Polymer Property : Flexural Modulus = 5.75 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Modulus 5.75 GPa
834 ksi
Plastcom SLOVAMID 66 GF 20 GB 10 HI PA66, improved strength
FeaturesModified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets for sport and other safe..
Flexural Modulus 5.75 GPa
834 ksi
ASTM D790
Omni Plastics OmniLon™ 6 PA6 GR15 NA Glass Reinforced Nylon
Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics
Flexural Modulus 5.75 GPa
834 ksi
ASTM D790
LATI LARIL 13 G/20 20% Glass Fiber Reinforced Polyphenylene Oxide (PPOm)  (Unverified Data**)
Description: Laril thermoplastics are polyphenylene oxide (PPOm) products. They exhibit excellent toughness, even at low temperatures, good thermal resistance and dimensional stability are the most ..
Flexural Modulus 5.75 GPa
834 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP KFL23LH Acetal Copolymer (Asia Pacific)
LNP* LUBRICOMP* KFL23LH is a compound based on Acetal Copolymer resin containing PTFE, Glass Fiber. Added features of this material include: Internally Lubricated.
Flexural Modulus 5.75 GPa
834 ksi
ISO 178
SABIC Innovative Plastics LNP THERMOCOMP DF004ER PC
LNP THERMOCOMP* DF004ER is a compound based on Polycarbonate resin containing 20% Glass Fiber. Added features of this material include: Easy Molding. Mold Release.
Flexural Modulus 5.75 GPa
<br>@Temperature 90.0 °C
834 ksi
<br>@Temperature 194 °F
ASTM D790
LATI LASULF G/20 20% Glass Reinforced Polysulfone (PSU) &nbsp;(Unverified Data**)
Description: Lasulf products are composed of polysulfone (PSU). They feature good thermal and mechanical properties such as excellent toughness, even at low temperatures, excellent dimensional stabi..