| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 5.50 GPa | 798 ksi | ISO 178 |
|
PolyOne OnForce™ LFT PP-30LGF/001 Natural Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | |
|
Plastcom SLOVASTER® B1 GF 20 PBT, 20% glass fibre
FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending..
|
|||
| Flexural Modulus |
5.50
GPa <br>@Temperature 90.0 °C
|
798
ksi <br>@Temperature 194 °F
|
ISO 178, ASTM D790 |
|
Nilit Nilamid A3 H5 G6 30% Glass Reinforced PA66
Description: Nilamid A3 H5 G6 has an outstanding mechanical performance and is 30% glass fiber reinforced. It is stabilized against chemical attack from peroxides and other oxidizing substances. It ..
|
|||
| Flexural Modulus |
5.50
GPa <br>@Temperature 23.0 °C
|
798
ksi <br>@Temperature 73.4 °F
|
ISO 178 |
|
Polykemi AB POLYshine PBT D221 QF30 PBT, Glass and Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Flexural Modulus |
5.50
GPa <br>@Temperature 23.0 °C
|
798
ksi <br>@Temperature 73.4 °F
|
ISO 178 |
|
Polykemi AB SCANBLEND FS7 F20 PBT/ASA Blend, Glass Fiber-Reinforced
Information provided by Polykemi AB
|
|||
| Flexural Modulus |
5.50
GPa <br>@Temperature 23.0 °C
|
798
ksi <br>@Temperature 73.4 °F
|
ISO 178 |
|
Polykemi AB SCANTEC PC S75R GF20 V0 Polycarbonate, Glass Fiber Reinforced, Flame Retardant
Information provided by Polykemi AB
|
|||
| Flexural Modulus | 5.50 - 6.50 GPa | 798 - 943 ksi | ISO 178 |
|
Perstorp Compounds Aminel FX Melamine
Organically reinforced melamine material with excellent flow properties and high flexibility suitable for applications involving high complexity and surface demands.Information provided by Perstorp ..
|
|||
| Flexural Modulus |
5.50
GPa <br>@Temperature 23.0 °C
|
798
ksi <br>@Temperature 73.4 °F
|
ISO 178 |
|
Polykemi AB SCANMID 6 B12^ Q40 Nylon 6, Mineral Reinforced
Information provided by Polykemi AB
|
|||
| Flexural Modulus |
5.50
GPa <br>@Temperature 90.0 °C
|
798
ksi <br>@Temperature 194 °F
|
ISO 178, ASTM D790 |
|
Nilit Nilamid A3 H G6 General Purpose 30% Glass Reinforced PA66
Description: Nilamid A3 H G6 is a general purpose 30% glass fiber reinforced NYLON 66 that gives an excellent combination of tensile strength, stiffness and impact strength. It is one of the most wi..
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics ULTEM 2312EPR PEI
30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics ULTEM 2312EPR PEI (Asia Pacific)
30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Ultem 2312EPR PEI (Europe-Africa-Middle East)
30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing.This data was supplied by SABIC-IP for the Eu..
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
|
SABIC Innovative Plastics ULTEM HU2100 PEI (Asia Pacific)
10% Glass fiber filled, standard flow Polyetherimide (Tg 217C). US FDA and European Food Contact approved. For medical devices and pharmaceutical applications.Healthcare management of change, biocom..
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | ISO Data |
|
Styrolution Terblend® N NG-06 30% Glass Filled ABS/PA6 (Conditioned)
Terblend N NG-06 is a 30% glass fiber reinforced ABS/PA6 blend with extra high rigidity and dimensional stability.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS..
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | |
|
Shandong Guangyin 1212 Reinforced Nylon
Features and Applications: Wear resistance, higher strength, better tenacity, strong adhesion and better low temperature resistance. It is applicable to surface coating of wires, cables, optical cab..
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
|
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS (Asia Pacific)
Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX..
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | ASTM-D790 |
|
Polyram PlusTek PA870G33 Nylon 6.6, 33% Glass Fiber
33% glass fiber reinforced, impact modified polyamide 6.6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | ASTM-D790 |
|
Polyram PlusTek PB825G5 Nylon 6, 25% Glass Fiber
25% glass fiber reinforced, impact modified polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | ASTM D790 |
|
Covestro Makrolon® 8325 Polycarbonate
High viscosity injection molding and extrusion grade with 20% standard glass fibers and easy mold release, high strength and stiffness.Information provided by Bayer.As of 1 September 2015, Bayer Mat..
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | cond; ISO 178 |
|
DSM Novamid® 1010GN2-20 NAT/BK37 PA6-GF20 FR(17)
20% Glass Reinforced, Flame Retardant
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | 2 mm/min; ISO 178 |
|
Eurostar Starflam BFR552Y3 PA6, Mineral/Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam BFR552Y3 is a Halogen and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar.
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | ISO 178 |
|
Eurotec® Tecomid® NB40 KK30 NL PA 6 30% glass fiber/mineral reinforced, low warpage
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | ISO 178 |
|
Eurotec® Tecomid® NA40 GR15 NL PA 6.6 15% glass fiber reinforced
Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good..
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | ASTM D790 |
|
Adell AT-14 Nylon 66, 20% Glass Reinforced; Impact Modified
Data provided by Adell Plastics, Inc.
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | ASTM D790 |
|
Beijing Chemical Industry KAIFA® 201-G20R PBT Resin
15% glass fiber reinforced, good flow and toughnessInformation provided by Beijing Chemical Industry Research Institute (Group)
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | ASTM D790 |
|
A. Schulman ComAlloy Hiloy® 512 Polycarbonate, Glass Reinforced, UL
Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | ISO 178 |
|
BASF Ultramid® A3WG3 15% Glass Filled PA66 (Dry)
Description: 15% Glass-fiber reinforced and heat aging resistant injection-molding grade for machine elements and housings of medium stiffness. For electric insulating parts, preference should be gi..
|
|||
| Flexural Modulus | 5.50 GPa | 798 ksi | ISO 178 |
|
BASF Ultramid® B3WG6 GP BK 23210 30% Glass Filled PA6 (Conditioned)
Description: 30% Glass fiber reinforced and heat aging resistant injection molding grade used e.g. for automobile manifold.Information provided by BASF
|
|||