| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Flexural Modulus | 5.60 GPa | 812 ksi | ISO 178 |
|
Polyplastic Armlen® PP GF 30-5HS-901 Polypropylene, 30% Glass Filled
Heat stabilized, black colorInformation provided by PolyPlastic Group.
|
|||
| Flexural Modulus | 5.60 GPa | 812 ksi | ISO 178 |
|
Nilit FRIANYL A63 GV15 Nylon 6.6 for injection molding, 15% glass fiber reinforced
Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Flexural Modulus | 5.60 GPa | 812 ksi | ISO 178 |
|
Nilit FRIANYL B63 CV10 Nylon 6.6 for injection molding, 10% carbon fiber reinforced
Nylon 6.6 for injection molding, good conductive and electrostatic properties.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Flexural Modulus | 5.60 GPa | 812 ksi | ISO 178 |
|
Nilit FRIANYL B63 KV50 Nylon 6 for injection molding, 50% glass ball reinforced
Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics
|
|||
| Flexural Modulus |
5.60
GPa @Temperature 23.0 °C |
812
ksi @Temperature 73.4 °F |
ISO 178 |
|
Polykemi AB SCANAMID 66 A13^ FX30 Nylon 66, Glass Fiber Reinforced
Information provided by Polykemi AB
|
|||
| Flexural Modulus | 5.60 GPa | 812 ksi | |
|
Plastcom SLOVALEN PH 66 GF 30 FRO 4 PP, 30% glass fibre, mod. of mech. prop.
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0..
|
|||
| Flexural Modulus |
5.60
GPa @Temperature 23.0 °C |
812
ksi @Temperature 73.4 °F |
ISO 178 |
|
Polykemi AB POLYfill PPH GF2030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB
|
|||
| Flexural Modulus |
5.60
GPa @Temperature 23.0 °C |
812
ksi @Temperature 73.4 °F |
ISO 178 |
|
Polykemi AB POLYfill PPH GF3030 PD2 PP, Glass Fiber-Reinforced, Chemically Coupled
Information provided by Polykemi AB
|
|||
| Flexural Modulus |
5.60
GPa @Temperature 23.0 °C |
812
ksi @Temperature 73.4 °F |
ISO 178 |
|
Polykemi AB POLYfill PPH GF5030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB
|
|||
| Flexural Modulus | 5.60 GPa | 812 ksi | 2mm/min; ASTM D790 |
|
Kingfa PBT-RG152 Flame Retardant, 15% Glass Fiber Reinforced PBT
Features:Flame retardantHigh strengthHigh temperature propertiesHigh glossyGood surfaceNo bloomingApplications:Injection moldingConnectorsRelayBobbinsPlugsE & E partsInformation Provided by Kingfa S..
|
|||
| Flexural Modulus | 5.60 GPa | 812 ksi | 2 mm/min; ISO 178-A |
|
Lanxess Pocan® B 3216 HR 000000 PBT 16% Glass Fiber
PBT, 16% glass fibers, injection molding, improved impact strength, hydrolysis stabilizedInformation provided by LANXESS.
|
|||
| Flexural Modulus | 5.60 GPa | 812 ksi | ASTM D790 |
|
Solvay Specialty Polymers KetaSpire® KT-820 GF13 Polyetheretherketone (PEEK), 13% Glass Fiber
KetaSpire® KT-820 is a low flow, 13% glass fiber reinforced grade of polyetheretherketone (PEEK). The glass fiber content is optimized to provide a balance of strength and stiffness with toughnes..
|
|||
| Flexural Modulus | 5.60 GPa | 812 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Valox® EH7025AG PBT+PET
Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application.
|
|||
| Flexural Modulus | 5.60 GPa | 812 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Asia Pacific)
Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application.
|
|||
| Flexural Modulus | 5.60 GPa | 812 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics Valox® SHF4340 PBT (Europe-Africa-Middle East)
20% GF Super High Flow PBT
|
|||
| Flexural Modulus | 5.60 GPa | 812 ksi | 2 mm/min; ISO 178 |
|
SABIC Innovative Plastics LNP Thermocomp MX06050 PP (Europe-Africa-Middle East)
LNP* THERMOCOMP* MX06050 is a compound based on Polypropylene resin containing Glass Fiber. Added features include; Heat Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea..
|
|||
| Flexural Modulus | 5.60 GPa | 812 ksi | ASTM D790 |
|
SABIC Innovative Plastics LNP THERMOCOMP PF003 PA 6
LNP THERMOCOMP* PF003 is a compound based on Nylon 6 resin containing 15% Glass Fiber.
|
|||
| Flexural Modulus | 5.60 GPa | 812 ksi | ISO 178 |
|
SABIC Innovative Plastics LNP THERMOCOMP MF004AS PP
LNP THERMOCOMP* MF004AS is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this material include: Heat Stabilized.
|
|||
| Flexural Modulus | 5.60 GPa | 812 ksi | ASTM D790 |
|
Saint-Gobain Meldin® 5001 Thermoplastic Bearing Material
General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin..
|
|||
| Flexural Modulus | 5.60 GPa | 812 ksi | ASTM D790 |
|
PlastxWorld Veroplas PB3301F Nylon 66
flame retarded (UL94 V0), 30% glass filled injection molding gradeInformation provided by PlastxWorld Inc.
|
|||
| Flexural Modulus | 5.60 GPa | 812 ksi | ASTM D790 |
|
Tipco Tipcolene® FPM 40 - 40% Mica Reinforced Polypropylene Homopolymer, High Stiffness
40% Mica Reinforced PP HomopolymerApplications: Electrical & AutomotiveProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India.
|
|||
| Flexural Modulus | 5.60 GPa | 812 ksi | ASTM-D790 |
|
Polyram RamOfin PPH302G6 Polypropylene, 30% Glass Fiber
30% glass fiber reinforced polypropylene for injection molding applicationsInformation provided by Polyram Ram On Ind.
|
|||
| Flexural Modulus | 5.60 GPa | 812 ksi | ISO 178 |
|
Polyram RamLloy PB917G6 Nylon 6/Polypropylene Alloy, 30% Glass Fiber Reinforced
30% Glass fiber reinforced Nylon6/PP alloy with reduced water absorption, dimensional stability and UV stabilized, for injection molding applications.Information provided by Polyram.
|
|||
| Flexural Modulus | 5.60 GPa | 812 ksi | cond; ISO 178 |
|
DSM Novamid® 1010GH30 NAT PA6-GF30
30% Glass Reinforced, Heat Stabilized, Injection Molding
|
|||
| Flexural Modulus | 5.60 GPa | 812 ksi | 50%RH; ISO 178 |
|
DuPont Performance Polymers Zytel® 84G33 BKB031 Nylon 66 + Nylon 6
(Unverified Data**)
33% Glass Reinforced Toughened Polyamide 66 + Polyamide 6 Zytel 84G33 BKB031 is a 33% glass reinforced toughened polyamide 66 and polyamide 6 co-melt black cube blended resin. This resin was develop..
|
|||
| Flexural Modulus | 5.60 GPa | 812 ksi | 2 mm/min; ISO 178 |
|
Eurostar Starflam PX08029 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded
Starflam PX08029 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
|
|||
| Flexural Modulus | 5.60 GPa | 812 ksi | ASTM D790 |
|
E-Polymers TEKAMID® TA250G15 , 15% Glass Fiber Reinforced PA66, DAM
15% Glass Fiber Reinforced, Good surfaceInformation provided by E-Polymers Co. Ltd.
|
|||
| Flexural Modulus | 5.60 GPa | 812 ksi | ISO 178 |
|
BASF Ultramid® S3EG6 Balance 30% Glass Filled PA 610 (Conditioned)
Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. ..
|
|||
| Flexural Modulus | 5.60 GPa | 812 ksi | ISO 178 |
|
BASF Ultramid® S3WG6 Balance 30% Glass Filled PA 610 (Conditioned)
Description: BASF supplies polyamide 610 for processing by injection molding under the trade name Ultramid® Balance which is produced by polycondensation of hexamethylene diamine and sebacic acid. ..
|
|||
| Flexural Modulus | 5.60 GPa | 812 ksi | ASTM D790 |
|
A. Schulman ComAlloy Hiloy® 109 Polypropylene, Glass/Mineral Reinforced, Chemically Coupled
Data provided by the manufacturer, ComAlloy International Company.40% Glass/Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
|
|||