexural Modulus 2.96 - 3.30 GPa
429 - 479 ksi
Average value: 3.16 GPa Grade Count:3
Overview of materials for Acrylic, Cast
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW..