Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 500 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most.
Mechanical Properties Metric English Comments
Flexural Modulus 1.38 - 3.45 GPa
200 - 500 ksi
ASTM D790
PolyOne Stat-Tech™ AT-CB2/000 CR Acetal (POM) Copolymer
Stat-Tech™ AT-CB2/000 CR XP020229R2Information provided by PolyOne
Flexural Modulus 1.50 - 3.45 GPa
218 - 500 ksi
Average value: 2.98 GPa Grade Count:76
Overview of materials for Polystyrene, Heat Resistant Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Heat Resistant Grade". Each property range of values reported is minimum and maximum values..
Flexural Modulus 2.76 - 3.45 GPa
400 - 500 ksi
Average value: 3.00 GPa Grade Count:8
Overview of materials for Polycarbonate, Aramid Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Aramid Fiber Reinforced". Each property range of values reported is minimum and maximum v..
Flexural Modulus 2.76 - 3.45 GPa
400 - 500 ksi
Average value: 3.07 GPa Grade Count:11
Overview of materials for Nylon 612, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of..
Flexural Modulus 2.41 - 3.45 GPa
350 - 500 ksi
Average value: 3.02 GPa Grade Count:4
Overview of materials for Nylon 11 with 10% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 10% Glass Fiber Filler". Specific grades with glass content between 5% and 14% are includ..
Flexural Modulus 1.72 - 3.45 GPa
250 - 500 ksi
Average value: 2.69 GPa Grade Count:8
Overview of materials for Acrylic, UV Stabilized, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, UV Stabilized, Molded". Each property range of values reported is minimum and maximum values of..
Flexural Modulus 2.00 - 3.45 GPa
290 - 500 ksi
Average value: 2.96 GPa Grade Count:20
Overview of materials for Acrylic, Optical Grade, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Grade, Molded". Each property range of values reported is minimum and maximum values of..
Copyright © lookpolymers.com All Rights Reserved